CC 20170401 HOYA Optical Glass Catalog NM FC5 1 487704 1.48749 70.45 0 0 4 GC General glass Type ED 9.300000000E+000 1.020000000E+001 2.450000000E+000 9.200000000E-003 0 0 CD 2.189405400E+000 -9.904490800E-003 8.640337000E-003 2.226306700E-004 -1.229194200E-005 5.938634900E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -6.604600000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 5.00000 5.00000 5.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.20000E-001 1.00000E+001 IT 2.90000E-001 4.30000E-001 1.00000E+001 IT 3.00000E-001 7.10000E-001 1.00000E+001 IT 3.10000E-001 8.68000E-001 1.00000E+001 IT 3.20000E-001 9.37000E-001 1.00000E+001 IT 3.30000E-001 9.70000E-001 1.00000E+001 IT 3.40000E-001 9.84000E-001 1.00000E+001 IT 3.50000E-001 9.92000E-001 1.00000E+001 IT 3.60000E-001 9.95000E-001 1.00000E+001 IT 3.70000E-001 9.96000E-001 1.00000E+001 IT 3.80000E-001 9.93000E-001 1.00000E+001 IT 3.90000E-001 9.98000E-001 1.00000E+001 IT 4.00000E-001 9.98000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.71000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM FCD1 1 497816 1.49700 81.61 0 1 1 GC Recommended glass type ED 1.320000000E+001 1.550000000E+001 3.700000000E+000 3.750000000E-002 0 0 CD 2.218113200E+000 -5.799427000E-003 8.347067900E-003 6.504652300E-005 8.514218600E-006 -5.885226900E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.920000000E-005 -8.390000000E-009 5.310000000E-012 3.680000000E-007 4.150000000E-010 -1.430000000E-001 2.000000000E+001 OD -1.00000 2.00000 4.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.70000E-002 1.00000E+001 IT 2.90000E-001 7.70000E-002 1.00000E+001 IT 3.00000E-001 1.90000E-001 1.00000E+001 IT 3.10000E-001 3.76000E-001 1.00000E+001 IT 3.20000E-001 5.86000E-001 1.00000E+001 IT 3.30000E-001 7.61000E-001 1.00000E+001 IT 3.40000E-001 8.78000E-001 1.00000E+001 IT 3.50000E-001 9.39000E-001 1.00000E+001 IT 3.60000E-001 9.72000E-001 1.00000E+001 IT 3.70000E-001 9.90000E-001 1.00000E+001 IT 3.80000E-001 9.95000E-001 1.00000E+001 IT 3.90000E-001 9.96000E-001 1.00000E+001 IT 4.00000E-001 9.95000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM FCD1B 1 497816 1.49710 81.56 0 0 4 GC General glass Type ED 1.290000000E+001 1.630000000E+001 3.640000000E+000 3.690000000E-002 0 0 CD 2.218906800E+000 -6.170706500E-003 8.088763100E-003 1.335778200E-004 1.947618600E-007 -2.257780400E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.750000000E-005 -5.280000000E-009 2.390000000E-011 3.520000000E-007 1.970000000E-010 1.860000000E-001 2.000000000E+001 OD -1.00000 1.00000 4.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 2.80000E-002 1.00000E+001 IT 3.10000E-001 1.12000E-001 1.00000E+001 IT 3.20000E-001 2.88000E-001 1.00000E+001 IT 3.30000E-001 5.20000E-001 1.00000E+001 IT 3.40000E-001 7.26000E-001 1.00000E+001 IT 3.50000E-001 8.63000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.72000E-001 1.00000E+001 IT 3.80000E-001 9.87000E-001 1.00000E+001 IT 3.90000E-001 9.93000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM FCD10A 1 459902 1.45860 90.20 0 1 1 GC Recommended glass type ED 1.330000000E+001 1.650000000E+001 3.630000000E+000 4.940000000E-002 0 0 CD 2.108588800E+000 -4.655372200E-003 6.954748000E-003 3.218414100E-005 5.267094600E-006 -2.716484400E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.040000000E-005 -8.810000000E-009 1.300000000E-011 3.440000000E-007 7.670000000E-011 1.540000000E-001 2.000000000E+001 OD -1.00000 1.00000 5.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.60000E-002 1.00000E+001 IT 2.90000E-001 5.90000E-002 1.00000E+001 IT 3.00000E-001 1.66000E-001 1.00000E+001 IT 3.10000E-001 3.47000E-001 1.00000E+001 IT 3.20000E-001 5.61000E-001 1.00000E+001 IT 3.30000E-001 7.44000E-001 1.00000E+001 IT 3.40000E-001 8.67000E-001 1.00000E+001 IT 3.50000E-001 9.35000E-001 1.00000E+001 IT 3.60000E-001 9.68000E-001 1.00000E+001 IT 3.70000E-001 9.83000E-001 1.00000E+001 IT 3.80000E-001 9.90000E-001 1.00000E+001 IT 3.90000E-001 9.94000E-001 1.00000E+001 IT 4.00000E-001 9.95000E-001 1.00000E+001 IT 4.20000E-001 9.96000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM FCD100 1 437951 1.43700 95.10 0 1 1 GC Recommended glass type ED 1.390000000E+001 1.750000000E+001 3.530000000E+000 5.640000000E-002 0 0 CD 2.048215700E+000 -4.321122200E-003 6.182675500E-003 3.141148000E-005 3.537079300E-006 -1.669449700E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.110000000E-005 -8.570000000E-009 2.980000000E-011 2.780000000E-007 2.180000000E-010 2.010000000E-001 2.000000000E+001 OD -1.00000 1.00000 -1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.50000E-002 1.00000E+001 IT 2.90000E-001 5.70000E-002 1.00000E+001 IT 3.00000E-001 1.68000E-001 1.00000E+001 IT 3.10000E-001 3.58000E-001 1.00000E+001 IT 3.20000E-001 5.79000E-001 1.00000E+001 IT 3.30000E-001 7.61000E-001 1.00000E+001 IT 3.40000E-001 8.80000E-001 1.00000E+001 IT 3.50000E-001 9.44000E-001 1.00000E+001 IT 3.60000E-001 9.76000E-001 1.00000E+001 IT 3.70000E-001 9.89000E-001 1.00000E+001 IT 3.80000E-001 9.95000E-001 1.00000E+001 IT 3.90000E-001 9.98000E-001 1.00000E+001 IT 4.00000E-001 9.97000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.98000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.95000E-001 1.00000E+001 IT 1.05000E+000 9.95000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM FCD515 1 593686 1.59282 68.63 0 1 1 GC Recommended glass type ED 1.110000000E+001 1.340000000E+001 4.130000000E+000 1.940000000E-002 0 0 CD 2.502355000E+000 -7.208004200E-003 1.201274300E-002 3.492084200E-004 -2.472967600E-005 1.380156700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.580000000E-005 3.730000000E-009 -1.830000000E-011 3.660000000E-007 1.720000000E-010 1.690000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 2.60000E-002 1.00000E+001 IT 3.30000E-001 1.09000E-001 1.00000E+001 IT 3.40000E-001 2.90000E-001 1.00000E+001 IT 3.50000E-001 5.18000E-001 1.00000E+001 IT 3.60000E-001 7.14000E-001 1.00000E+001 IT 3.70000E-001 8.56000E-001 1.00000E+001 IT 3.80000E-001 9.26000E-001 1.00000E+001 IT 3.90000E-001 9.62000E-001 1.00000E+001 IT 4.00000E-001 9.80000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM FCD705 1 550755 1.55032 75.50 0 1 1 GC Recommended glass type ED 1.220000000E+001 1.400000000E+001 4.090000000E+000 2.770000000E-002 0 0 CD 2.374283200E+000 -6.201441800E-003 1.058296700E-002 6.310070300E-005 8.196715000E-006 -3.442444600E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.640000000E-005 -6.430000000E-010 1.970000000E-011 3.830000000E-007 2.950000000E-010 7.710000000E-002 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 1.90000E-002 1.00000E+001 IT 3.20000E-001 8.70000E-002 1.00000E+001 IT 3.30000E-001 2.47000E-001 1.00000E+001 IT 3.40000E-001 4.78000E-001 1.00000E+001 IT 3.50000E-001 6.87000E-001 1.00000E+001 IT 3.60000E-001 8.30000E-001 1.00000E+001 IT 3.70000E-001 9.18000E-001 1.00000E+001 IT 3.80000E-001 9.56000E-001 1.00000E+001 IT 3.90000E-001 9.77000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.94000E-001 1.00000E+001 IT 7.80000E-001 9.94000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.84000E-001 1.00000E+001 IT 8.50000E-001 9.92000E-001 1.00000E+001 IT 9.00000E-001 9.92000E-001 1.00000E+001 IT 9.50000E-001 9.91000E-001 1.00000E+001 IT 1.00000E+000 9.92000E-001 1.00000E+001 IT 1.05000E+000 9.92000E-001 1.00000E+001 IT 1.06000E+000 9.92000E-001 1.00000E+001 IT 1.10000E+000 9.93000E-001 1.00000E+001 IT 1.20000E+000 9.94000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM PCD4 1 618634 1.61800 63.40 0 1 2 GC Recommended glass type ED 8.700000000E+000 1.110000000E+001 3.520000000E+000 6.000000000E-003 0 0 CD 2.580704500E+000 -1.095753800E-002 1.268943000E-002 6.638781200E-004 -6.484966400E-005 3.478786300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -8.930000000E-006 1.280000000E-008 -1.340000000E-011 5.360000000E-007 -8.840000000E-011 2.930000000E-009 2.000000000E+001 OD -1.00000 1.00000 3.00000 5.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.90000E-002 1.00000E+001 IT 2.90000E-001 9.30000E-002 1.00000E+001 IT 3.00000E-001 1.88000E-001 1.00000E+001 IT 3.10000E-001 3.14000E-001 1.00000E+001 IT 3.20000E-001 4.67000E-001 1.00000E+001 IT 3.30000E-001 6.16000E-001 1.00000E+001 IT 3.40000E-001 7.52000E-001 1.00000E+001 IT 3.50000E-001 8.47000E-001 1.00000E+001 IT 3.60000E-001 9.17000E-001 1.00000E+001 IT 3.70000E-001 9.55000E-001 1.00000E+001 IT 3.80000E-001 9.76000E-001 1.00000E+001 IT 3.90000E-001 9.89000E-001 1.00000E+001 IT 4.00000E-001 9.93000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM PCD40 1 620639 1.61997 63.88 0 1 1 GC Recommended glass type ED 1.030000000E+001 1.300000000E+001 3.570000000E+000 9.300000000E-003 0 0 CD 2.584446300E+000 -9.052185800E-003 1.430198700E-002 1.705077000E-004 4.964536000E-006 -1.292747900E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.080000000E-005 2.420000000E-009 1.570000000E-011 7.210000000E-007 4.290000000E-010 1.460000000E-009 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.40000E-002 1.00000E+001 IT 3.20000E-001 9.20000E-002 1.00000E+001 IT 3.30000E-001 2.40000E-001 1.00000E+001 IT 3.40000E-001 4.55000E-001 1.00000E+001 IT 3.50000E-001 6.63000E-001 1.00000E+001 IT 3.60000E-001 8.15000E-001 1.00000E+001 IT 3.70000E-001 9.11000E-001 1.00000E+001 IT 3.80000E-001 9.54000E-001 1.00000E+001 IT 3.90000E-001 9.76000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.94000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.94000E-001 1.00000E+001 IT 9.50000E-001 9.94000E-001 1.00000E+001 IT 1.00000E+000 9.94000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM PCD51 1 593670 1.59349 67.00 0 1 2 GC Recommended glass type ED 8.900000000E+000 1.160000000E+001 3.140000000E+000 9.100000000E-003 0 0 CD 2.504663800E+000 -1.014944800E-002 1.265376900E-002 1.656664200E-004 5.387174700E-007 5.584093000E-008 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -5.750000000E-006 4.330000000E-009 -1.700000000E-011 3.990000000E-007 4.040000000E-010 1.750000000E-001 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.45000E-001 1.00000E+001 IT 2.90000E-001 2.60000E-001 1.00000E+001 IT 3.00000E-001 3.97000E-001 1.00000E+001 IT 3.10000E-001 5.47000E-001 1.00000E+001 IT 3.20000E-001 6.90000E-001 1.00000E+001 IT 3.30000E-001 8.02000E-001 1.00000E+001 IT 3.40000E-001 8.84000E-001 1.00000E+001 IT 3.50000E-001 9.35000E-001 1.00000E+001 IT 3.60000E-001 9.64000E-001 1.00000E+001 IT 3.70000E-001 9.78000E-001 1.00000E+001 IT 3.80000E-001 9.86000E-001 1.00000E+001 IT 3.90000E-001 9.90000E-001 1.00000E+001 IT 4.00000E-001 9.91000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM BSC7 1 517642 1.51680 64.20 0 0 4 GC General glass Type ED 7.600000000E+000 9.300000000E+000 2.520000000E+000 1.600000000E-003 0 0 CD 2.270256600E+000 -9.198810100E-003 1.160970600E-002 -7.612391100E-005 2.855872700E-005 -1.256648600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.254790000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.70000E-002 1.00000E+001 IT 2.90000E-001 1.51000E-001 1.00000E+001 IT 3.00000E-001 3.96000E-001 1.00000E+001 IT 3.10000E-001 6.52000E-001 1.00000E+001 IT 3.20000E-001 8.18000E-001 1.00000E+001 IT 3.30000E-001 9.06000E-001 1.00000E+001 IT 3.40000E-001 9.48000E-001 1.00000E+001 IT 3.50000E-001 9.70000E-001 1.00000E+001 IT 3.60000E-001 9.89000E-001 1.00000E+001 IT 3.70000E-001 9.92000E-001 1.00000E+001 IT 3.80000E-001 9.93000E-001 1.00000E+001 IT 3.90000E-001 9.97000E-001 1.00000E+001 IT 4.00000E-001 9.98000E-001 1.00000E+001 IT 4.20000E-001 9.99000E-001 1.00000E+001 IT 4.40000E-001 9.98000E-001 1.00000E+001 IT 4.60000E-001 9.99000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.94000E-001 1.00000E+001 IT 1.40000E+000 9.74000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.89000E-001 1.00000E+001 NM E-C3 1 518590 1.51823 58.96 0 0 4 GC General glass Type ED 9.900000000E+000 1.220000000E+001 2.530000000E+000 2.000000000E-003 0 0 CD 2.272545200E+000 -8.410491000E-003 1.130684300E-002 3.778229700E-004 -2.690342300E-005 1.597648900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -3.246080000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.90000E-002 1.00000E+001 IT 2.90000E-001 1.42000E-001 1.00000E+001 IT 3.00000E-001 4.22000E-001 1.00000E+001 IT 3.10000E-001 7.12000E-001 1.00000E+001 IT 3.20000E-001 8.71000E-001 1.00000E+001 IT 3.30000E-001 9.32000E-001 1.00000E+001 IT 3.40000E-001 9.69000E-001 1.00000E+001 IT 3.50000E-001 9.75000E-001 1.00000E+001 IT 3.60000E-001 9.91000E-001 1.00000E+001 IT 3.70000E-001 9.84000E-001 1.00000E+001 IT 3.80000E-001 9.88000E-001 1.00000E+001 IT 3.90000E-001 9.91000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.93000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.94000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM BAC4 1 569560 1.56883 56.04 0 0 4 GC General glass Type ED 5.300000000E+000 6.900000000E+000 2.850000000E+000 1.000000000E-003 0 0 CD 2.419664500E+000 -8.332931400E-003 1.539739000E-002 -1.739165400E-004 6.218322000E-005 -3.062131000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 9.310000000E-006 1.090000000E-008 -5.680000000E-011 4.670000000E-007 7.990000000E-010 2.480000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 1.50000E-002 1.00000E+001 IT 3.00000E-001 9.70000E-002 1.00000E+001 IT 3.10000E-001 2.81000E-001 1.00000E+001 IT 3.20000E-001 5.00000E-001 1.00000E+001 IT 3.30000E-001 6.84000E-001 1.00000E+001 IT 3.40000E-001 8.12000E-001 1.00000E+001 IT 3.50000E-001 8.92000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.64000E-001 1.00000E+001 IT 3.80000E-001 9.76000E-001 1.00000E+001 IT 3.90000E-001 9.85000E-001 1.00000E+001 IT 4.00000E-001 9.88000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.87000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM BACD5 1 589613 1.58913 61.25 0 0 4 GC General glass Type ED 5.500000000E+000 6.900000000E+000 3.270000000E+000 2.400000000E-003 0 0 CD 2.486149900E+000 -9.568484500E-003 1.468505900E-002 -1.121648700E-004 4.197877700E-005 -1.885619000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.090000000E-006 1.250000000E-008 -4.950000000E-011 5.430000000E-007 5.600000000E-010 1.570000000E-009 2.000000000E+001 OD -1.00000 2.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 5.90000E-002 1.00000E+001 IT 3.00000E-001 1.89000E-001 1.00000E+001 IT 3.10000E-001 3.87000E-001 1.00000E+001 IT 3.20000E-001 5.90000E-001 1.00000E+001 IT 3.30000E-001 7.52000E-001 1.00000E+001 IT 3.40000E-001 8.56000E-001 1.00000E+001 IT 3.50000E-001 9.22000E-001 1.00000E+001 IT 3.60000E-001 9.56000E-001 1.00000E+001 IT 3.70000E-001 9.76000E-001 1.00000E+001 IT 3.80000E-001 9.85000E-001 1.00000E+001 IT 3.90000E-001 9.90000E-001 1.00000E+001 IT 4.00000E-001 9.94000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.80000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM BACD14 1 603607 1.60311 60.69 0 0 4 GC General glass Type ED 6.000000000E+000 7.400000000E+000 3.430000000E+000 1.900000000E-003 0 0 CD 2.533525600E+000 -1.190333800E-002 1.225724900E-002 7.917214900E-004 -7.738182900E-005 3.993544100E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.221230000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 5.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 2.80000E-002 1.00000E+001 IT 3.00000E-001 1.28000E-001 1.00000E+001 IT 3.10000E-001 3.13000E-001 1.00000E+001 IT 3.20000E-001 5.22000E-001 1.00000E+001 IT 3.30000E-001 6.93000E-001 1.00000E+001 IT 3.40000E-001 8.19000E-001 1.00000E+001 IT 3.50000E-001 8.94000E-001 1.00000E+001 IT 3.60000E-001 9.41000E-001 1.00000E+001 IT 3.70000E-001 9.65000E-001 1.00000E+001 IT 3.80000E-001 9.78000E-001 1.00000E+001 IT 3.90000E-001 9.88000E-001 1.00000E+001 IT 4.00000E-001 9.90000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.83000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM BACD15 1 623581 1.62299 58.12 0 0 4 GC General glass Type ED 6.100000000E+000 7.500000000E+000 3.550000000E+000 8.000000000E-004 0 0 CD 2.586483200E+000 -8.035782900E-003 1.808057300E-002 -4.597417200E-004 8.848432100E-005 -3.754476500E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.969200000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 1.00000E-002 1.00000E+001 IT 3.00000E-001 8.00000E-002 1.00000E+001 IT 3.10000E-001 2.20000E-001 1.00000E+001 IT 3.20000E-001 4.30000E-001 1.00000E+001 IT 3.30000E-001 6.20000E-001 1.00000E+001 IT 3.40000E-001 7.70000E-001 1.00000E+001 IT 3.50000E-001 8.70000E-001 1.00000E+001 IT 3.60000E-001 9.27000E-001 1.00000E+001 IT 3.70000E-001 9.59000E-001 1.00000E+001 IT 3.80000E-001 9.75000E-001 1.00000E+001 IT 3.90000E-001 9.86000E-001 1.00000E+001 IT 4.00000E-001 9.91000E-001 1.00000E+001 IT 4.20000E-001 9.94000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.84000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM BACD16 1 620603 1.62041 60.34 0 0 4 GC General glass Type ED 6.000000000E+000 7.100000000E+000 3.520000000E+000 -3.000000000E-004 0 0 CD 2.585989800E+000 -1.194043200E-002 1.399550200E-002 4.897450200E-004 -3.912071700E-005 2.261191500E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.986760000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 -1.00000 5.