Optical constants of HOYA - TaFD (Dense tantalum flint)
TAFD65
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=4.0113202-0.017752009λ^{2}+0.05856933λ^{-2}+0.0043200932λ^{-4}-0.00031070842λ^{-6}+3.7485638\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -6.69e-07 9.68e-09 -3.75e-11 1.14e-06 1.22e-09 0.264 nd: 2.05090 Vd: 26.94 glass_status: standard density: 5.27 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.9e-06 K-1 dPgF: 0.0055 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links