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 4.80000E-002 1.00000E+001 IT 3.10000E-001 1.42000E-001 1.00000E+001 IT 3.20000E-001 3.06000E-001 1.00000E+001 IT 3.30000E-001 5.03000E-001 1.00000E+001 IT 3.40000E-001 6.77000E-001 1.00000E+001 IT 3.50000E-001 8.03000E-001 1.00000E+001 IT 3.60000E-001 8.90000E-001 1.00000E+001 IT 3.70000E-001 9.39000E-001 1.00000E+001 IT 3.80000E-001 9.65000E-001 1.00000E+001 IT 3.90000E-001 9.79000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.93000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.84000E-001 1.00000E+001 IT 1.50000E+000 9.90000E-001 1.00000E+001 IT 1.55000E+000 9.90000E-001 1.00000E+001 NM BACD18 1 639555 1.63854 55.45 0 0 4 GC General glass Type ED 6.900000000E+000 8.100000000E+000 3.660000000E+000 -1.100000000E-003 0 0 CD 2.636527700E+000 -9.755846400E-003 1.714366500E-002 2.259249700E-004 3.085534200E-006 4.583191700E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.937960000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 7.90000E-002 1.00000E+001 IT 3.30000E-001 3.36000E-001 1.00000E+001 IT 3.40000E-001 6.21000E-001 1.00000E+001 IT 3.50000E-001 7.99000E-001 1.00000E+001 IT 3.60000E-001 9.02000E-001 1.00000E+001 IT 3.70000E-001 9.49000E-001 1.00000E+001 IT 3.80000E-001 9.71000E-001 1.00000E+001 IT 3.90000E-001 9.82000E-001 1.00000E+001 IT 4.00000E-001 9.87000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM BACED5 1 658509 1.65844 50.86 0 0 4 GC General glass Type ED 7.200000000E+000 8.900000000E+000 3.640000000E+000 8.000000000E-004 0 0 CD 2.693424500E+000 -8.637014000E-003 2.049645000E-002 -9.320545300E-005 6.270974700E-005 -2.083465200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.341010000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.30000E-001 3.90000E-002 1.00000E+001 IT 3.40000E-001 2.38000E-001 1.00000E+001 IT 3.50000E-001 5.23000E-001 1.00000E+001 IT 3.60000E-001 7.47000E-001 1.00000E+001 IT 3.70000E-001 8.72000E-001 1.00000E+001 IT 3.80000E-001 9.33000E-001 1.00000E+001 IT 3.90000E-001 9.62000E-001 1.00000E+001 IT 4.00000E-001 9.79000E-001 1.00000E+001 IT 4.20000E-001 9.88000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM LAC8 1 713539 1.71300 53.94 0 1 2 GC Recommended glass type ED 5.900000000E+000 7.200000000E+000 3.810000000E+000 -7.000000000E-003 0 0 CD 2.877853700E+000 -1.383290600E-002 2.030118500E-002 2.775987100E-004 5.905983000E-006 1.774764700E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.587760000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.80000E-001 1.00000E+001 IT 2.90000E-001 3.06000E-001 1.00000E+001 IT 3.00000E-001 4.31000E-001 1.00000E+001 IT 3.10000E-001 5.51000E-001 1.00000E+001 IT 3.20000E-001 6.63000E-001 1.00000E+001 IT 3.30000E-001 7.61000E-001 1.00000E+001 IT 3.40000E-001 8.38000E-001 1.00000E+001 IT 3.50000E-001 8.89000E-001 1.00000E+001 IT 3.60000E-001 9.32000E-001 1.00000E+001 IT 3.70000E-001 9.62000E-001 1.00000E+001 IT 3.80000E-001 9.76000E-001 1.00000E+001 IT 3.90000E-001 9.81000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.90000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM LAC14 1 697555 1.69680 55.46 0 1 2 GC Recommended glass type ED 5.600000000E+000 7.200000000E+000 3.670000000E+000 -5.900000000E-003 0 0 CD 2.825522900E+000 -1.363290200E-002 1.979140200E-002 1.503256400E-005 4.076136800E-005 -1.752726700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.050000000E-006 1.070000000E-008 -2.210000000E-011 4.350000000E-007 4.490000000E-010 1.850000000E-001 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.31000E-001 1.00000E+001 IT 2.90000E-001 3.64000E-001 1.00000E+001 IT 3.00000E-001 4.91000E-001 1.00000E+001 IT 3.10000E-001 6.02000E-001 1.00000E+001 IT 3.20000E-001 7.01000E-001 1.00000E+001 IT 3.30000E-001 7.92000E-001 1.00000E+001 IT 3.40000E-001 8.63000E-001 1.00000E+001 IT 3.50000E-001 9.10000E-001 1.00000E+001 IT 3.60000E-001 9.39000E-001 1.00000E+001 IT 3.70000E-001 9.63000E-001 1.00000E+001 IT 3.80000E-001 9.74000E-001 1.00000E+001 IT 3.90000E-001 9.83000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM TAC8 1 729547 1.72916 54.67 0 1 2 GC Recommended glass type ED 5.600000000E+000 7.300000000E+000 4.050000000E+000 -4.600000000E-003 0 0 CD 2.932417800E+000 -1.460315600E-002 2.112163600E-002 4.824014400E-005 4.966947500E-005 -2.490449100E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.780000000E-006 1.020000000E-008 -2.660000000E-011 4.130000000E-007 1.530000000E-010 2.020000000E-001 2.000000000E+001 OD -1.00000 1.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.78000E-001 1.00000E+001 IT 2.90000E-001 3.33000E-001 1.00000E+001 IT 3.00000E-001 4.67000E-001 1.00000E+001 IT 3.10000E-001 5.62000E-001 1.00000E+001 IT 3.20000E-001 6.89000E-001 1.00000E+001 IT 3.30000E-001 7.85000E-001 1.00000E+001 IT 3.40000E-001 8.53000E-001 1.00000E+001 IT 3.50000E-001 9.08000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.60000E-001 1.00000E+001 IT 3.80000E-001 9.73000E-001 1.00000E+001 IT 3.90000E-001 9.82000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.92000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.82000E-001 1.00000E+001 IT 1.50000E+000 9.83000E-001 1.00000E+001 IT 1.55000E+000 9.86000E-001 1.00000E+001 NM E-CF6 1 517522 1.51742 52.15 0 0 4 GC General glass Type ED 8.200000000E+000 9.200000000E+000 2.430000000E+000 4.500000000E-003 0 0 CD 2.266891200E+000 -9.386621200E-003 1.217419500E-002 5.076903000E-004 -3.357341400E-005 2.905901300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.624530000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 1.50000E-001 1.00000E+001 IT 3.50000E-001 5.59000E-001 1.00000E+001 IT 3.60000E-001 8.47000E-001 1.00000E+001 IT 3.70000E-001 9.39000E-001 1.00000E+001 IT 3.80000E-001 9.67000E-001 1.00000E+001 IT 3.90000E-001 9.78000E-001 1.00000E+001 IT 4.00000E-001 9.82000E-001 1.00000E+001 IT 4.20000E-001 9.85000E-001 1.00000E+001 IT 4.40000E-001 9.86000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.89000E-001 1.00000E+001 IT 5.00000E-001 9.90000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM E-FEL1 1 548458 1.54814 45.82 0 0 4 GC General glass Type ED 7.900000000E+000 9.600000000E+000 2.540000000E+000 4.100000000E-003 0 0 CD 2.353448400E+000 -1.033043800E-002 1.409732500E-002 8.716787500E-004 -6.998197000E-005 5.786735900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.324170000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.92000E-001 1.00000E+001 IT 3.60000E-001 6.30000E-001 1.00000E+001 IT 3.70000E-001 8.64000E-001 1.00000E+001 IT 3.80000E-001 9.44000E-001 1.00000E+001 IT 3.90000E-001 9.67000E-001 1.00000E+001 IT 4.00000E-001 9.80000E-001 1.00000E+001 IT 4.20000E-001 9.85000E-001 1.00000E+001 IT 4.40000E-001 9.85000E-001 1.00000E+001 IT 4.60000E-001 9.87000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.92000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM E-FEL2 1 541472 1.54072 47.20 0 0 4 GC General glass Type ED 8.200000000E+000 1.000000000E+001 2.530000000E+000 4.400000000E-003 0 0 CD 2.331798300E+000 -9.704219200E-003 1.403276100E-002 6.482289600E-004 -4.081376100E-005 3.906487300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 2.70000E-002 1.00000E+001 IT 3.50000E-001 3.12000E-001 1.00000E+001 IT 3.60000E-001 7.28000E-001 1.00000E+001 IT 3.70000E-001 9.08000E-001 1.00000E+001 IT 3.80000E-001 9.60000E-001 1.00000E+001 IT 3.90000E-001 9.79000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.92000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM E-FL5 1 581409 1.58144 40.89 0 0 4 GC General glass Type ED 7.900000000E+000 9.100000000E+000 2.590000000E+000 2.000000000E-003 0 0 CD 2.446575400E+000 -1.010704100E-002 1.775913200E-002 8.797025900E-004 -5.701492900E-005 6.092466300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.750000000E-006 1.660000000E-008 -9.670000000E-011 6.440000000E-007 4.370000000E-010 2.640000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 3.20000E-002 1.00000E+001 IT 3.60000E-001 3.25000E-001 1.00000E+001 IT 3.70000E-001 6.92000E-001 1.00000E+001 IT 3.80000E-001 8.73000E-001 1.00000E+001 IT 3.90000E-001 9.41000E-001 1.00000E+001 IT 4.00000E-001 9.67000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM E-FL6 1 567428 1.56732 42.84 0 0 4 GC General glass Type ED 6.700000000E+000 7.900000000E+000 2.530000000E+000 3.100000000E-003 0 0 CD 2.407965300E+000 -1.113563800E-002 1.570471500E-002 9.918650700E-004 -7.993465300E-005 7.098547300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.427210000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.90000E-002 1.00000E+001 IT 3.60000E-001 2.54000E-001 1.00000E+001 IT 3.70000E-001 6.19000E-001 1.00000E+001 IT 3.80000E-001 8.33000E-001 1.00000E+001 IT 3.90000E-001 9.21000E-001 1.00000E+001 IT 4.00000E-001 9.60000E-001 1.00000E+001 IT 4.20000E-001 9.83000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.90000E-001 1.00000E+001 IT 4.80000E-001 9.93000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.79000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM E-F2 1 620363 1.62004 36.30 0 0 4 GC General glass Type ED 8.300000000E+000 1.020000000E+001 2.670000000E+000 4.300000000E-003 0 0 CD 2.556182200E+000 -1.023703800E-002 2.247034800E-002 8.458067900E-004 -3.308708900E-005 7.105491900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.388410000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.47000E-001 1.00000E+001 IT 3.70000E-001 5.42000E-001 1.00000E+001 IT 3.80000E-001 8.02000E-001 1.00000E+001 IT 3.90000E-001 9.10000E-001 1.00000E+001 IT 4.00000E-001 9.52000E-001 1.00000E+001 IT 4.20000E-001 9.74000E-001 1.00000E+001 IT 4.40000E-001 9.81000E-001 1.00000E+001 IT 4.60000E-001 9.82000E-001 1.00000E+001 IT 4.80000E-001 9.85000E-001 1.00000E+001 IT 5.00000E-001 9.89000E-001 1.00000E+001 IT 5.50000E-001 9.95000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.93000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-F5 1 603380 1.60342 38.01 0 0 4 GC General glass Type ED 8.000000000E+000 9.500000000E+000 2.630000000E+000 2.900000000E-003 0 0 CD 2.509567300E+000 -1.086266100E-002 1.989477400E-002 1.013713400E-003 -6.269711700E-005 7.508004500E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.639670000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.90000E-001 1.00000E+001 IT 3.70000E-001 5.74000E-001 1.00000E+001 IT 3.80000E-001 8.20000E-001 1.00000E+001 IT 3.90000E-001 9.16000E-001 1.00000E+001 IT 4.00000E-001 9.57000E-001 1.00000E+001 IT 4.20000E-001 9.78000E-001 1.00000E+001 IT 4.40000E-001 9.84000E-001 1.00000E+001 IT 4.60000E-001 9.85000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.91000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM E-FD1 1 717295 1.71736 29.50 0 0 4 GC General glass Type ED 9.200000000E+000 1.090000000E+001 3.080000000E+000 8.200000000E-003 0 0 CD 2.850849900E+000 -1.323461000E-002 2.941532500E-002 2.554266600E-003 -2.123213300E-004 2.226193600E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -3.500330000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.50000E-002 1.00000E+001 IT 3.70000E-001 2.14000E-001 1.00000E+001 IT 3.80000E-001 5.43000E-001 1.00000E+001 IT 3.90000E-001 7.62000E-001 1.00000E+001 IT 4.00000E-001 8.68000E-001 1.00000E+001 IT 4.20000E-001 9.48000E-001 1.00000E+001 IT 4.40000E-001 9.68000E-001 1.00000E+001 IT 4.60000E-001 9.76000E-001 1.00000E+001 IT 4.80000E-001 9.82000E-001 1.00000E+001 IT 5.00000E-001 9.88000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM E-FD2 1 648338 1.64769 33.84 0 0 4 GC General glass Type ED 8.800000000E+000 1.090000000E+001 2.770000000E+000 4.900000000E-003 0 0 CD 2.639964400E+000 -1.164571800E-002 2.306173300E-002 1.734821900E-003 -1.398605900E-004 1.391667000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.24000E-001 1.00000E+001 IT 3.70000E-001 4.96000E-001 1.00000E+001 IT 3.80000E-001 7.69000E-001 1.00000E+001 IT 3.90000E-001 8.91000E-001 1.00000E+001 IT 4.00000E-001 9.45000E-001 1.00000E+001 IT 4.20000E-001 9.75000E-001 1.00000E+001 IT 4.40000E-001 9.83000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.91000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-FD4 1 755275 1.75520 27.53 0 0 4 GC General glass Type ED 8.700000000E+000 1.000000000E+001 3.230000000E+000 1.030000000E-002 0 0 CD 2.967317300E+000 -1.398956500E-002 3.345668000E-002 3.071780400E-003 -2.668243500E-004 2.895024100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.675000000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.91000E-001 1.00000E+001 IT 3.80000E-001 5.51000E-001 1.00000E+001 IT 3.90000E-001 7.78000E-001 1.00000E+001 IT 4.00000E-001 8.76000E-001 1.00000E+001 IT 4.20000E-001 9.44000E-001 1.00000E+001 IT 4.40000E-001 9.66000E-001 1.00000E+001 IT 4.60000E-001 9.74000E-001 1.00000E+001 IT 4.80000E-001 9.82000E-001 1.00000E+001 IT 5.00000E-001 9.87000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.93000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM E-FD5 1 673322 1.67270 32.17 0 0 4 GC General glass Type ED 8.900000000E+000 1.090000000E+001 2.900000000E+000 5.900000000E-003 0 0 CD 2.713583900E+000 -1.141971900E-002 2.613370800E-002 1.757647900E-003 -1.330773700E-004 1.520335100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.849170000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 4.80000E-002 1.00000E+001 IT 3.70000E-001 3.60000E-001 1.00000E+001 IT 3.80000E-001 6.92000E-001 1.00000E+001 IT 3.90000E-001 8.57000E-001 1.00000E+001 IT 4.00000E-001 9.22000E-001 1.00000E+001 IT 4.20000E-001 9.62000E-001 1.00000E+001 IT 4.40000E-001 9.75000E-001 1.00000E+001 IT 4.60000E-001 9.79000E-001 1.00000E+001 IT 4.80000E-001 9.85000E-001 1.00000E+001 IT 5.00000E-001 9.88000E-001 1.00000E+001 IT 5.50000E-001 9.94000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM E-FD8 1 689312 1.68893 31.16 0 0 4 GC General glass Type ED 9.300000000E+000 1.120000000E+001 2.970000000E+000 6.700000000E-003 0 0 CD 2.761758600E+000 -1.125403900E-002 2.822173700E-002 1.754031500E-003 -1.212705300E-004 1.552238400E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.087060000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 3.70000E-002 1.00000E+001 IT 3.70000E-001 3.08000E-001 1.00000E+001 IT 3.80000E-001 6.40000E-001 1.00000E+001 IT 3.90000E-001 8.22000E-001 1.00000E+001 IT 4.00000E-001 9.04000E-001 1.00000E+001 IT 4.20000E-001 9.60000E-001 1.00000E+001 IT 4.40000E-001 9.77000E-001 1.00000E+001 IT 4.60000E-001 9.81000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.87000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-FD10 1 728283 1.72825 28.32 0 0 4 GC General glass Type ED 9.000000000E+000 1.090000000E+001 3.070000000E+000 8.500000000E-003 0 0 CD 2.881518000E+000 -1.322831200E-002 3.145559000E-002 2.685166600E-003 -2.257754400E-004 2.469326800E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -3.455050000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.68000E-001 1.00000E+001 IT 3.80000E-001 4.97000E-001 1.00000E+001 IT 3.90000E-001 7.33000E-001 1.00000E+001 IT 4.00000E-001 8.53000E-001 1.00000E+001 IT 4.20000E-001 9.37000E-001 1.00000E+001 IT 4.40000E-001 9.64000E-001 1.00000E+001 IT 4.60000E-001 9.73000E-001 1.00000E+001 IT 4.80000E-001 9.80000E-001 1.00000E+001 IT 5.00000E-001 9.85000E-001 1.00000E+001 IT 5.50000E-001 9.94000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-FD13 1 741278 1.74077 27.76 0 0 4 GC General glass Type ED 9.100000000E+000 1.100000000E+001 3.110000000E+000 9.300000000E-003 0 0 CD 2.920590600E+000 -1.368161800E-002 3.256776000E-002 2.872551900E-003 -2.427710700E-004 2.661451400E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -3.405170000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.67000E-001 1.00000E+001 IT 3.80000E-001 4.87000E-001 1.00000E+001 IT 3.90000E-001 7.22000E-001 1.00000E+001 IT 4.00000E-001 8.45000E-001 1.00000E+001 IT 4.20000E-001 9.36000E-001 1.00000E+001 IT 4.40000E-001 9.61000E-001 1.00000E+001 IT 4.60000E-001 9.73000E-001 1.00000E+001 IT 4.80000E-001 9.79000E-001 1.00000E+001 IT 5.00000E-001 9.85000E-001 1.00000E+001 IT 5.50000E-001 9.95000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.91000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM E-FD15 1 699301 1.69895 30.05 0 0 4 GC General glass Type ED 8.700000000E+000 1.060000000E+001 2.950000000E+000 8.600000000E-003 0 0 CD 2.791994300E+000 -1.231120600E-002 2.880274100E-002 2.143005900E-003 -1.693211900E-004 1.974176600E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.367990000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 3.50000E-002 1.00000E+001 IT 3.70000E-001 2.31000E-001 1.00000E+001 IT 3.80000E-001 5.42000E-001 1.00000E+001 IT 3.90000E-001 7.65000E-001 1.00000E+001 IT 4.00000E-001 8.74000E-001 1.00000E+001 IT 4.20000E-001 9.48000E-001 1.00000E+001 IT 4.40000E-001 9.66000E-001 1.00000E+001 IT 4.60000E-001 9.73000E-001 1.00000E+001 IT 4.80000E-001 9.80000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.92000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM FD60-W 1 805255 1.80518 25.46 0 1 2 GC Recommended glass type ED 8.800000000E+000 1.090000000E+001 3.360000000E+000 1.320000000E-002 0 0 CD 3.117148300E+000 -1.161627700E-002 4.486497500E-002 1.658849100E-003 2.571685400E-005 1.475765700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -5.290000000E-006 9.600000000E-009 -5.100000000E-011 1.060000000E-006 1.340000000E-009 2.820000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.30000E-002 1.00000E+001 IT 3.70000E-001 2.32000E-001 1.00000E+001 IT 3.80000E-001 5.93000E-001 1.00000E+001 IT 3.90000E-001 8.00000E-001 1.00000E+001 IT 4.00000E-001 8.91000E-001 1.00000E+001 IT 4.20000E-001 9.52000E-001 1.00000E+001 IT 4.40000E-001 9.69000E-001 1.00000E+001 IT 4.60000E-001 9.77000E-001 1.00000E+001 IT 4.80000E-001 9.82000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.93000E-001 1.00000E+001 IT 6.00000E-001 9.92000E-001 1.00000E+001 IT 6.50000E-001 9.93000E-001 1.00000E+001 IT 7.00000E-001 9.93000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM FD60 1 805255 1.80518 25.46 0 0 4 GC General glass Type ED 8.800000000E+000 1.090000000E+001 3.360000000E+000 1.320000000E-002 0 0 CD 3.117148300E+000 -1.161627700E-002 4.486497500E-002 1.658849100E-003 2.571685400E-005 1.475765700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -5.290000000E-006 9.600000000E-009 -5.100000000E-011 1.060000000E-006 1.340000000E-009 2.820000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.40000E-002 1.00000E+001 IT 3.70000E-001 2.34000E-001 1.00000E+001 IT 3.80000E-001 5.99000E-001 1.00000E+001 IT 3.90000E-001 8.06000E-001 1.00000E+001 IT 4.00000E-001 8.89000E-001 1.00000E+001 IT 4.20000E-001 9.39000E-001 1.00000E+001 IT 4.40000E-001 9.57000E-001 1.00000E+001 IT 4.60000E-001 9.65000E-001 1.00000E+001 IT 4.80000E-001 9.72000E-001 1.00000E+001 IT 5.00000E-001 9.79000E-001 1.00000E+001 IT 5.50000E-001 9.91000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.90000E-001 1.00000E+001 IT 7.00000E-001 9.93000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM FD110 1 785257 1.78472 25.72 0 0 4 GC General glass Type ED 9.100000000E+000 1.080000000E+001 3.220000000E+000 1.380000000E-002 0 0 CD 3.053441500E+000 -1.275181000E-002 4.060936900E-002 2.270610900E-003 -7.808660600E-005 1.987402600E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.296760000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.32000E-001 1.00000E+001 IT 3.80000E-001 4.54000E-001 1.00000E+001 IT 3.90000E-001 6.87000E-001 1.00000E+001 IT 4.00000E-001 8.10000E-001 1.00000E+001 IT 4.20000E-001 9.12000E-001 1.00000E+001 IT 4.40000E-001 9.46000E-001 1.00000E+001 IT 4.60000E-001 9.64000E-001 1.00000E+001 IT 4.80000E-001 9.75000E-001 1.00000E+001 IT 5.00000E-001 9.83000E-001 1.00000E+001 IT 5.50000E-001 9.93000E-001 1.00000E+001 IT 6.00000E-001 9.92000E-001 1.00000E+001 IT 6.50000E-001 9.90000E-001 1.00000E+001 IT 7.00000E-001 9.91000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM FD140 1 762266 1.76182 26.61 0 0 4 GC General glass Type ED 8.400000000E+000 1.020000000E+001 3.140000000E+000 1.180000000E-002 0 0 CD 2.985129400E+000 -1.423798800E-002 3.549643700E-002 2.845755700E-003 -1.900679900E-004 2.430925200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.311570000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 9.10000E-002 1.00000E+001 IT 3.80000E-001 3.92000E-001 1.00000E+001 IT 3.90000E-001 6.63000E-001 1.00000E+001 IT 4.00000E-001 8.12000E-001 1.00000E+001 IT 4.20000E-001 9.24000E-001 1.00000E+001 IT 4.40000E-001 9.54000E-001 1.00000E+001 IT 4.60000E-001 9.66000E-001 1.00000E+001 IT 4.80000E-001 9.76000E-001 1.00000E+001 IT 5.00000E-001 9.82000E-001 1.00000E+001 IT 5.50000E-001 9.93000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.89000E-001 1.00000E+001 IT 7.00000E-001 9.92000E-001 1.00000E+001 IT 7.50000E-001 9.94000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.95000E-001 1.00000E+001 IT 8.30000E-001 9.95000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM FD225 1 808228 1.80809 22.76 0 1 1 GC Recommended glass type ED 9.600000000E+000 1.180000000E+001 3.320000000E+000 2.130000000E-002 0 0 CD 3.118986900E+000 -1.582077200E-002 4.442502400E-002 3.583488200E-003 -2.394344900E-004 3.875654200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.090000000E-005 4.100000000E-009 -1.040000000E-011 1.010000000E-006 1.330000000E-009 3.070000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 4.80000E-002 1.00000E+001 IT 3.80000E-001 3.97000E-001 1.00000E+001 IT 3.90000E-001 7.53000E-001 1.00000E+001 IT 4.00000E-001 8.90000E-001 1.00000E+001 IT 4.20000E-001 9.53000E-001 1.00000E+001 IT 4.40000E-001 9.67000E-001 1.00000E+001 IT 4.60000E-001 9.75000E-001 1.00000E+001 IT 4.80000E-001 9.81000E-001 1.00000E+001 IT 5.00000E-001 9.84000E-001 1.00000E+001 IT 5.50000E-001 9.92000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.90000E-001 1.00000E+001 IT 1.55000E+000 9.90000E-001 1.00000E+001 NM E-FDS1-W 1 923209 1.92286 20.88 0 1 1 GC Recommended glass type ED 6.000000000E+000 7.500000000E+000 3.940000000E+000 2.820000000E-002 0 0 CD 3.504463900E+000 -2.033383300E-002 5.380270000E-002 6.287419200E-003 -5.692217600E-004 7.355938700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -4.370000000E-006 1.100000000E-008 -2.290000000E-011 1.060000000E-006 1.516000000E-009 3.110000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.80000E-001 3.90000E-002 1.00000E+001 IT 3.90000E-001 3.53000E-001 1.00000E+001 IT 4.00000E-001 7.10000E-001 1.00000E+001 IT 4.20000E-001 9.26000E-001 1.00000E+001 IT 4.40000E-001 9.63000E-001 1.00000E+001 IT 4.60000E-001 9.76000E-001 1.00000E+001 IT 4.80000E-001 9.83000E-001 1.00000E+001 IT 5.00000E-001 9.89000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.83000E-001 1.00000E+001 IT 1.55000E+000 9.85000E-001 1.00000E+001 NM E-FDS1 1 923209 1.92286 20.88 0 0 4 GC General glass Type ED 6.000000000E+000 7.500000000E+000 3.940000000E+000 2.820000000E-002 0 0 CD 3.504463900E+000 -2.033383300E-002 5.380270000E-002 6.287419200E-003 -5.692217600E-004 7.355938700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -4.370000000E-006 1.100000000E-008 -2.290000000E-011 1.060000000E-006 1.516000000E-009 3.110000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.90000E-001 1.22000E-001 1.00000E+001 IT 4.00000E-001 3.76000E-001 1.00000E+001 IT 4.20000E-001 7.37000E-001 1.00000E+001 IT 4.40000E-001 8.68000E-001 1.00000E+001 IT 4.60000E-001 9.19000E-001 1.00000E+001 IT 4.80000E-001 9.44000E-001 1.00000E+001 IT 5.00000E-001 9.60000E-001 1.00000E+001 IT 5.50000E-001 9.83000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM E-FDS2 1 003193 2.00272 19.32 0 1 1 GC Recommended glass type ED 7.900000000E+000 1.010000000E+001 5.080000000E+000 3.150000000E-002 0 0 CD 3.767260300E+000 -1.700122700E-002 6.984963400E-002 6.386289200E-003 -5.081253900E-004 8.445552900E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.170000000E-007 1.140000000E-008 -3.070000000E-011 1.840000000E-006 2.480000000E-009 3.080000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.00000E-001 3.20000E-002 1.00000E+001 IT 4.20000E-001 4.57000E-001 1.00000E+001 IT 4.40000E-001 7.74000E-001 1.00000E+001 IT 4.60000E-001 8.84000E-001 1.00000E+001 IT 4.80000E-001 9.28000E-001 1.00000E+001 IT 5.00000E-001 9.54000E-001 1.00000E+001 IT 5.50000E-001 9.84000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.92000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-FDS3 1 104170 2.10420 17.02 0 0 4 GC General glass Type ED 6.800000000E+000 8.200000000E+000 5.630000000E+000 4.550000000E-002 0 0 CD 4.112038700E+000 -1.822767000E-002 8.985210500E-002 7.871440000E-003 -5.222800800E-004 1.177306100E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.980000000E-006 1.440000000E-008 -3.950000000E-011 2.170000000E-006 2.050000000E-009 3.020000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.20000E-001 8.10000E-002 1.00000E+001 IT 4.40000E-001 5.70000E-001 1.00000E+001 IT 4.60000E-001 8.14000E-001 1.00000E+001 IT 4.80000E-001 8.91000E-001 1.00000E+001 IT 5.00000E-001 9.25000E-001 1.00000E+001 IT 5.50000E-001 9.65000E-001 1.00000E+001 IT 6.00000E-001 9.82000E-001 1.00000E+001 IT 6.50000E-001 9.88000E-001 1.00000E+001 IT 7.00000E-001 9.92000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.94000E-001 1.00000E+001 IT 8.00000E-001 9.94000E-001 1.00000E+001 IT 8.30000E-001 9.95000E-001 1.00000E+001 IT 8.50000E-001 9.95000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM FDS16-W 1 986165 1.98612 16.48 0 1 1 GC Recommended glass type ED 4.100000000E+000 5.400000000E+000 3.540000000E+000 4.700000000E-002 0 0 CD 3.690609800E+000 -2.784902400E-002 6.313905100E-002 1.244369800E-002 -1.477408500E-003 1.747870100E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.970000000E-006 1.370000000E-008 -4.940000000E-011 1.360000000E-006 1.860000000E-009 3.330000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.00000E-001 1.70000E-002 1.00000E+001 IT 4.20000E-001 5.99000E-001 1.00000E+001 IT 4.40000E-001 8.77000E-001 1.00000E+001 IT 4.60000E-001 9.28000E-001 1.00000E+001 IT 4.80000E-001 9.48000E-001 1.00000E+001 IT 5.00000E-001 9.62000E-001 1.00000E+001 IT 5.50000E-001 9.84000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.82000E-001 1.00000E+001 IT 1.55000E+000 9.85000E-001 1.00000E+001 NM FDS18-W 1 946180 1.94595 17.98 0 1 1 GC Recommended glass type ED 5.700000000E+000 7.100000000E+000 3.510000000E+000 3.860000000E-002 0 0 CD 3.563784000E+000 -2.544964400E-002 5.840165900E-002 9.231098300E-003 -9.549972700E-004 1.177745600E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.609840000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.90000E-001 4.60000E-002 1.00000E+001 IT 4.00000E-001 3.60000E-001 1.00000E+001 IT 4.20000E-001 8.63000E-001 1.00000E+001 IT 4.40000E-001 9.43000E-001 1.00000E+001 IT 4.60000E-001 9.63000E-001 1.00000E+001 IT 4.80000E-001 9.74000E-001 1.00000E+001 IT 5.00000E-001 9.80000E-001 1.00000E+001 IT 5.50000E-001 9.91000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.82000E-001 1.00000E+001 IT 1.55000E+000 9.85000E-001 1.00000E+001 NM FDS18 1 946180 1.94595 17.98 0 0 4 GC General glass Type ED 5.700000000E+000 7.100000000E+000 3.510000000E+000 3.860000000E-002 0 0 CD 3.563784000E+000 -2.544964400E-002 5.840165900E-002 9.231098300E-003 -9.549972700E-004 1.177745600E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.609840000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.00000E-001 7.40000E-002 1.00000E+001 IT 4.20000E-001 4.91000E-001 1.00000E+001 IT 4.40000E-001 7.43000E-001 1.00000E+001 IT 4.60000E-001 8.45000E-001 1.00000E+001 IT 4.80000E-001 8.94000E-001 1.00000E+001 IT 5.00000E-001 9.23000E-001 1.00000E+001 IT 5.50000E-001 9.66000E-001 1.00000E+001 IT 6.00000E-001 9.82000E-001 1.00000E+001 IT 6.50000E-001 9.87000E-001 1.00000E+001 IT 7.00000E-001 9.92000E-001 1.00000E+001 IT 7.50000E-001 9.94000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.93000E-001 1.00000E+001 IT 1.00000E+000 9.92000E-001 1.00000E+001 IT 1.05000E+000 9.90000E-001 1.00000E+001 IT 1.06000E+000 9.90000E-001 1.00000E+001 IT 1.10000E+000 9.90000E-001 1.00000E+001 IT 1.20000E+000 9.88000E-001 1.00000E+001 IT 1.30000E+000 9.86000E-001 1.00000E+001 IT 1.40000E+000 9.82000E-001 1.00000E+001 IT 1.50000E+000 9.79000E-001 1.00000E+001 IT 1.55000E+000 9.80000E-001 1.00000E+001 NM FDS24 1 921240 1.92119 23.96 0 1 2 GC Recommended glass type ED 7.800000000E+000 9.600000000E+000 3.840000000E+000 1.510000000E-002 0 0 CD 3.512632700E+000 -1.530150000E-002 5.393606100E-002 3.494936900E-003 -1.795029500E-004 3.440318100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -3.370000000E-006 7.780000000E-009 -2.330000000E-011 1.130000000E-006 1.320000000E-009 2.750000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 6.90000E-002 1.00000E+001 IT 3.80000E-001 3.01000E-001 1.00000E+001 IT 3.90000E-001 5.21000E-001 1.00000E+001 IT 4.00000E-001 6.57000E-001 1.00000E+001 IT 4.20000E-001 8.06000E-001 1.00000E+001 IT 4.40000E-001 8.81000E-001 1.00000E+001 IT 4.60000E-001 9.20000E-001 1.00000E+001 IT 4.80000E-001 9.42000E-001 1.00000E+001 IT 5.00000E-001 9.58000E-001 1.00000E+001 IT 5.50000E-001 9.83000E-001 1.00000E+001 IT 6.00000E-001 9.89000E-001 1.00000E+001 IT 6.50000E-001 9.89000E-001 1.00000E+001 IT 7.00000E-001 9.92000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM FDS90-SG 1 847238 1.84666 23.78 0 1 1 GC Recommended glass type ED 8.700000000E+000 1.070000000E+001 3.500000000E+000 1.370000000E-002 0 0 CD 3.260632100E+000 -1.778039800E-002 4.090293800E-002 5.607693400E-003 -5.643403900E-004 5.476339100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -4.620000000E-006 1.290000000E-008 -2.110000000E-011 1.040000000E-006 1.270000000E-009 2.960000000E-001 2.000000000E+001 OD -1.00000 2.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.21000E-001 1.00000E+001 IT 3.80000E-001 4.15000E-001 1.00000E+001 IT 3.90000E-001 6.86000E-001 1.00000E+001 IT 4.00000E-001 8.25000E-001 1.00000E+001 IT 4.20000E-001 9.21000E-001 1.00000E+001 IT 4.40000E-001 9.52000E-001 1.00000E+001 IT 4.60000E-001 9.66000E-001 1.00000E+001 IT 4.80000E-001 9.75000E-001 1.00000E+001 IT 5.00000E-001 9.83000E-001 1.00000E+001 IT 5.50000E-001 9.95000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.93000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM FDS90 1 847238 1.84666 23.78 0 0 4 GC General glass Type ED 8.700000000E+000 1.070000000E+001 3.500000000E+000 1.370000000E-002 0 0 CD 3.260632100E+000 -1.778039800E-002 4.090293800E-002 5.607693400E-003 -5.643403900E-004 5.476339100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -4.620000000E-006 1.290000000E-008 -2.110000000E-011 1.040000000E-006 1.270000000E-009 2.960000000E-001 2.000000000E+001 OD -1.00000 2.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 8.90000E-002 1.00000E+001 IT 3.80000E-001 3.93000E-001 1.00000E+001 IT 3.90000E-001 6.53000E-001 1.00000E+001 IT 4.00000E-001 7.86000E-001 1.00000E+001 IT 4.20000E-001 8.95000E-001 1.00000E+001 IT 4.40000E-001 9.37000E-001 1.00000E+001 IT 4.60000E-001 9.54000E-001 1.00000E+001 IT 4.80000E-001 9.68000E-001 1.00000E+001 IT 5.00000E-001 9.77000E-001 1.00000E+001 IT 5.50000E-001 9.90000E-001 1.00000E+001 IT 6.00000E-001 9.91000E-001 1.00000E+001 IT 6.50000E-001 9.88000E-001 1.00000E+001 IT 7.00000E-001 9.92000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM FDS90(P) 1 847239 1.84666 23.88 0 0 4 GC General glass Type ED 8.700000000E+000 1.070000000E+001 3.500000000E+000 1.370000000E-002 0 0 CD 3.256561900E+000 -1.580396500E-002 4.433032200E-002 4.362009800E-003 -3.691226100E-004 4.299968200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -4.620000000E-006 1.290000000E-008 -2.110000000E-011 1.040000000E-006 1.270000000E-009 2.960000000E-001 2.000000000E+001 OD -1.00000 2.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 8.90000E-002 1.00000E+001 IT 3.80000E-001 3.93000E-001 1.00000E+001 IT 3.90000E-001 6.53000E-001 1.00000E+001 IT 4.00000E-001 7.86000E-001 1.00000E+001 IT 4.20000E-001 8.95000E-001 1.00000E+001 IT 4.40000E-001 9.37000E-001 1.00000E+001 IT 4.60000E-001 9.54000E-001 1.00000E+001 IT 4.80000E-001 9.68000E-001 1.00000E+001 IT 5.00000E-001 9.77000E-001 1.00000E+001 IT 5.50000E-001 9.90000E-001 1.00000E+001 IT 6.00000E-001 9.91000E-001 1.00000E+001 IT 6.50000E-001 9.88000E-001 1.00000E+001 IT 7.00000E-001 9.92000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM FF5 1 593354 1.59270 35.44 0 0 4 GC General glass Type ED 8.600000000E+000 1.020000000E+001 2.640000000E+000 8.100000000E-003 0 0 CD 2.474332400E+000 -1.095533800E-002 1.929380100E-002 1.449773200E-003 -1.103874400E-004 1.113600800E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.236660000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 4.20000E-002 1.00000E+001 IT 3.60000E-001 3.72000E-001 1.00000E+001 IT 3.70000E-001 7.21000E-001 1.00000E+001 IT 3.80000E-001 8.78000E-001 1.00000E+001 IT 3.90000E-001 9.39000E-001 1.00000E+001 IT 4.00000E-001 9.64000E-001 1.00000E+001 IT 4.20000E-001 9.82000E-001 1.00000E+001 IT 4.40000E-001 9.88000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 NM FF8 1 752251 1.75211 25.05 0 0 4 GC General glass Type ED 6.100000000E+000 7.000000000E+000 3.140000000E+000 1.590000000E-002 0 0 CD 2.956436100E+000 -1.976219500E-002 2.987882300E-002 5.183085200E-003 -5.420238900E-004 4.846324500E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -3.670000000E-006 1.100000000E-008 -3.230000000E-011 7.570000000E-007 9.890000000E-010 3.060000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 3.00000E-002 1.00000E+001 IT 3.70000E-001 2.62000E-001 1.00000E+001 IT 3.80000E-001 5.66000E-001 1.00000E+001 IT 3.90000E-001 7.48000E-001 1.00000E+001 IT 4.00000E-001 8.46000E-001 1.00000E+001 IT 4.20000E-001 9.32000E-001 1.00000E+001 IT 4.40000E-001 9.60000E-001 1.00000E+001 IT 4.60000E-001 9.75000E-001 1.00000E+001 IT 4.80000E-001 9.81000E-001 1.00000E+001 IT 5.00000E-001 9.87000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.80000E-001 1.00000E+001 IT 1.50000E+000 9.82000E-001 1.00000E+001 IT 1.55000E+000 9.84000E-001 1.00000E+001 NM BAFD7 1 702412 1.70154 41.15 0 0 4 GC General glass Type ED 6.800000000E+000 8.400000000E+000 3.650000000E+000 2.800000000E-003 0 0 CD 2.821721100E+000 -9.726548300E-003 2.434597900E-002 7.840630500E-004 -2.243149700E-005 4.672602900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 6.075320000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 6.40000E-002 1.00000E+001 IT 3.60000E-001 3.51000E-001 1.00000E+001 IT 3.70000E-001 6.36000E-001 1.00000E+001 IT 3.80000E-001 7.99000E-001 1.00000E+001 IT 3.90000E-001 8.82000E-001 1.00000E+001 IT 4.00000E-001 9.24000E-001 1.00000E+001 IT 4.20000E-001 9.62000E-001 1.00000E+001 IT 4.40000E-001 9.75000E-001 1.00000E+001 IT 4.60000E-001 9.82000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM BAFD8 1 723380 1.72342 37.99 0 0 4 GC General glass Type ED 7.100000000E+000 8.600000000E+000 3.620000000E+000 2.100000000E-003 0 0 CD 2.886323600E+000 -9.802724000E-003 2.765425600E-002 8.900636700E-004 -3.630910900E-005 7.618106200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.569080000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 8.40000E-002 1.00000E+001 IT 3.70000E-001 3.22000E-001 1.00000E+001 IT 3.80000E-001 5.73000E-001 1.00000E+001 IT 3.90000E-001 7.47000E-001 1.00000E+001 IT 4.00000E-001 8.54000E-001 1.00000E+001 IT 4.20000E-001 9.45000E-001 1.00000E+001 IT 4.40000E-001 9.74000E-001 1.00000E+001 IT 4.60000E-001 9.84000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM LAF2 1 744449 1.74400 44.90 0 0 4 GC General glass Type ED 7.200000000E+000 8.700000000E+000 4.390000000E+000 -4.400000000E-003 0 0 CD 2.965737400E+000 -9.657162400E-003 2.602452500E-002 3.668464100E-004 2.820555100E-005 -1.373992900E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.211190000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 5.20000E-002 1.00000E+001 IT 3.30000E-001 2.19000E-001 1.00000E+001 IT 3.40000E-001 4.50000E-001 1.00000E+001 IT 3.50000E-001 6.55000E-001 1.00000E+001 IT 3.60000E-001 8.01000E-001 1.00000E+001 IT 3.70000E-001 8.95000E-001 1.00000E+001 IT 3.80000E-001 9.40000E-001 1.00000E+001 IT 3.90000E-001 9.65000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.85000E-001 1.00000E+001 IT 4.40000E-001 9.87000E-001 1.00000E+001 IT 4.60000E-001 9.90000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM LAF3 1 717480 1.71700 47.98 0 0 4 GC General glass Type ED 8.000000000E+000 9.300000000E+000 4.200000000E+000 -6.300000000E-003 0 0 CD 2.878979900E+000 -8.729237000E-003 2.442565600E-002 4.549177300E-005 4.280292800E-005 -7.283430600E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.755380000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 2.00000E-002 1.00000E+001 IT 3.30000E-001 1.90000E-001 1.00000E+001 IT 3.40000E-001 4.60000E-001 1.00000E+001 IT 3.50000E-001 6.80000E-001 1.00000E+001 IT 3.60000E-001 8.20000E-001 1.00000E+001 IT 3.70000E-001 9.00000E-001 1.00000E+001 IT 3.80000E-001 9.43000E-001 1.00000E+001 IT 3.90000E-001 9.65000E-001 1.00000E+001 IT 4.00000E-001 9.75000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.87000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM NBF1 1 743492 1.74330 49.22 0 0 4 GC General glass Type ED 5.300000000E+000 6.800000000E+000 4.170000000E+000 -1.030000000E-002 0 0 CD 2.975349100E+000 -1.461347000E-002 2.109638300E-002 1.198038000E-003 -1.188738800E-004 7.344435000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.089870000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 6.80000E-002 1.00000E+001 IT 3.10000E-001 2.54000E-001 1.00000E+001 IT 3.20000E-001 4.72000E-001 1.00000E+001 IT 3.30000E-001 6.37000E-001 1.00000E+001 IT 3.40000E-001 7.55000E-001 1.00000E+001 IT 3.50000E-001 8.41000E-001 1.00000E+001 IT 3.60000E-001 9.02000E-001 1.00000E+001 IT 3.70000E-001 9.43000E-001 1.00000E+001 IT 3.80000E-001 9.64000E-001 1.00000E+001 IT 3.90000E-001 9.77000E-001 1.00000E+001 IT 4.00000E-001 9.84000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.89000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM NBFD3 1 805396 1.80450 39.63 0 0 4 GC General glass Type ED 5.300000000E+000 7.000000000E+000 4.390000000E+000 -5.600000000E-003 0 0 CD 3.163374600E+000 -1.327628000E-002 3.113330900E-002 8.352338000E-004 2.998049900E-006 2.556885300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.161840000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 3.00000 5.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.54000E-001 1.00000E+001 IT 3.60000E-001 4.97000E-001 1.00000E+001 IT 3.70000E-001 7.35000E-001 1.00000E+001 IT 3.80000E-001 8.50000E-001 1.00000E+001 IT 3.90000E-001 9.06000E-001 1.00000E+001 IT 4.00000E-001 9.40000E-001 1.00000E+001 IT 4.20000E-001 9.66000E-001 1.00000E+001 IT 4.40000E-001 9.78000E-001 1.00000E+001 IT 4.60000E-001 9.85000E-001 1.00000E+001 IT 4.80000E-001 9.89000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM NBFD10 1 834373 1.83400 37.34 0 1 2 GC Recommended glass type ED 5.900000000E+000 7.300000000E+000 4.570000000E+000 -2.100000000E-003 0 0 CD 3.261557300E+000 -1.454285100E-002 3.347073900E-002 1.226647900E-003 -2.539184200E-005 5.597173900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.466890000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 8.10000E-002 1.00000E+001 IT 3.60000E-001 3.28000E-001 1.00000E+001 IT 3.70000E-001 6.05000E-001 1.00000E+001 IT 3.80000E-001 7.71000E-001 1.00000E+001 IT 3.90000E-001 8.59000E-001 1.00000E+001 IT 4.00000E-001 9.06000E-001 1.00000E+001 IT 4.20000E-001 9.50000E-001 1.00000E+001 IT 4.40000E-001 9.69000E-001 1.00000E+001 IT 4.60000E-001 9.80000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM NBFD11 1 786439 1.78590 43.93 0 0 4 GC General glass Type ED 5.700000000E+000 7.100000000E+000 4.430000000E+000 -8.000000000E-003 0 0 CD 3.101026700E+000 -1.002210800E-002 3.263168700E-002 -8.102926800E-004 1.935011000E-004 -8.027979900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.088070000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 1.16000E-001 1.00000E+001 IT 3.30000E-001 3.96000E-001 1.00000E+001 IT 3.40000E-001 6.32000E-001 1.00000E+001 IT 3.50000E-001 7.76000E-001 1.00000E+001 IT 3.60000E-001 8.66000E-001 1.00000E+001 IT 3.70000E-001 9.19000E-001 1.00000E+001 IT 3.80000E-001 9.44000E-001 1.00000E+001 IT 3.90000E-001 9.64000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM NBFD13 1 806407 1.80610 40.73 0 1 2 GC Recommended glass type ED 5.700000000E+000 7.200000000E+000 4.380000000E+000 -7.800000000E-003 0 0 CD 3.172922300E+000 -1.424853400E-002 2.916811400E-002 1.342876000E-003 -9.617875300E-005 8.404255600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 6.674240000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 5.50000E-002 1.00000E+001 IT 3.50000E-001 2.85000E-001 1.00000E+001 IT 3.60000E-001 5.91000E-001 1.00000E+001 IT 3.70000E-001 7.68000E-001 1.00000E+001 IT 3.80000E-001 8.56000E-001 1.00000E+001 IT 3.90000E-001 9.08000E-001 1.00000E+001 IT 4.00000E-001 9.36000E-001 1.00000E+001 IT 4.20000E-001 9.63000E-001 1.00000E+001 IT 4.40000E-001 9.74000E-001 1.00000E+001 IT 4.60000E-001 9.83000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM NBFD15-W 1 806333 1.80610 33.27 0 1 2 GC Recommended glass type ED 7.100000000E+000 9.100000000E+000 3.470000000E+000 0.000000000E+000 0 0 CD 3.154001100E+000 -1.325675300E-002 3.410331200E-002 1.847216700E-003 -1.080733200E-004 1.297590100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.020000000E-006 7.390000000E-009 -1.850000000E-011 7.780000000E-007 6.810000000E-010 2.680000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 3.50000E-002 1.00000E+001 IT 3.60000E-001 3.10000E-001 1.00000E+001 IT 3.70000E-001 6.43000E-001 1.00000E+001 IT 3.80000E-001 8.25000E-001 1.00000E+001 IT 3.90000E-001 9.00000E-001 1.00000E+001 IT 4.00000E-001 9.43000E-001 1.00000E+001 IT 4.20000E-001 9.68000E-001 1.00000E+001 IT 4.40000E-001 9.78000E-001 1.00000E+001 IT 4.60000E-001 9.82000E-001 1.00000E+001 IT 4.80000E-001 9.85000E-001 1.00000E+001 IT 5.00000E-001 9.88000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM NBFD15 1 806333 1.80610 33.27 0 0 4 GC General glass Type ED 7.100000000E+000 9.100000000E+000 3.470000000E+000 0.000000000E+000 0 0 CD 3.154001100E+000 -1.325675300E-002 3.410331200E-002 1.847216700E-003 -1.080733200E-004 1.297590100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.020000000E-006 7.390000000E-009 -1.850000000E-011 7.780000000E-007 6.810000000E-010 2.680000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 2.90000E-002 1.00000E+001 IT 3.60000E-001 2.74000E-001 1.00000E+001 IT 3.70000E-001 6.02000E-001 1.00000E+001 IT 3.80000E-001 7.84000E-001 1.00000E+001 IT 3.90000E-001 8.71000E-001 1.00000E+001 IT 4.00000E-001 9.14000E-001 1.00000E+001 IT 4.20000E-001 9.49000E-001 1.00000E+001 IT 4.40000E-001 9.64000E-001 1.00000E+001 IT 4.60000E-001 9.72000E-001 1.00000E+001 IT 4.80000E-001 9.81000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM TAF1 1 773496 1.77250 49.62 0 1 2 GC Recommended glass type ED 5.600000000E+000 7.300000000E+000 4.280000000E+000 -8.600000000E-003 0 0 CD 3.073637800E+000 -1.550128400E-002 2.362769900E-002 6.630085200E-004 -2.835343800E-005 2.209079900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.760000000E-006 9.560000000E-009 -3.120000000E-011 5.100000000E-007 3.460000000E-010 2.160000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 2.70000E-002 1.00000E+001 IT 3.10000E-001 1.89000E-001 1.00000E+001 IT 3.20000E-001 4.29000E-001 1.00000E+001 IT 3.30000E-001 6.04000E-001 1.00000E+001 IT 3.40000E-001 7.36000E-001 1.00000E+001 IT 3.50000E-001 8.35000E-001 1.00000E+001 IT 3.60000E-001 9.00000E-001 1.00000E+001 IT 3.70000E-001 9.34000E-001 1.00000E+001 IT 3.80000E-001 9.67000E-001 1.00000E+001 IT 3.90000E-001 9.77000E-001 1.00000E+001 IT 4.00000E-001 9.83000E-001 1.00000E+001 IT 4.20000E-001 9.89000E-001 1.00000E+001 IT 4.40000E-001 9.94000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM TAF3D 1 804465 1.80420 46.50 0 1 2 GC Recommended glass type ED 6.100000000E+000 7.600000000E+000 4.400000000E+000 -7.300000000E-003 0 0 CD 3.175337000E+000 -1.410760100E-002 2.786090000E-002 4.010282400E-004 2.450476400E-005 2.443573100E-008 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.820000000E-006 8.490000000E-009 -3.350000000E-011 6.910000000E-007 6.180000000E-010 1.560000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 8.50000E-002 1.00000E+001 IT 3.30000E-001 3.24000E-001 1.00000E+001 IT 3.40000E-001 5.70000E-001 1.00000E+001 IT 3.50000E-001 7.37000E-001 1.00000E+001 IT 3.60000E-001 8.46000E-001 1.00000E+001 IT 3.70000E-001 9.07000E-001 1.00000E+001 IT 3.80000E-001 9.42000E-001 1.00000E+001 IT 3.90000E-001 9.63000E-001 1.00000E+001 IT 4.00000E-001 9.75000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM TAF3 1 804465 1.80420 46.50 0 0 4 GC General glass Type ED 5.900000000E+000 7.500000000E+000 4.650000000E+000 -6.600000000E-003 0 0 CD 3.174370700E+000 -1.411046600E-002 2.886263700E-002 3.355949000E-005 8.042210900E-005 -2.895674400E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.150000000E-006 9.330000000E-009 -4.330000000E-011 5.570000000E-007 5.720000000E-010 2.090000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 9.80000E-002 1.00000E+001 IT 3.30000E-001 3.55000E-001 1.00000E+001 IT 3.40000E-001 5.93000E-001 1.00000E+001 IT 3.50000E-001 7.50000E-001 1.00000E+001 IT 3.60000E-001 8.43000E-001 1.00000E+001 IT 3.70000E-001 9.06000E-001 1.00000E+001 IT 3.80000E-001 9.42000E-001 1.00000E+001 IT 3.90000E-001 9.59000E-001 1.00000E+001 IT 4.00000E-001 9.70000E-001 1.00000E+001 IT 4.20000E-001 9.82000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM TAFD5G 1 835427 1.83481 42.72 0 1 1 GC Recommended glass type ED 6.300000000E+000 7.800000000E+000 4.570000000E+000 -6.500000000E-003 0 0 CD 3.275679900E+000 -1.448562500E-002 3.078010200E-002 7.891551500E-004 -4.081022900E-006 2.227396500E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.220000000E-006 9.370000000E-009 -5.940000000E-011 8.370000000E-007 7.860000000E-010 1.570000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 3.40000E-002 1.00000E+001 IT 3.30000E-001 2.17000E-001 1.00000E+001 IT 3.40000E-001 4.65000E-001 1.00000E+001 IT 3.50000E-001 6.54000E-001 1.00000E+001 IT 3.60000E-001 7.84000E-001 1.00000E+001 IT 3.70000E-001 8.60000E-001 1.00000E+001 IT 3.80000E-001 9.08000E-001 1.00000E+001 IT 3.90000E-001 9.38000E-001 1.00000E+001 IT 4.00000E-001 9.55000E-001 1.00000E+001 IT 4.20000E-001 9.73000E-001 1.00000E+001 IT 4.40000E-001 9.82000E-001 1.00000E+001 IT 4.60000E-001 9.87000E-001 1.00000E+001 IT 4.80000E-001 9.91000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM TAFD5F 1 835427 1.83481 42.72 0 0 4 GC General glass Type ED 6.200000000E+000 7.800000000E+000 4.720000000E+000 -6.200000000E-003 0 0 CD 3.275546000E+000 -1.447035400E-002 3.092206200E-002 7.328998100E-004 4.657330700E-006 1.824274600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.790000000E-006 8.810000000E-009 -2.500000000E-011 7.250000000E-007 7.240000000E-010 1.970000000E-001 2.000000000E+001 OD -1.00000 2.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 2.00000E-002 1.00000E+001 IT 3.30000E-001 1.89000E-001 1.00000E+001 IT 3.40000E-001 4.59000E-001 1.00000E+001 IT 3.50000E-001 6.75000E-001 1.00000E+001 IT 3.60000E-001 7.96000E-001 1.00000E+001 IT 3.70000E-001 8.77000E-001 1.00000E+001 IT 3.80000E-001 9.22000E-001 1.00000E+001 IT 3.90000E-001 9.44000E-001 1.00000E+001 IT 4.00000E-001 9.65000E-001 1.00000E+001 IT 4.20000E-001 9.78000E-001 1.00000E+001 IT 4.40000E-001 9.87000E-001 1.00000E+001 IT 4.60000E-001 9.88000E-001 1.00000E+001 IT 4.80000E-001 9.93000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM TAFD25 1 904313 1.90366 31.32 0 1 1 GC Recommended glass type ED 7.000000000E+000 8.800000000E+000 4.510000000E+000 2.800000000E-003 0 0 CD 3.490552800E+000 -1.632577100E-002 4.114632200E-002 2.716912400E-003 -1.826051800E-004 2.064186200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.770000000E-007 7.510000000E-009 -2.950000000E-011 1.020000000E-006 9.450000000E-010 2.450000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 6.90000E-002 1.00000E+001 IT 3.70000E-001 3.52000E-001 1.00000E+001 IT 3.80000E-001 6.19000E-001 1.00000E+001 IT 3.90000E-001 7.75000E-001 1.00000E+001 IT 4.00000E-001 8.54000E-001 1.00000E+001 IT 4.20000E-001 9.26000E-001 1.00000E+001 IT 4.40000E-001 9.55000E-001 1.00000E+001 IT 4.60000E-001 9.69000E-001 1.00000E+001 IT 4.80000E-001 9.80000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM TAFD30 1 883408 1.88300 40.80 0 1 1 GC Recommended glass type ED 6.500000000E+000 8.200000000E+000 5.420000000E+000 -9.400000000E-003 0 0 CD 3.441903800E+000 -1.417524500E-002 3.435104000E-002 1.175227100E-003 -3.901034300E-005 3.741705400E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.210000000E-006 9.960000000E-009 -3.190000000E-011 8.400000000E-007 2.810000000E-010 1.840000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.90000E-002 1.00000E+001 IT 3.20000E-001 1.83000E-001 1.00000E+001 IT 3.30000E-001 3.70000E-001 1.00000E+001 IT 3.40000E-001 5.37000E-001 1.00000E+001 IT 3.50000E-001 6.72000E-001 1.00000E+001 IT 3.60000E-001 7.81000E-001 1.00000E+001 IT 3.70000E-001 8.60000E-001 1.00000E+001 IT 3.80000E-001 9.06000E-001 1.00000E+001 IT 3.90000E-001 9.35000E-001 1.00000E+001 IT 4.00000E-001 9.53000E-001 1.00000E+001 IT 4.20000E-001 9.71000E-001 1.00000E+001 IT 4.40000E-001 9.80000E-001 1.00000E+001 IT 4.60000E-001 9.87000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM TAFD32 1 871407 1.87070 40.73 0 1 1 GC Recommended glass type ED 6.800000000E+000 8.400000000E+000 4.840000000E+000 -6.700000000E-003 0 0 CD 3.396108000E+000 -1.308706500E-002 3.485351600E-002 7.908317700E-004 7.699521200E-006 2.351674200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.820000000E-007 8.110000000E-009 -2.840000000E-011 9.600000000E-007 9.610000000E-010 1.410000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 1.60000E-002 1.00000E+001 IT 3.30000E-001 1.39000E-001 1.00000E+001 IT 3.40000E-001 3.60000E-001 1.00000E+001 IT 3.50000E-001 5.53000E-001 1.00000E+001 IT 3.60000E-001 7.04000E-001 1.00000E+001 IT 3.70000E-001 8.00000E-001 1.00000E+001 IT 3.80000E-001 8.64000E-001 1.00000E+001 IT 3.90000E-001 9.06000E-001 1.00000E+001 IT 4.00000E-001 9.32000E-001 1.00000E+001 IT 4.20000E-001 9.58000E-001 1.00000E+001 IT 4.40000E-001 9.71000E-001 1.00000E+001 IT 4.60000E-001 9.79000E-001 1.00000E+001 IT 4.80000E-001 9.86000E-001 1.00000E+001 IT 5.00000E-001 9.90000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM TAFD33 1 881401 1.88100 40.14 0 1 2 GC Recommended glass type ED 6.800000000E+000 8.300000000E+000 5.400000000E+000 -5.900000000E-003 0 0 CD 3.431695500E+000 -1.315627300E-002 3.563186200E-002 9.137810900E-004 -4.036688600E-006 3.386768800E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.040000000E-006 9.900000000E-009 -5.860000000E-011 9.550000000E-007 8.810000000E-010 1.590000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 1.70000E-002 1.00000E+001 IT 3.50000E-001 1.71000E-001 1.00000E+001 IT 3.60000E-001 4.64000E-001 1.00000E+001 IT 3.70000E-001 6.72000E-001 1.00000E+001 IT 3.80000E-001 7.94000E-001 1.00000E+001 IT 3.90000E-001 8.64000E-001 1.00000E+001 IT 4.00000E-001 9.04000E-001 1.00000E+001 IT 4.20000E-001 9.43000E-001 1.00000E+001 IT 4.40000E-001 9.61000E-001 1.00000E+001 IT 4.60000E-001 9.72000E-001 1.00000E+001 IT 4.80000E-001 9.80000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.93000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM TAFD35 1 911353 1.91082 35.25 0 1 1 GC Recommended glass type ED 6.800000000E+000 8.200000000E+000 4.970000000E+000 -2.600000000E-003 0 0 CD 3.527474700E+000 -1.483994800E-002 3.974540200E-002 1.803472000E-003 -8.927933400E-005 1.137778300E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.960000000E-006 1.040000000E-008 -2.570000000E-011 8.880000000E-007 9.730000000E-010 2.390000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 3.00000E-002 1.00000E+001 IT 3.60000E-001 2.70000E-001 1.00000E+001 IT 3.70000E-001 5.50000E-001 1.00000E+001 IT 3.80000E-001 7.30000E-001 1.00000E+001 IT 3.90000E-001 8.20000E-001 1.00000E+001 IT 4.00000E-001 8.79000E-001 1.00000E+001 IT 4.20000E-001 9.31000E-001 1.00000E+001 IT 4.40000E-001 9.53000E-001 1.00000E+001 IT 4.60000E-001 9.66000E-001 1.00000E+001 IT 4.80000E-001 9.76000E-001 1.00000E+001 IT 5.00000E-001 9.84000E-001 1.00000E+001 IT 5.50000E-001 9.93000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.94000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.93000E-001 1.00000E+001 IT 1.20000E+000 9.92000E-001 1.00000E+001 IT 1.30000E+000 9.92000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.88000E-001 1.00000E+001 IT 1.55000E+000 9.89000E-001 1.00000E+001 NM TAFD37A 1 900374 1.90043 37.37 0 1 2 GC Recommended glass type ED 7.000000000E+000 8.500000000E+000 4.900000000E+000 -4.300000000E-003 0 0 CD 3.495812500E+000 -1.434235400E-002 3.780725100E-002 1.418407300E-003 -4.647026900E-005 6.919444000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 6.280000000E-007 8.140000000E-009 -5.080000000E-011 8.440000000E-007 7.600000000E-010 2.250000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.46000E-001 1.00000E+001 IT 3.60000E-001 3.96000E-001 1.00000E+001 IT 3.70000E-001 6.23000E-001 1.00000E+001 IT 3.80000E-001 7.50000E-001 1.00000E+001 IT 3.90000E-001 8.31000E-001 1.00000E+001 IT 4.00000E-001 8.80000E-001 1.00000E+001 IT 4.20000E-001 9.31000E-001 1.00000E+001 IT 4.40000E-001 9.54000E-001 1.00000E+001 IT 4.60000E-001 9.68000E-001 1.00000E+001 IT 4.80000E-001 9.77000E-001 1.00000E+001 IT 5.00000E-001 9.85000E-001 1.00000E+001 IT 5.50000E-001 9.94000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.90000E-001 1.00000E+001 IT 8.50000E-001 9.90000E-001 1.00000E+001 IT 9.00000E-001 9.88000E-001 1.00000E+001 IT 9.50000E-001 9.87000E-001 1.00000E+001 IT 1.00000E+000 9.87000E-001 1.00000E+001 IT 1.05000E+000 9.87000E-001 1.00000E+001 IT 1.06000E+000 9.86000E-001 1.00000E+001 IT 1.10000E+000 9.86000E-001 1.00000E+001 IT 1.20000E+000 9.85000E-001 1.00000E+001 IT 1.30000E+000 9.85000E-001 1.00000E+001 IT 1.40000E+000 9.84000E-001 1.00000E+001 IT 1.50000E+000 9.81000E-001 1.00000E+001 IT 1.55000E+000 9.81000E-001 1.00000E+001 NM TAFD37 1 900374 1.90043 37.37 0 0 4 GC General glass Type ED 7.000000000E+000 8.400000000E+000 5.190000000E+000 -3.800000000E-003 0 0 CD 3.494336900E+000 -1.364762400E-002 3.883317000E-002 1.113255500E-003 -7.402237000E-006 5.302775400E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.060000000E-006 9.550000000E-009 -8.390000000E-012 7.470000000E-007 7.080000000E-010 2.490000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 8.20000E-002 1.00000E+001 IT 3.60000E-001 3.64000E-001 1.00000E+001 IT 3.70000E-001 5.97000E-001 1.00000E+001 IT 3.80000E-001 7.45000E-001 1.00000E+001 IT 3.90000E-001 8.33000E-001 1.00000E+001 IT 4.00000E-001 8.84000E-001 1.00000E+001 IT 4.20000E-001 9.34000E-001 1.00000E+001 IT 4.40000E-001 9.55000E-001 1.00000E+001 IT 4.60000E-001 9.67000E-001 1.00000E+001 IT 4.80000E-001 9.77000E-001 1.00000E+001 IT 5.00000E-001 9.84000E-001 1.00000E+001 IT 5.50000E-001 9.92000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM TAFD40 1 001255 2.00069 25.46 0 1 1 GC Recommended glass type ED 7.200000000E+000 8.700000000E+000 4.730000000E+000 1.110000000E-002 0 0 CD 3.810623200E+000 -1.635156500E-002 5.880109700E-002 3.491902600E-003 -1.694811000E-004 3.256933300E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.530000000E-006 7.620000000E-009 -3.120000000E-011 1.080000000E-006 1.190000000E-009 2.870000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 3.90000E-002 1.00000E+001 IT 3.80000E-001 2.19000E-001 1.00000E+001 IT 3.90000E-001 4.41000E-001 1.00000E+001 IT 4.00000E-001 6.02000E-001 1.00000E+001 IT 4.20000E-001 7.82000E-001 1.00000E+001 IT 4.40000E-001 8.73000E-001 1.00000E+001 IT 4.60000E-001 9.19000E-001 1.00000E+001 IT 4.80000E-001 9.45000E-001 1.00000E+001 IT 5.00000E-001 9.62000E-001 1.00000E+001 IT 5.50000E-001 9.88000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM TAFD45 1 954323 1.95375 32.32 0 1 2 GC Recommended glass type ED 7.000000000E+000 8.500000000E+000 5.100000000E+000 0.000000000E+000 0 0 CD 3.672962000E+000 -1.518050000E-002 4.571870000E-002 2.186221000E-003 -9.937420000E-005 1.490466000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.360000000E-007 9.080000000E-009 -4.590000000E-011 9.610000000E-007 1.390000000E-009 2.460000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.58000E-001 1.00000E+001 IT 3.70000E-001 4.54000E-001 1.00000E+001 IT 3.80000E-001 6.68000E-001 1.00000E+001 IT 3.90000E-001 7.88000E-001 1.00000E+001 IT 4.00000E-001 8.57000E-001 1.00000E+001 IT 4.20000E-001 9.21000E-001 1.00000E+001 IT 4.40000E-001 9.50000E-001 1.00000E+001 IT 4.60000E-001 9.64000E-001 1.00000E+001 IT 4.80000E-001 9.77000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM TAFD55 1 001291 2.00100 29.13 0 1 1 GC Recommended glass type ED 7.300000000E+000 9.000000000E+000 5.120000000E+000 3.600000000E-003 0 0 CD 3.831757800E+000 -1.526639700E-002 5.457384300E-002 2.310934600E-003 -4.447620100E-005 1.614388700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -4.170000000E-007 8.970000000E-009 -4.730000000E-011 1.050000000E-006 8.820000000E-010 2.620000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 2.10000E-002 1.00000E+001 IT 3.70000E-001 1.91000E-001 1.00000E+001 IT 3.80000E-001 4.46000E-001 1.00000E+001 IT 3.90000E-001 6.33000E-001 1.00000E+001 IT 4.00000E-001 7.49000E-001 1.00000E+001 IT 4.20000E-001 8.70000E-001 1.00000E+001 IT 4.40000E-001 9.25000E-001 1.00000E+001 IT 4.60000E-001 9.50000E-001 1.00000E+001 IT 4.80000E-001 9.68000E-001 1.00000E+001 IT 5.00000E-001 9.81000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM TAFD65 1 051269 2.05090 26.94 0 1 1 GC Recommended glass type ED 7.300000000E+000 8.900000000E+000 5.270000000E+000 5.500000000E-003 0 0 CD 4.011320200E+000 -1.775200900E-002 5.856933000E-002 4.320093200E-003 -3.107084200E-004 3.748563800E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -6.690000000E-007 9.680000000E-009 -3.750000000E-011 1.140000000E-006 1.220000000E-009 2.640000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 8.70000E-002 1.00000E+001 IT 3.80000E-001 2.80000E-001 1.00000E+001 IT 3.90000E-001 4.69000E-001 1.00000E+001 IT 4.00000E-001 6.09000E-001 1.00000E+001 IT 4.20000E-001 7.81000E-001 1.00000E+001 IT 4.40000E-001 8.68000E-001 1.00000E+001 IT 4.60000E-001 9.13000E-001 1.00000E+001 IT 4.80000E-001 9.41000E-001 1.00000E+001 IT 5.00000E-001 9.62000E-001 1.00000E+001 IT 5.50000E-001 9.89000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM FCD10 1 457903 1.45650 90.27 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 1.340000000E+001 1.570000000E+001 3.600000000E+000 4.900000000E-002 0 0 CD 2.103249000E+000 -5.024798800E-003 6.532307700E-003 1.307840500E-004 -6.365207200E-006 1.925474500E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.866000000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.00000E-002 1.00000E+001 IT 2.90000E-001 1.00000E-001 1.00000E+001 IT 3.00000E-001 2.60000E-001 1.00000E+001 IT 3.10000E-001 4.70000E-001 1.00000E+001 IT 3.20000E-001 6.70000E-001 1.00000E+001 IT 3.30000E-001 8.20000E-001 1.00000E+001 IT 3.40000E-001 9.14000E-001 1.00000E+001 IT 3.50000E-001 9.60000E-001 1.00000E+001 IT 3.60000E-001 9.82000E-001 1.00000E+001 IT 3.70000E-001 9.92000E-001 1.00000E+001 IT 3.80000E-001 9.97000E-001 1.00000E+001 IT 3.90000E-001 9.98000E-001 1.00000E+001 IT 4.00000E-001 9.98000E-001 1.00000E+001 IT 4.20000E-001 9.96000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM FCD505 1 593686 1.59282 68.63 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 1.150000000E+001 1.400000000E+001 4.200000000E+000 1.940000000E-002 0 0 CD 2.502355000E+000 -7.208004200E-003 1.201274300E-002 3.492084200E-004 -2.472967600E-005 1.380156700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.880000000E-005 4.930000000E-009 5.590000000E-011 5.350000000E-007 4.250000000E-010 1.810000000E-008 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 4.50000E-002 1.00000E+001 IT 3.30000E-001 1.52000E-001 1.00000E+001 IT 3.40000E-001 3.42000E-001 1.00000E+001 IT 3.50000E-001 5.60000E-001 1.00000E+001 IT 3.60000E-001 7.50000E-001 1.00000E+001 IT 3.70000E-001 8.66000E-001 1.00000E+001 IT 3.80000E-001 9.30000E-001 1.00000E+001 IT 3.90000E-001 9.62000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.88000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM LBC3N 1 606637 1.60625 63.71 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 1.240000000E+001 1.400000000E+001 3.840000000E+000 1.080000000E-002 0 0 CD 2.538848400E+000 -6.685586500E-003 1.511145600E-002 -1.524724100E-004 4.834011600E-005 -2.406178500E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.945620000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.20000E-002 1.00000E+001 IT 2.90000E-001 1.13000E-001 1.00000E+001 IT 3.00000E-001 2.36000E-001 1.00000E+001 IT 3.10000E-001 3.90000E-001 1.00000E+001 IT 3.20000E-001 5.50000E-001 1.00000E+001 IT 3.30000E-001 6.98000E-001 1.00000E+001 IT 3.40000E-001 8.10000E-001 1.00000E+001 IT 3.50000E-001 8.86000E-001 1.00000E+001 IT 3.60000E-001 9.39000E-001 1.00000E+001 IT 3.70000E-001 9.61000E-001 1.00000E+001 IT 3.80000E-001 9.71000E-001 1.00000E+001 IT 3.90000E-001 9.82000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.88000E-001 1.00000E+001 IT 4.40000E-001 9.88000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM BACD2 1 607567 1.60738 56.71 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.300000000E+000 7.200000000E+000 3.530000000E+000 2.000000000E-003 0 0 CD 2.539325500E+000 -8.720788300E-003 1.590956600E-002 8.816303600E-005 2.587659300E-005 -1.173352300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.258910000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.50000E-001 1.00000E+001 IT 3.20000E-001 2.70000E-001 1.00000E+001 IT 3.30000E-001 5.10000E-001 1.00000E+001 IT 3.40000E-001 7.00000E-001 1.00000E+001 IT 3.50000E-001 8.30000E-001 1.00000E+001 IT 3.60000E-001 9.08000E-001 1.00000E+001 IT 3.70000E-001 9.51000E-001 1.00000E+001 IT 3.80000E-001 9.69000E-001 1.00000E+001 IT 3.90000E-001 9.82000E-001 1.00000E+001 IT 4.00000E-001 9.87000E-001 1.00000E+001 IT 4.20000E-001 9.92000E-001 1.00000E+001 IT 4.40000E-001 9.94000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.88000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM BACD4 1 613586 1.61272 58.58 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.600000000E+000 7.700000000E+000 3.580000000E+000 1.900000000E-003 0 0 CD 2.558462100E+000 -9.745728300E-003 1.511049500E-002 2.327333300E-004 1.113724900E-006 1.642476700E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.409410000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 3.00000E-002 1.00000E+001 IT 3.10000E-001 1.30000E-001 1.00000E+001 IT 3.20000E-001 3.00000E-001 1.00000E+001 IT 3.30000E-001 5.10000E-001 1.00000E+001 IT 3.40000E-001 6.90000E-001 1.00000E+001 IT 3.50000E-001 8.20000E-001 1.00000E+001 IT 3.60000E-001 9.01000E-001 1.00000E+001 IT 3.70000E-001 9.46000E-001 1.00000E+001 IT 3.80000E-001 9.71000E-001 1.00000E+001 IT 3.90000E-001 9.83000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.96000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.84000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM BACD11 1 564608 1.56384 60.83 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 6.600000000E+000 7.800000000E+000 3.070000000E+000 2.000000000E-003 0 0 CD 2.409516300E+000 -9.190441500E-003 1.293996800E-002 2.346143000E-004 -1.113058900E-005 1.013186300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.665770000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.70000E-002 1.00000E+001 IT 2.90000E-001 9.70000E-002 1.00000E+001 IT 3.00000E-001 2.78000E-001 1.00000E+001 IT 3.10000E-001 5.16000E-001 1.00000E+001 IT 3.20000E-001 7.03000E-001 1.00000E+001 IT 3.30000E-001 8.34000E-001 1.00000E+001 IT 3.40000E-001 9.05000E-001 1.00000E+001 IT 3.50000E-001 9.44000E-001 1.00000E+001 IT 3.60000E-001 9.84000E-001 1.00000E+001 IT 3.70000E-001 9.85000E-001 1.00000E+001 IT 3.80000E-001 9.93000E-001 1.00000E+001 IT 3.90000E-001 9.95000E-001 1.00000E+001 IT 4.00000E-001 9.97000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.79000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM LAC7 1 652584 1.65160 58.40 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.900000000E+000 8.300000000E+000 3.620000000E+000 -3.500000000E-003 0 0 CD 2.687622300E+000 -1.437518700E-002 1.254595400E-002 1.464229500E-003 -1.698246100E-004 8.804863900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 9.525990000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 4.00000 -1.00000 5.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 1.00000E-002 1.00000E+001 IT 3.00000E-001 5.00000E-002 1.00000E+001 IT 3.10000E-001 1.20000E-001 1.00000E+001 IT 3.20000E-001 2.60000E-001 1.00000E+001 IT 3.30000E-001 4.30000E-001 1.00000E+001 IT 3.40000E-001 6.20000E-001 1.00000E+001 IT 3.50000E-001 7.50000E-001 1.00000E+001 IT 3.60000E-001 8.50000E-001 1.00000E+001 IT 3.70000E-001 9.15000E-001 1.00000E+001 IT 3.80000E-001 9.54000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.81000E-001 1.00000E+001 IT 4.20000E-001 9.89000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.89000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM LAC9 1 691547 1.69100 54.69 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.800000000E+000 7.300000000E+000 3.650000000E+000 -8.000000000E-003 0 0 CD 2.808152300E+000 -1.416788500E-002 1.769370700E-002 7.678875900E-004 -7.488617400E-005 4.704475600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 6.885960000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 -1.00000 5.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 8.00000E-002 1.00000E+001 IT 2.90000E-001 2.01000E-001 1.00000E+001 IT 3.00000E-001 3.03000E-001 1.00000E+001 IT 3.10000E-001 4.22000E-001 1.00000E+001 IT 3.20000E-001 5.52000E-001 1.00000E+001 IT 3.30000E-001 6.75000E-001 1.00000E+001 IT 3.40000E-001 7.80000E-001 1.00000E+001 IT 3.50000E-001 8.58000E-001 1.00000E+001 IT 3.60000E-001 9.17000E-001 1.00000E+001 IT 3.70000E-001 9.50000E-001 1.00000E+001 IT 3.80000E-001 9.70000E-001 1.00000E+001 IT 3.90000E-001 9.79000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.92000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM LAC10 1 720503 1.72000 50.34 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.400000000E+000 9.100000000E+000 3.870000000E+000 -7.500000000E-003 0 0 CD 2.895199800E+000 -1.170121800E-002 2.212648500E-002 3.849479100E-004 -7.980830200E-006 1.503511600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.449340000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 4.60000E-002 1.00000E+001 IT 3.10000E-001 2.42000E-001 1.00000E+001 IT 3.20000E-001 4.76000E-001 1.00000E+001 IT 3.30000E-001 6.50000E-001 1.00000E+001 IT 3.40000E-001 7.72000E-001 1.00000E+001 IT 3.50000E-001 8.58000E-001 1.00000E+001 IT 3.60000E-001 9.17000E-001 1.00000E+001 IT 3.70000E-001 9.50000E-001 1.00000E+001 IT 3.80000E-001 9.70000E-001 1.00000E+001 IT 3.90000E-001 9.79000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.94000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM LAC12 1 678555 1.67790 55.52 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.700000000E+000 9.000000000E+000 3.800000000E+000 -3.100000000E-003 0 0 CD 2.763484400E+000 -1.106833900E-002 1.824644200E-002 3.769735600E-004 -1.778865500E-005 1.531426200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.105120000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 5.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 1.00000E-002 1.00000E+001 IT 3.10000E-001 3.00000E-002 1.00000E+001 IT 3.20000E-001 9.00000E-002 1.00000E+001 IT 3.30000E-001 2.20000E-001 1.00000E+001 IT 3.40000E-001 4.10000E-001 1.00000E+001 IT 3.50000E-001 6.00000E-001 1.00000E+001 IT 3.60000E-001 7.60000E-001 1.00000E+001 IT 3.70000E-001 8.60000E-001 1.00000E+001 IT 3.80000E-001 9.17000E-001 1.00000E+001 IT 3.90000E-001 9.51000E-001 1.00000E+001 IT 4.00000E-001 9.80000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM LAC13 1 694533 1.69350 53.34 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.300000000E+000 6.800000000E+000 3.560000000E+000 -6.600000000E-003 0 0 CD 2.812531600E+000 -1.291527100E-002 1.996033900E-002 1.987788800E-004 1.764706100E-005 -4.476763200E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.225530000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 3.00000E-002 1.00000E+001 IT 3.10000E-001 1.60000E-001 1.00000E+001 IT 3.20000E-001 3.40000E-001 1.00000E+001 IT 3.30000E-001 5.20000E-001 1.00000E+001 IT 3.40000E-001 6.70000E-001 1.00000E+001 IT 3.50000E-001 7.90000E-001 1.00000E+001 IT 3.60000E-001 8.70000E-001 1.00000E+001 IT 3.70000E-001 9.21000E-001 1.00000E+001 IT 3.80000E-001 9.52000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.80000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.93000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.82000E-001 1.00000E+001 IT 1.50000E+000 9.86000E-001 1.00000E+001 IT 1.55000E+000 9.88000E-001 1.00000E+001 NM LACL60 1 640602 1.64000 60.20 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.000000000E+000 7.800000000E+000 3.020000000E+000 -3.900000000E-003 0 0 CD 2.649088400E+000 -1.415986900E-002 1.445113500E-002 5.270787300E-004 -4.344752300E-005 2.461297100E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.289070000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 5.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 8.00000E-002 1.00000E+001 IT 2.90000E-001 1.70000E-001 1.00000E+001 IT 3.00000E-001 2.90000E-001 1.00000E+001 IT 3.10000E-001 4.30000E-001 1.00000E+001 IT 3.20000E-001 5.70000E-001 1.00000E+001 IT 3.30000E-001 7.00000E-001 1.00000E+001 IT 3.40000E-001 8.00000E-001 1.00000E+001 IT 3.50000E-001 8.70000E-001 1.00000E+001 IT 3.60000E-001 9.22000E-001 1.00000E+001 IT 3.70000E-001 9.52000E-001 1.00000E+001 IT 3.80000E-001 9.69000E-001 1.00000E+001 IT 3.90000E-001 9.79000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.93000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.91000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM E-FEL6 1 532488 1.53172 48.84 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 8.600000000E+000 9.500000000E+000 2.510000000E+000 5.100000000E-003 0 0 CD 2.306894600E+000 -9.688875500E-003 1.309702000E-002 6.501392700E-004 -4.232822200E-005 3.588877700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.492770000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 7.70000E-002 1.00000E+001 IT 3.50000E-001 4.48000E-001 1.00000E+001 IT 3.60000E-001 7.99000E-001 1.00000E+001 IT 3.70000E-001 9.29000E-001 1.00000E+001 IT 3.80000E-001 9.65000E-001 1.00000E+001 IT 3.90000E-001 9.82000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM E-F1 1 626357 1.62588 35.74 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 8.600000000E+000 1.070000000E+001 2.700000000E+000 3.800000000E-003 0 0 CD 2.573056500E+000 -1.020360500E-002 2.309578400E-002 8.711425200E-004 -3.073007900E-005 6.945798600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.902350000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.19000E-001 1.00000E+001 IT 3.70000E-001 4.95000E-001 1.00000E+001 IT 3.80000E-001 7.69000E-001 1.00000E+001 IT 3.90000E-001 8.96000E-001 1.00000E+001 IT 4.00000E-001 9.46000E-001 1.00000E+001 IT 4.20000E-001 9.76000E-001 1.00000E+001 IT 4.40000E-001 9.82000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.89000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.92000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM E-F3 1 613370 1.61293 36.96 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 7.700000000E+000 9.600000000E+000 2.640000000E+000 3.200000000E-003 0 0 CD 2.536269700E+000 -1.061042400E-002 2.123382100E-002 9.901210500E-004 -5.998434800E-005 8.235436600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.405530000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.40000E-002 1.00000E+001 IT 3.60000E-001 1.68000E-001 1.00000E+001 IT 3.70000E-001 5.04000E-001 1.00000E+001 IT 3.80000E-001 7.75000E-001 1.00000E+001 IT 3.90000E-001 9.01000E-001 1.00000E+001 IT 4.00000E-001 9.49000E-001 1.00000E+001 IT 4.20000E-001 9.77000E-001 1.00000E+001 IT 4.40000E-001 9.83000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-F8 1 596392 1.59551 39.22 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 8.200000000E+000 1.000000000E+001 2.620000000E+000 2.700000000E-003 0 0 CD 2.486656100E+000 -1.018848400E-002 1.928741700E-002 8.855373700E-004 -5.093710600E-005 6.425695600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.259280000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.50000E-002 1.00000E+001 IT 3.60000E-001 2.56000E-001 1.00000E+001 IT 3.70000E-001 6.41000E-001 1.00000E+001 IT 3.80000E-001 8.51000E-001 1.00000E+001 IT 3.90000E-001 9.34000E-001 1.00000E+001 IT 4.00000E-001 9.65000E-001 1.00000E+001 IT 4.20000E-001 9.84000E-001 1.00000E+001 IT 4.40000E-001 9.88000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM E-FD7 1 640346 1.63980 34.57 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 8.700000000E+000 1.070000000E+001 2.750000000E+000 5.500000000E-003 0 0 CD 2.616586500E+000 -1.142785400E-002 2.253436100E-002 1.551289000E-003 -1.176985200E-004 1.240189100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.861100000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 8.20000E-002 1.00000E+001 IT 3.70000E-001 4.23000E-001 1.00000E+001 IT 3.80000E-001 7.26000E-001 1.00000E+001 IT 3.90000E-001 8.72000E-001 1.00000E+001 IT 4.00000E-001 9.33000E-001 1.00000E+001 IT 4.20000E-001 9.73000E-001 1.00000E+001 IT 4.40000E-001 9.82000E-001 1.00000E+001 IT 4.60000E-001 9.87000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.92000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM TAC2 1 741526 1.74100 52.60 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.200000000E+000 7.100000000E+000 4.190000000E+000 -9.100000000E-003 0 0 CD 2.971713700E+000 -1.495259300E-002 2.016286800E-002 9.407228300E-004 -8.861410400E-005 5.319124200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 9.222230000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.00000E-002 1.00000E+001 IT 2.90000E-001 3.00000E-002 1.00000E+001 IT 3.00000E-001 8.00000E-002 1.00000E+001 IT 3.10000E-001 4.00000E-002 1.00000E+001 IT 3.20000E-001 2.70000E-001 1.00000E+001 IT 3.30000E-001 4.10000E-001 1.00000E+001 IT 3.40000E-001 5.70000E-001 1.00000E+001 IT 3.50000E-001 7.00000E-001 1.00000E+001 IT 3.60000E-001 8.00000E-001 1.00000E+001 IT 3.70000E-001 8.70000E-001 1.00000E+001 IT 3.80000E-001 9.20000E-001 1.00000E+001 IT 3.90000E-001 9.44000E-001 1.00000E+001 IT 4.00000E-001 9.65000E-001 1.00000E+001 IT 4.20000E-001 9.77000E-001 1.00000E+001 IT 4.40000E-001 9.84000E-001 1.00000E+001 IT 4.60000E-001 9.87000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM TAC4 1 734511 1.73400 51.05 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.200000000E+000 6.600000000E+000 4.060000000E+000 -6.300000000E-003 0 0 CD 2.942564500E+000 -1.326655400E-002 2.355922300E-002 -1.639900900E-004 9.237075900E-005 -4.861598200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 9.295490000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 8.50000E-002 1.00000E+001 IT 2.90000E-001 1.87000E-001 1.00000E+001 IT 3.00000E-001 2.92000E-001 1.00000E+001 IT 3.10000E-001 3.98000E-001 1.00000E+001 IT 3.20000E-001 5.42000E-001 1.00000E+001 IT 3.30000E-001 6.65000E-001 1.00000E+001 IT 3.40000E-001 7.68000E-001 1.00000E+001 IT 3.50000E-001 8.50000E-001 1.00000E+001 IT 3.60000E-001 9.11000E-001 1.00000E+001 IT 3.70000E-001 9.48000E-001 1.00000E+001 IT 3.80000E-001 9.68000E-001 1.00000E+001 IT 3.90000E-001 9.80000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.92000E-001 1.00000E+001 IT 4.40000E-001 9.94000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.91000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.91000E-001 1.00000E+001 NM TAC6 1 755523 1.75500 52.33 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.000000000E+000 7.400000000E+000 4.270000000E+000 -6.700000000E-003 0 0 CD 3.018218400E+000 -1.538163300E-002 2.152013700E-002 6.460830300E-004 -3.235574800E-005 2.079159300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.211160000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 4.30000E-002 1.00000E+001 IT 2.90000E-001 1.19000E-001 1.00000E+001 IT 3.00000E-001 2.10000E-001 1.00000E+001 IT 3.10000E-001 2.79000E-001 1.00000E+001 IT 3.20000E-001 4.66000E-001 1.00000E+001 IT 3.30000E-001 6.02000E-001 1.00000E+001 IT 3.40000E-001 7.22000E-001 1.00000E+001 IT 3.50000E-001 8.15000E-001 1.00000E+001 IT 3.60000E-001 8.88000E-001 1.00000E+001 IT 3.70000E-001 9.31000E-001 1.00000E+001 IT 3.80000E-001 9.58000E-001 1.00000E+001 IT 3.90000E-001 9.74000E-001 1.00000E+001 IT 4.00000E-001 9.81000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM BAF10 1 670472 1.67003 47.19 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.200000000E+000 8.600000000E+000 3.610000000E+000 7.000000000E-004 0 0 CD 2.732462100E+000 -1.249046000E-002 1.856233400E-002 9.999053600E-004 -6.838855200E-005 4.925793100E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 6.134890000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 5.00000E-002 1.00000E+001 IT 3.50000E-001 3.20000E-001 1.00000E+001 IT 3.60000E-001 6.10000E-001 1.00000E+001 IT 3.70000E-001 7.80000E-001 1.00000E+001 IT 3.80000E-001 8.80000E-001 1.00000E+001 IT 3.90000E-001 9.21000E-001 1.00000E+001 IT 4.00000E-001 9.51000E-001 1.00000E+001 IT 4.20000E-001 9.69000E-001 1.00000E+001 IT 4.40000E-001 9.72000E-001 1.00000E+001 IT 4.60000E-001 9.82000E-001 1.00000E+001 IT 4.80000E-001 9.86000E-001 1.00000E+001 IT 5.00000E-001 9.90000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 NM BAF11 1 667483 1.66672 48.30 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.200000000E+000 8.700000000E+000 3.630000000E+000 2.200000000E-003 0 0 CD 2.727295500E+000 -1.347023600E-002 1.480927100E-002 1.961533500E-003 -1.978766300E-004 1.085111700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.787910000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.30000E-001 1.00000E-002 1.00000E+001 IT 3.40000E-001 1.10000E-001 1.00000E+001 IT 3.50000E-001 2.70000E-001 1.00000E+001 IT 3.60000E-001 6.60000E-001 1.00000E+001 IT 3.70000E-001 8.30000E-001 1.00000E+001 IT 3.80000E-001 9.04000E-001 1.00000E+001 IT 3.90000E-001 9.46000E-001 1.00000E+001 IT 4.00000E-001 9.66000E-001 1.00000E+001 IT 4.20000E-001 9.76000E-001 1.00000E+001 IT 4.40000E-001 9.80000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM E-ADF10 1 613444 1.61310 44.36 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 4.700000000E+000 6.000000000E+000 3.040000000E+000 -8.000000000E-003 0 0 CD 2.552898300E+000 -1.570936400E-002 1.564768800E-002 1.446164100E-003 -1.445887900E-004 9.527573300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 9.220960000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 -1.00000 6.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 9.00000E-002 1.00000E+001 IT 3.50000E-001 3.80000E-001 1.00000E+001 IT 3.60000E-001 6.70000E-001 1.00000E+001 IT 3.70000E-001 8.20000E-001 1.00000E+001 IT 3.80000E-001 8.93000E-001 1.00000E+001 IT 3.90000E-001 9.32000E-001 1.00000E+001 IT 4.00000E-001 9.54000E-001 1.00000E+001 IT 4.20000E-001 9.75000E-001 1.00000E+001 IT 4.40000E-001 9.84000E-001 1.00000E+001 IT 4.60000E-001 9.89000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.95000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.92000E-001 1.00000E+001 IT 1.40000E+000 9.26000E-001 1.00000E+001 IT 1.50000E+000 9.54000E-001 1.00000E+001 IT 1.55000E+000 9.63000E-001 1.00000E+001 NM E-ADF50 1 654396 1.65412 39.62 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.100000000E+000 6.500000000E+000 3.380000000E+000 -3.300000000E-003 0 0 CD 2.668042200E+000 -1.318425800E-002 2.393047900E-002 2.392865500E-004 5.069794100E-005 9.124095800E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.080650000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 -1.00000 6.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 9.00000E-002 1.00000E+001 IT 3.60000E-001 3.80000E-001 1.00000E+001 IT 3.70000E-001 6.30000E-001 1.00000E+001 IT 3.80000E-001 7.90000E-001 1.00000E+001 IT 3.90000E-001 8.70000E-001 1.00000E+001 IT 4.00000E-001 9.09000E-001 1.00000E+001 IT 4.20000E-001 9.50000E-001 1.00000E+001 IT 4.40000E-001 9.69000E-001 1.00000E+001 IT 4.60000E-001 9.80000E-001 1.00000E+001 IT 4.80000E-001 9.87000E-001 1.00000E+001 IT 5.00000E-001 9.92000E-001 1.00000E+001 IT 5.50000E-001 9.95000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.93000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.93000E-001 1.00000E+001 IT 8.50000E-001 9.92000E-001 1.00000E+001 IT 9.00000E-001 9.93000E-001 1.00000E+001 IT 9.50000E-001 9.92000E-001 1.00000E+001 IT 1.00000E+000 9.93000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.94000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.93000E-001 1.00000E+001 IT 1.40000E+000 9.53000E-001 1.00000E+001 IT 1.50000E+000 9.67000E-001 1.00000E+001 IT 1.55000E+000 9.72000E-001 1.00000E+001 NM E-BACD10 1 623569 1.62280 56.91 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.700000000E+000 8.200000000E+000 3.660000000E+000 1.200000000E-003 0 0 CD 2.590632600E+000 -1.060899400E-002 1.449091600E-002 6.754224700E-004 -5.530311600E-005 3.006136400E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.771780000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 1.00000E-002 1.00000E+001 IT 3.00000E-001 8.00000E-002 1.00000E+001 IT 3.10000E-001 2.50000E-001 1.00000E+001 IT 3.20000E-001 4.70000E-001 1.00000E+001 IT 3.30000E-001 6.60000E-001 1.00000E+001 IT 3.40000E-001 8.00000E-001 1.00000E+001 IT 3.50000E-001 8.84000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.67000E-001 1.00000E+001 IT 3.80000E-001 9.83000E-001 1.00000E+001 IT 3.90000E-001 9.89000E-001 1.00000E+001 IT 4.00000E-001 9.94000E-001 1.00000E+001 IT 4.20000E-001 9.98000E-001 1.00000E+001 IT 4.40000E-001 9.98000E-001 1.00000E+001 IT 4.60000E-001 9.99000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.92000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-BACED20 1 649530 1.64850 53.03 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.000000000E+000 8.200000000E+000 3.680000000E+000 -8.000000000E-004 0 0 CD 2.666753700E+000 -9.731925900E-003 1.743628400E-002 4.755801500E-004 -1.714498900E-005 1.104958900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.633350000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 1.00000E-002 1.00000E+001 IT 3.00000E-001 4.00000E-002 1.00000E+001 IT 3.10000E-001 1.40000E-001 1.00000E+001 IT 3.20000E-001 3.20000E-001 1.00000E+001 IT 3.30000E-001 5.30000E-001 1.00000E+001 IT 3.40000E-001 7.00000E-001 1.00000E+001 IT 3.50000E-001 8.20000E-001 1.00000E+001 IT 3.60000E-001 9.03000E-001 1.00000E+001 IT 3.70000E-001 9.45000E-001 1.00000E+001 IT 3.80000E-001 9.66000E-001 1.00000E+001 IT 3.90000E-001 9.78000E-001 1.00000E+001 IT 4.00000E-001 9.84000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-BAF8 1 624471 1.62374 47.05 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 8.000000000E+000 9.500000000E+000 3.320000000E+000 -1.000000000E-003 0 0 CD 2.580112100E+000 -7.971794500E-003 1.972805400E-002 1.387607600E-004 3.763207100E-005 -7.463471700E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.149290000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 8.00000E-002 1.00000E+001 IT 3.50000E-001 3.20000E-001 1.00000E+001 IT 3.60000E-001 6.10000E-001 1.00000E+001 IT 3.70000E-001 7.90000E-001 1.00000E+001 IT 3.80000E-001 8.83000E-001 1.00000E+001 IT 3.90000E-001 9.34000E-001 1.00000E+001 IT 4.00000E-001 9.62000E-001 1.00000E+001 IT 4.20000E-001 9.84000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.91000E-001 1.00000E+001 IT 1.50000E+000 9.93000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM E-LAF7 1 750350 1.74950 35.04 0 3 4 GC Not in a position to accept new order because of discontinuation. ED 6.800000000E+000 8.200000000E+000 3.720000000E+000 5.300000000E-003 0 0 CD 2.970417800E+000 -1.329067900E-002 2.835900600E-002 1.766178600E-003 -1.245348200E-004 1.395193700E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.207790000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 3.20000E-002 1.00000E+001 IT 3.70000E-001 2.35000E-001 1.00000E+001 IT 3.80000E-001 5.13000E-001 1.00000E+001 IT 3.90000E-001 7.15000E-001 1.00000E+001 IT 4.00000E-001 8.31000E-001 1.00000E+001 IT 4.20000E-001 9.34000E-001 1.00000E+001 IT 4.40000E-001 9.62000E-001 1.00000E+001 IT 4.60000E-001 9.75000E-001 1.00000E+001 IT 4.80000E-001 9.82000E-001 1.00000E+001 IT 5.00000E-001 9.84000E-001 1.00000E+001 IT 5.50000E-001 9.94000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM NBFD12 1 800423 1.79950 42.34 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.700000000E+000 7.000000000E+000 4.450000000E+000 -7.200000000E-003 0 0 CD 3.151365500E+000 -1.305201500E-002 2.950211100E-002 6.764343700E-004 3.667970100E-006 1.823329300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.056280000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 1.10000E-002 1.00000E+001 IT 3.30000E-001 1.58000E-001 1.00000E+001 IT 3.40000E-001 4.69000E-001 1.00000E+001 IT 3.50000E-001 7.08000E-001 1.00000E+001 IT 3.60000E-001 8.47000E-001 1.00000E+001 IT 3.70000E-001 9.11000E-001 1.00000E+001 IT 3.80000E-001 9.45000E-001 1.00000E+001 IT 3.90000E-001 9.62000E-001 1.00000E+001 IT 4.00000E-001 9.74000E-001 1.00000E+001 IT 4.20000E-001 9.82000E-001 1.00000E+001 IT 4.40000E-001 9.86000E-001 1.00000E+001 IT 4.60000E-001 9.89000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM TAF2 1 795454 1.79450 45.39 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.000000000E+000 7.400000000E+000 4.350000000E+000 -9.300000000E-003 0 0 CD 3.141556400E+000 -1.437030400E-002 2.648305100E-002 9.564271400E-004 -5.941108700E-005 4.703953000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.632940000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 1.00000E-003 1.00000E+001 IT 3.20000E-001 5.50000E-002 1.00000E+001 IT 3.30000E-001 2.61000E-001 1.00000E+001 IT 3.40000E-001 5.02000E-001 1.00000E+001 IT 3.50000E-001 6.72000E-001 1.00000E+001 IT 3.60000E-001 7.97000E-001 1.00000E+001 IT 3.70000E-001 8.71000E-001 1.00000E+001 IT 3.80000E-001 9.17000E-001 1.00000E+001 IT 3.90000E-001 9.45000E-001 1.00000E+001 IT 4.00000E-001 9.60000E-001 1.00000E+001 IT 4.20000E-001 9.77000E-001 1.00000E+001 IT 4.40000E-001 9.83000E-001 1.00000E+001 IT 4.60000E-001 9.88000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.92000E-001 1.00000E+001 IT 1.50000E+000 9.91000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM TAF4 1 788475 1.78800 47.49 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.800000000E+000 7.400000000E+000 4.540000000E+000 -9.000000000E-003 0 0 CD 3.121228100E+000 -1.411990900E-002 2.652062200E-002 4.041576300E-004 1.426063400E-005 3.164256000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.510990000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.00000E-002 1.00000E+001 IT 3.20000E-001 2.15000E-001 1.00000E+001 IT 3.30000E-001 4.90000E-001 1.00000E+001 IT 3.40000E-001 6.87000E-001 1.00000E+001 IT 3.50000E-001 8.06000E-001 1.00000E+001 IT 3.60000E-001 8.87000E-001 1.00000E+001 IT 3.70000E-001 9.30000E-001 1.00000E+001 IT 3.80000E-001 9.56000E-001 1.00000E+001 IT 3.90000E-001 9.71000E-001 1.00000E+001 IT 4.00000E-001 9.80000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM TAF5 1 816466 1.81600 46.57 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.300000000E+000 7.700000000E+000 5.060000000E+000 -8.300000000E-003 0 0 CD 3.219157100E+000 -1.531056200E-002 2.636257000E-002 1.053445200E-003 -6.166041200E-005 3.973389700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.564160000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 2.00000E-002 1.00000E+001 IT 3.10000E-001 6.00000E-002 1.00000E+001 IT 3.20000E-001 1.90000E-001 1.00000E+001 IT 3.30000E-001 3.40000E-001 1.00000E+001 IT 3.40000E-001 5.10000E-001 1.00000E+001 IT 3.50000E-001 6.60000E-001 1.00000E+001 IT 3.60000E-001 7.70000E-001 1.00000E+001 IT 3.70000E-001 8.60000E-001 1.00000E+001 IT 3.80000E-001 9.20000E-001 1.00000E+001 IT 3.90000E-001 9.46000E-001 1.00000E+001 IT 4.00000E-001 9.64000E-001 1.00000E+001 IT 4.20000E-001 9.85000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 NM M-FCD1 1 497816 1.49710 81.56 0 1 1 GC Glass for molded optics lens ED 1.290000000E+001 1.630000000E+001 3.640000000E+000 3.690000000E-002 0 0 CD 2.218906800E+000 -6.170706500E-003 8.088763100E-003 1.335778200E-004 1.947618600E-007 -2.257780400E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.750000000E-005 -5.280000000E-009 2.390000000E-011 3.520000000E-007 1.970000000E-010 1.860000000E-001 2.000000000E+001 OD -1.00000 1.00000 4.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 2.80000E-002 1.00000E+001 IT 3.10000E-001 1.12000E-001 1.00000E+001 IT 3.20000E-001 2.88000E-001 1.00000E+001 IT 3.30000E-001 5.20000E-001 1.00000E+001 IT 3.40000E-001 7.26000E-001 1.00000E+001 IT 3.50000E-001 8.63000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.72000E-001 1.00000E+001 IT 3.80000E-001 9.87000E-001 1.00000E+001 IT 3.90000E-001 9.93000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-FCD1-M20 1 497815 1.49690 81.53 0 1 1 GC Preforms for Precision molding ED 1.290000000E+001 1.630000000E+001 3.640000000E+000 3.460000000E-002 0 0 CD 2.220941800E+000 -7.483037200E-003 6.246339200E-003 7.115775900E-004 -8.227425400E-005 4.043054600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.750000000E-005 -5.280000000E-009 2.390000000E-011 3.520000000E-007 1.970000000E-010 1.860000000E-001 2.000000000E+001 OD -1.00000 1.00000 4.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 2.80000E-002 1.00000E+001 IT 3.10000E-001 1.12000E-001 1.00000E+001 IT 3.20000E-001 2.88000E-001 1.00000E+001 IT 3.30000E-001 5.20000E-001 1.00000E+001 IT 3.40000E-001 7.26000E-001 1.00000E+001 IT 3.50000E-001 8.63000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.72000E-001 1.00000E+001 IT 3.80000E-001 9.87000E-001 1.00000E+001 IT 3.90000E-001 9.93000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-FCD1-M20 1 497815 1.49690 81.53 0 1 1 GC Preforms for Precision molding ED 1.290000000E+001 1.630000000E+001 3.640000000E+000 3.460000000E-002 0 0 CD 2.220941800E+000 -7.483037200E-003 6.246339200E-003 7.115775900E-004 -8.227425400E-005 4.043054600E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.750000000E-005 -5.280000000E-009 2.390000000E-011 3.520000000E-007 1.970000000E-010 1.860000000E-001 2.000000000E+001 OD -1.00000 1.00000 4.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.00000E-001 2.80000E-002 1.00000E+001 IT 3.10000E-001 1.12000E-001 1.00000E+001 IT 3.20000E-001 2.88000E-001 1.00000E+001 IT 3.30000E-001 5.20000E-001 1.00000E+001 IT 3.40000E-001 7.26000E-001 1.00000E+001 IT 3.50000E-001 8.63000E-001 1.00000E+001 IT 3.60000E-001 9.38000E-001 1.00000E+001 IT 3.70000E-001 9.72000E-001 1.00000E+001 IT 3.80000E-001 9.87000E-001 1.00000E+001 IT 3.90000E-001 9.93000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM M-FCD500 1 553717 1.55332 71.68 0 1 1 GC Glass for molded optics lens ED 1.240000000E+001 1.530000000E+001 3.660000000E+000 2.110000000E-002 0 0 CD 2.384155400E+000 -7.808442300E-003 9.713088300E-003 4.995988900E-004 -4.730322400E-005 2.320544100E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.780000000E-005 -4.970000000E-009 7.880000000E-011 4.910000000E-007 3.430000000E-010 4.410000000E-008 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.60000E-002 1.00000E+001 IT 3.20000E-001 1.09000E-001 1.00000E+001 IT 3.30000E-001 2.87000E-001 1.00000E+001 IT 3.40000E-001 5.21000E-001 1.00000E+001 IT 3.50000E-001 7.28000E-001 1.00000E+001 IT 3.60000E-001 8.67000E-001 1.00000E+001 IT 3.70000E-001 9.39000E-001 1.00000E+001 IT 3.80000E-001 9.72000E-001 1.00000E+001 IT 3.90000E-001 9.86000E-001 1.00000E+001 IT 4.00000E-001 9.93000E-001 1.00000E+001 IT 4.20000E-001 9.94000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-FCD500-20 1 554717 1.55352 71.72 0 1 1 GC Preforms for Precision molding ED 1.240000000E+001 1.530000000E+001 3.660000000E+000 2.070000000E-002 0 0 CD 2.385042700E+000 -7.914269000E-003 9.488685200E-003 5.798009300E-004 -6.001167700E-005 3.035542200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.780000000E-005 -4.970000000E-009 7.880000000E-011 4.910000000E-007 3.430000000E-010 4.410000000E-008 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.60000E-002 1.00000E+001 IT 3.20000E-001 1.09000E-001 1.00000E+001 IT 3.30000E-001 2.87000E-001 1.00000E+001 IT 3.40000E-001 5.21000E-001 1.00000E+001 IT 3.50000E-001 7.28000E-001 1.00000E+001 IT 3.60000E-001 8.67000E-001 1.00000E+001 IT 3.70000E-001 9.39000E-001 1.00000E+001 IT 3.80000E-001 9.72000E-001 1.00000E+001 IT 3.90000E-001 9.86000E-001 1.00000E+001 IT 4.00000E-001 9.93000E-001 1.00000E+001 IT 4.20000E-001 9.94000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-FCD500-20 1 554717 1.55352 71.72 0 1 1 GC Preforms for Precision molding ED 1.240000000E+001 1.530000000E+001 3.660000000E+000 2.070000000E-002 0 0 CD 2.385042700E+000 -7.914269000E-003 9.488685200E-003 5.798009300E-004 -6.001167700E-005 3.035542200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.780000000E-005 -4.970000000E-009 7.880000000E-011 4.910000000E-007 3.430000000E-010 4.410000000E-008 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.60000E-002 1.00000E+001 IT 3.20000E-001 1.09000E-001 1.00000E+001 IT 3.30000E-001 2.87000E-001 1.00000E+001 IT 3.40000E-001 5.21000E-001 1.00000E+001 IT 3.50000E-001 7.28000E-001 1.00000E+001 IT 3.60000E-001 8.67000E-001 1.00000E+001 IT 3.70000E-001 9.39000E-001 1.00000E+001 IT 3.80000E-001 9.72000E-001 1.00000E+001 IT 3.90000E-001 9.86000E-001 1.00000E+001 IT 4.00000E-001 9.93000E-001 1.00000E+001 IT 4.20000E-001 9.94000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM M-PCD4 1 619639 1.61881 63.85 0 1 1 GC Glass for molded optics lens ED 8.700000000E+000 1.300000000E+001 3.570000000E+000 8.400000000E-003 0 0 CD 2.582335000E+000 -9.952039000E-003 1.329184000E-002 4.550621000E-004 -3.327132000E-005 1.730172000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.080000000E-005 2.420000000E-009 1.570000000E-011 7.210000000E-007 4.290000000E-010 1.460000000E-009 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 3.40000E-002 1.00000E+001 IT 3.30000E-001 1.25000E-001 1.00000E+001 IT 3.40000E-001 3.00000E-001 1.00000E+001 IT 3.50000E-001 5.21000E-001 1.00000E+001 IT 3.60000E-001 7.23000E-001 1.00000E+001 IT 3.70000E-001 8.54000E-001 1.00000E+001 IT 3.80000E-001 9.24000E-001 1.00000E+001 IT 3.90000E-001 9.60000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.88000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-PCD4-40 1 619639 1.61921 63.86 0 1 1 GC Preforms for Precision molding ED 8.700000000E+000 1.300000000E+001 3.570000000E+000 8.500000000E-003 0 0 CD 2.583147100E+000 -9.750234400E-003 1.361537400E-002 3.634612200E-004 -2.118708200E-005 1.153613200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.080000000E-005 2.420000000E-009 1.570000000E-011 7.210000000E-007 4.290000000E-010 1.460000000E-009 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 3.40000E-002 1.00000E+001 IT 3.30000E-001 1.25000E-001 1.00000E+001 IT 3.40000E-001 3.00000E-001 1.00000E+001 IT 3.50000E-001 5.21000E-001 1.00000E+001 IT 3.60000E-001 7.23000E-001 1.00000E+001 IT 3.70000E-001 8.54000E-001 1.00000E+001 IT 3.80000E-001 9.24000E-001 1.00000E+001 IT 3.90000E-001 9.60000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.88000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.96000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-PCD4-40 1 619639 1.61921 63.86 0 1 1 GC Preforms for Precision molding ED 8.700000000E+000 1.300000000E+001 3.570000000E+000 8.500000000E-003 0 0 CD 2.583147100E+000 -9.750234400E-003 1.361537400E-002 3.634612200E-004 -2.118708200E-005 1.153613200E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -1.080000000E-005 2.420000000E-009 1.570000000E-011 7.210000000E-007 4.290000000E-010 1.460000000E-009 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 2.40000E-002 1.00000E+001 IT 3.20000E-001 9.20000E-002 1.00000E+001 IT 3.30000E-001 2.40000E-001 1.00000E+001 IT 3.40000E-001 4.55000E-001 1.00000E+001 IT 3.50000E-001 6.63000E-001 1.00000E+001 IT 3.60000E-001 8.15000E-001 1.00000E+001 IT 3.70000E-001 9.11000E-001 1.00000E+001 IT 3.80000E-001 9.54000E-001 1.00000E+001 IT 3.90000E-001 9.76000E-001 1.00000E+001 IT 4.00000E-001 9.86000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.94000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.94000E-001 1.00000E+001 IT 9.50000E-001 9.94000E-001 1.00000E+001 IT 1.00000E+000 9.94000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM M-PCD51 1 592670 1.59201 67.02 0 1 1 GC Glass for molded optics lens ED 8.900000000E+000 1.160000000E+001 3.140000000E+000 8.100000000E-003 0 0 CD 2.502026000E+000 -1.108292000E-002 1.127720000E-002 5.715408000E-004 -5.587455000E-005 2.905292000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -5.750000000E-006 4.330000000E-009 -1.700000000E-011 3.990000000E-007 4.040000000E-010 1.750000000E-001 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.70000E-002 1.00000E+001 IT 2.90000E-001 1.10000E-001 1.00000E+001 IT 3.00000E-001 2.26000E-001 1.00000E+001 IT 3.10000E-001 3.78000E-001 1.00000E+001 IT 3.20000E-001 5.44000E-001 1.00000E+001 IT 3.30000E-001 6.96000E-001 1.00000E+001 IT 3.40000E-001 8.13000E-001 1.00000E+001 IT 3.50000E-001 8.93000E-001 1.00000E+001 IT 3.60000E-001 9.43000E-001 1.00000E+001 IT 3.70000E-001 9.70000E-001 1.00000E+001 IT 3.80000E-001 9.83000E-001 1.00000E+001 IT 3.90000E-001 9.90000E-001 1.00000E+001 IT 4.00000E-001 9.93000E-001 1.00000E+001 IT 4.20000E-001 9.94000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-PCD51-70 1 593670 1.59271 66.97 0 1 1 GC Preforms for Precision molding ED 8.900000000E+000 1.160000000E+001 3.140000000E+000 9.000000000E-003 0 0 CD 2.502543600E+000 -1.032143700E-002 1.243363600E-002 2.186653500E-004 -5.579397700E-006 3.018838300E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -5.750000000E-006 4.330000000E-009 -1.700000000E-011 3.990000000E-007 4.040000000E-010 1.750000000E-001 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.70000E-002 1.00000E+001 IT 2.90000E-001 1.10000E-001 1.00000E+001 IT 3.00000E-001 2.26000E-001 1.00000E+001 IT 3.10000E-001 3.78000E-001 1.00000E+001 IT 3.20000E-001 5.44000E-001 1.00000E+001 IT 3.30000E-001 6.96000E-001 1.00000E+001 IT 3.40000E-001 8.13000E-001 1.00000E+001 IT 3.50000E-001 8.93000E-001 1.00000E+001 IT 3.60000E-001 9.43000E-001 1.00000E+001 IT 3.70000E-001 9.70000E-001 1.00000E+001 IT 3.80000E-001 9.83000E-001 1.00000E+001 IT 3.90000E-001 9.90000E-001 1.00000E+001 IT 4.00000E-001 9.93000E-001 1.00000E+001 IT 4.20000E-001 9.94000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-PCD51-70 1 593670 1.59271 66.97 0 1 1 GC Preforms for Precision molding ED 8.900000000E+000 1.160000000E+001 3.140000000E+000 9.000000000E-003 0 0 CD 2.502543600E+000 -1.032143700E-002 1.243363600E-002 2.186653500E-004 -5.579397700E-006 3.018838300E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -5.750000000E-006 4.330000000E-009 -1.700000000E-011 3.990000000E-007 4.040000000E-010 1.750000000E-001 2.000000000E+001 OD -1.00000 1.00000 -1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.90000E-001 1.00000E+001 IT 2.90000E-001 3.00000E-001 1.00000E+001 IT 3.00000E-001 4.10000E-001 1.00000E+001 IT 3.10000E-001 5.50000E-001 1.00000E+001 IT 3.20000E-001 6.90000E-001 1.00000E+001 IT 3.30000E-001 8.00000E-001 1.00000E+001 IT 3.40000E-001 8.84000E-001 1.00000E+001 IT 3.50000E-001 9.36000E-001 1.00000E+001 IT 3.60000E-001 9.64000E-001 1.00000E+001 IT 3.70000E-001 9.83000E-001 1.00000E+001 IT 3.80000E-001 9.90000E-001 1.00000E+001 IT 3.90000E-001 9.94000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.96000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.92000E-001 1.00000E+001 NM M-BACD5N 1 589613 1.58913 61.25 0 1 1 GC Glass for molded optics lens ED 6.600000000E+000 8.800000000E+000 2.820000000E+000 -7.000000000E-004 0 0 CD 2.489510000E+000 -1.224496000E-002 1.294262000E-002 3.490449000E-004 -1.777228000E-005 9.113719000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.330000000E-006 1.010000000E-008 -4.770000000E-011 6.070000000E-007 6.780000000E-010 8.150000000E-009 2.000000000E+001 OD -1.00000 2.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.10000E-002 1.00000E+001 IT 2.90000E-001 7.00000E-002 1.00000E+001 IT 3.00000E-001 1.77000E-001 1.00000E+001 IT 3.10000E-001 3.44000E-001 1.00000E+001 IT 3.20000E-001 5.34000E-001 1.00000E+001 IT 3.30000E-001 7.02000E-001 1.00000E+001 IT 3.40000E-001 8.22000E-001 1.00000E+001 IT 3.50000E-001 9.00000E-001 1.00000E+001 IT 3.60000E-001 9.46000E-001 1.00000E+001 IT 3.70000E-001 9.72000E-001 1.00000E+001 IT 3.80000E-001 9.84000E-001 1.00000E+001 IT 3.90000E-001 9.90000E-001 1.00000E+001 IT 4.00000E-001 9.94000E-001 1.00000E+001 IT 4.20000E-001 9.96000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.94000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.92000E-001 1.00000E+001 IT 9.00000E-001 9.92000E-001 1.00000E+001 IT 9.50000E-001 9.91000E-001 1.00000E+001 IT 1.00000E+000 9.91000E-001 1.00000E+001 IT 1.05000E+000 9.91000E-001 1.00000E+001 IT 1.06000E+000 9.90000E-001 1.00000E+001 IT 1.10000E+000 9.91000E-001 1.00000E+001 IT 1.20000E+000 9.92000E-001 1.00000E+001 IT 1.30000E+000 9.92000E-001 1.00000E+001 IT 1.40000E+000 9.81000E-001 1.00000E+001 IT 1.50000E+000 9.89000E-001 1.00000E+001 IT 1.55000E+000 9.90000E-001 1.00000E+001 NM MP-BACD5N 1 589613 1.58913 61.25 0 1 1 GC Preforms for Precision molding ED 6.600000000E+000 8.800000000E+000 2.820000000E+000 -7.000000000E-004 0 0 CD 2.489510000E+000 -1.224496000E-002 1.294262000E-002 3.490449000E-004 -1.777228000E-005 9.113719000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.330000000E-006 1.010000000E-008 -4.770000000E-011 6.070000000E-007 6.780000000E-010 8.150000000E-009 2.000000000E+001 OD -1.00000 2.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.10000E-002 1.00000E+001 IT 2.90000E-001 7.00000E-002 1.00000E+001 IT 3.00000E-001 1.77000E-001 1.00000E+001 IT 3.10000E-001 3.44000E-001 1.00000E+001 IT 3.20000E-001 5.34000E-001 1.00000E+001 IT 3.30000E-001 7.02000E-001 1.00000E+001 IT 3.40000E-001 8.22000E-001 1.00000E+001 IT 3.50000E-001 9.00000E-001 1.00000E+001 IT 3.60000E-001 9.46000E-001 1.00000E+001 IT 3.70000E-001 9.72000E-001 1.00000E+001 IT 3.80000E-001 9.84000E-001 1.00000E+001 IT 3.90000E-001 9.90000E-001 1.00000E+001 IT 4.00000E-001 9.94000E-001 1.00000E+001 IT 4.20000E-001 9.96000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.94000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.92000E-001 1.00000E+001 IT 9.00000E-001 9.92000E-001 1.00000E+001 IT 9.50000E-001 9.91000E-001 1.00000E+001 IT 1.00000E+000 9.91000E-001 1.00000E+001 IT 1.05000E+000 9.91000E-001 1.00000E+001 IT 1.06000E+000 9.90000E-001 1.00000E+001 IT 1.10000E+000 9.91000E-001 1.00000E+001 IT 1.20000E+000 9.92000E-001 1.00000E+001 IT 1.30000E+000 9.92000E-001 1.00000E+001 IT 1.40000E+000 9.81000E-001 1.00000E+001 IT 1.50000E+000 9.89000E-001 1.00000E+001 IT 1.55000E+000 9.90000E-001 1.00000E+001 NM MC-BACD5N 1 589613 1.58913 61.25 0 1 1 GC Preforms for Precision molding ED 6.600000000E+000 8.800000000E+000 2.820000000E+000 -7.000000000E-004 0 0 CD 2.489510000E+000 -1.224496000E-002 1.294262000E-002 3.490449000E-004 -1.777228000E-005 9.113719000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.330000000E-006 1.010000000E-008 -4.770000000E-011 6.070000000E-007 6.780000000E-010 8.150000000E-009 2.000000000E+001 OD -1.00000 2.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.70000E-002 1.00000E+001 IT 2.90000E-001 1.04000E-001 1.00000E+001 IT 3.00000E-001 2.33000E-001 1.00000E+001 IT 3.10000E-001 4.08000E-001 1.00000E+001 IT 3.20000E-001 6.00000E-001 1.00000E+001 IT 3.30000E-001 7.50000E-001 1.00000E+001 IT 3.40000E-001 8.61000E-001 1.00000E+001 IT 3.50000E-001 9.19000E-001 1.00000E+001 IT 3.60000E-001 9.65000E-001 1.00000E+001 IT 3.70000E-001 9.80000E-001 1.00000E+001 IT 3.80000E-001 9.88000E-001 1.00000E+001 IT 3.90000E-001 9.92000E-001 1.00000E+001 IT 4.00000E-001 9.95000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.97000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.94000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.92000E-001 1.00000E+001 IT 9.00000E-001 9.92000E-001 1.00000E+001 IT 9.50000E-001 9.91000E-001 1.00000E+001 IT 1.00000E+000 9.91000E-001 1.00000E+001 IT 1.05000E+000 9.91000E-001 1.00000E+001 IT 1.06000E+000 9.90000E-001 1.00000E+001 IT 1.10000E+000 9.91000E-001 1.00000E+001 IT 1.20000E+000 9.92000E-001 1.00000E+001 IT 1.30000E+000 9.92000E-001 1.00000E+001 IT 1.40000E+000 9.81000E-001 1.00000E+001 IT 1.50000E+000 9.89000E-001 1.00000E+001 IT 1.55000E+000 9.90000E-001 1.00000E+001 NM M-BACD12 1 583595 1.58313 59.46 0 1 1 GC Glass for molded optics lens ED 6.900000000E+000 9.000000000E+000 3.010000000E+000 -8.000000000E-004 0 0 CD 2.468781000E+000 -1.062639000E-002 1.325184000E-002 4.048612000E-004 -2.974799000E-005 1.825884000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.360000000E-006 1.020000000E-008 -4.810000000E-011 6.100000000E-007 6.810000000E-010 4.770000000E-009 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.60000E-002 1.00000E+001 IT 2.90000E-001 8.80000E-002 1.00000E+001 IT 3.00000E-001 2.20000E-001 1.00000E+001 IT 3.10000E-001 4.13000E-001 1.00000E+001 IT 3.20000E-001 6.12000E-001 1.00000E+001 IT 3.30000E-001 7.68000E-001 1.00000E+001 IT 3.40000E-001 8.69000E-001 1.00000E+001 IT 3.50000E-001 9.29000E-001 1.00000E+001 IT 3.60000E-001 9.64000E-001 1.00000E+001 IT 3.70000E-001 9.81000E-001 1.00000E+001 IT 3.80000E-001 9.88000E-001 1.00000E+001 IT 3.90000E-001 9.93000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.95000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-BACD12 1 583595 1.58313 59.46 0 1 1 GC Preforms for Precision molding ED 6.900000000E+000 9.000000000E+000 3.010000000E+000 -8.000000000E-004 0 0 CD 2.468781000E+000 -1.062639000E-002 1.325184000E-002 4.048612000E-004 -2.974799000E-005 1.825884000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.360000000E-006 1.020000000E-008 -4.810000000E-011 6.100000000E-007 6.810000000E-010 4.770000000E-009 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.60000E-002 1.00000E+001 IT 2.90000E-001 8.80000E-002 1.00000E+001 IT 3.00000E-001 2.20000E-001 1.00000E+001 IT 3.10000E-001 4.13000E-001 1.00000E+001 IT 3.20000E-001 6.12000E-001 1.00000E+001 IT 3.30000E-001 7.68000E-001 1.00000E+001 IT 3.40000E-001 8.69000E-001 1.00000E+001 IT 3.50000E-001 9.29000E-001 1.00000E+001 IT 3.60000E-001 9.64000E-001 1.00000E+001 IT 3.70000E-001 9.81000E-001 1.00000E+001 IT 3.80000E-001 9.88000E-001 1.00000E+001 IT 3.90000E-001 9.93000E-001 1.00000E+001 IT 4.00000E-001 9.96000E-001 1.00000E+001 IT 4.20000E-001 9.97000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.98000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.95000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MC-BACD12 1 583595 1.58313 59.46 0 1 1 GC Preforms for Precision molding ED 6.900000000E+000 9.000000000E+000 3.010000000E+000 -8.000000000E-004 0 0 CD 2.468781000E+000 -1.062639000E-002 1.325184000E-002 4.048612000E-004 -2.974799000E-005 1.825884000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.360000000E-006 1.020000000E-008 -4.810000000E-011 6.100000000E-007 6.810000000E-010 4.770000000E-009 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.50000E-002 1.00000E+001 IT 2.90000E-001 8.20000E-002 1.00000E+001 IT 3.00000E-001 2.43000E-001 1.00000E+001 IT 3.10000E-001 4.64000E-001 1.00000E+001 IT 3.20000E-001 6.77000E-001 1.00000E+001 IT 3.30000E-001 8.16000E-001 1.00000E+001 IT 3.40000E-001 9.04000E-001 1.00000E+001 IT 3.50000E-001 9.56000E-001 1.00000E+001 IT 3.60000E-001 9.77000E-001 1.00000E+001 IT 3.70000E-001 9.89000E-001 1.00000E+001 IT 3.80000E-001 9.91000E-001 1.00000E+001 IT 3.90000E-001 9.94000E-001 1.00000E+001 IT 4.00000E-001 9.99000E-001 1.00000E+001 IT 4.20000E-001 9.99000E-001 1.00000E+001 IT 4.40000E-001 9.98000E-001 1.00000E+001 IT 4.60000E-001 9.99000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.94000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.92000E-001 1.00000E+001 IT 9.00000E-001 9.91000E-001 1.00000E+001 IT 9.50000E-001 9.91000E-001 1.00000E+001 IT 1.00000E+000 9.91000E-001 1.00000E+001 IT 1.05000E+000 9.91000E-001 1.00000E+001 IT 1.06000E+000 9.90000E-001 1.00000E+001 IT 1.10000E+000 9.91000E-001 1.00000E+001 IT 1.20000E+000 9.92000E-001 1.00000E+001 IT 1.30000E+000 9.92000E-001 1.00000E+001 IT 1.40000E+000 9.81000E-001 1.00000E+001 IT 1.50000E+000 9.89000E-001 1.00000E+001 IT 1.55000E+000 9.90000E-001 1.00000E+001 NM M-BACD15 1 623582 1.62263 58.16 0 1 1 GC Glass for molded optics lens ED 6.300000000E+000 8.200000000E+000 3.020000000E+000 -4.500000000E-003 0 0 CD 2.590919000E+000 -1.259476000E-002 1.520205000E-002 2.999980000E-004 -1.131547000E-005 9.154640000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.129680000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.10000E-002 1.00000E+001 IT 2.90000E-001 1.11000E-001 1.00000E+001 IT 3.00000E-001 2.31000E-001 1.00000E+001 IT 3.10000E-001 3.63000E-001 1.00000E+001 IT 3.20000E-001 5.67000E-001 1.00000E+001 IT 3.30000E-001 7.18000E-001 1.00000E+001 IT 3.40000E-001 8.27000E-001 1.00000E+001 IT 3.50000E-001 9.00000E-001 1.00000E+001 IT 3.60000E-001 9.45000E-001 1.00000E+001 IT 3.70000E-001 9.68000E-001 1.00000E+001 IT 3.80000E-001 9.79000E-001 1.00000E+001 IT 3.90000E-001 9.85000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.95000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-BACD15 1 623582 1.62263 58.16 0 1 1 GC Preforms for Precision molding ED 6.300000000E+000 8.200000000E+000 3.020000000E+000 -4.500000000E-003 0 0 CD 2.590919000E+000 -1.259476000E-002 1.520205000E-002 2.999980000E-004 -1.131547000E-005 9.154640000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.129680000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 2.00000 3.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.10000E-002 1.00000E+001 IT 2.90000E-001 1.11000E-001 1.00000E+001 IT 3.00000E-001 2.31000E-001 1.00000E+001 IT 3.10000E-001 3.63000E-001 1.00000E+001 IT 3.20000E-001 5.67000E-001 1.00000E+001 IT 3.30000E-001 7.18000E-001 1.00000E+001 IT 3.40000E-001 8.27000E-001 1.00000E+001 IT 3.50000E-001 9.00000E-001 1.00000E+001 IT 3.60000E-001 9.45000E-001 1.00000E+001 IT 3.70000E-001 9.68000E-001 1.00000E+001 IT 3.80000E-001 9.79000E-001 1.00000E+001 IT 3.90000E-001 9.85000E-001 1.00000E+001 IT 4.00000E-001 9.89000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.95000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM M-LAC130 1 694532 1.69350 53.20 0 1 1 GC Glass for molded optics lens ED 6.500000000E+000 8.600000000E+000 3.520000000E+000 -5.900000000E-003 0 0 CD 2.813412000E+000 -1.332448000E-002 1.927865000E-002 4.124452000E-004 -9.940432000E-006 9.622024000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.060000000E-006 7.530000000E-009 -3.420000000E-011 7.880000000E-007 1.050000000E-009 4.450000000E-010 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 3.50000E-002 1.00000E+001 IT 3.00000E-001 9.60000E-002 1.00000E+001 IT 3.10000E-001 1.96000E-001 1.00000E+001 IT 3.20000E-001 3.41000E-001 1.00000E+001 IT 3.30000E-001 5.07000E-001 1.00000E+001 IT 3.40000E-001 6.64000E-001 1.00000E+001 IT 3.50000E-001 7.91000E-001 1.00000E+001 IT 3.60000E-001 8.80000E-001 1.00000E+001 IT 3.70000E-001 9.34000E-001 1.00000E+001 IT 3.80000E-001 9.63000E-001 1.00000E+001 IT 3.90000E-001 9.78000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.92000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-LAC130 1 694532 1.69350 53.20 0 1 1 GC Preforms for Precision molding ED 6.500000000E+000 8.600000000E+000 3.520000000E+000 -5.900000000E-003 0 0 CD 2.813412000E+000 -1.332448000E-002 1.927865000E-002 4.124452000E-004 -9.940432000E-006 9.622024000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.060000000E-006 7.530000000E-009 -3.420000000E-011 7.880000000E-007 1.050000000E-009 4.450000000E-010 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 3.50000E-002 1.00000E+001 IT 3.00000E-001 9.60000E-002 1.00000E+001 IT 3.10000E-001 1.96000E-001 1.00000E+001 IT 3.20000E-001 3.41000E-001 1.00000E+001 IT 3.30000E-001 5.07000E-001 1.00000E+001 IT 3.40000E-001 6.64000E-001 1.00000E+001 IT 3.50000E-001 7.91000E-001 1.00000E+001 IT 3.60000E-001 8.80000E-001 1.00000E+001 IT 3.70000E-001 9.34000E-001 1.00000E+001 IT 3.80000E-001 9.63000E-001 1.00000E+001 IT 3.90000E-001 9.78000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.92000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.99000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-LAC130 1 694532 1.69350 53.20 0 1 1 GC Preforms for Precision molding ED 6.500000000E+000 8.600000000E+000 3.520000000E+000 -5.900000000E-003 0 0 CD 2.813412000E+000 -1.332448000E-002 1.927865000E-002 4.124452000E-004 -9.940432000E-006 9.622024000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.060000000E-006 7.530000000E-009 -3.420000000E-011 7.880000000E-007 1.050000000E-009 4.450000000E-010 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 4.10000E-002 1.00000E+001 IT 3.00000E-001 1.16000E-001 1.00000E+001 IT 3.10000E-001 2.21000E-001 1.00000E+001 IT 3.20000E-001 3.77000E-001 1.00000E+001 IT 3.30000E-001 5.49000E-001 1.00000E+001 IT 3.40000E-001 6.98000E-001 1.00000E+001 IT 3.50000E-001 8.11000E-001 1.00000E+001 IT 3.60000E-001 8.97000E-001 1.00000E+001 IT 3.70000E-001 9.43000E-001 1.00000E+001 IT 3.80000E-001 9.66000E-001 1.00000E+001 IT 3.90000E-001 9.80000E-001 1.00000E+001 IT 4.00000E-001 9.87000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.94000E-001 1.00000E+001 IT 4.60000E-001 9.96000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM M-LAC14 1 697555 1.69680 55.46 0 1 1 GC Glass for molded optics lens ED 6.500000000E+000 8.000000000E+000 3.700000000E+000 -5.900000000E-003 0 0 CD 2.827838600E+000 -1.477393900E-002 1.821173300E-002 4.931196400E-004 -2.548688600E-005 1.679548700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.138570000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 5.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.90000E-002 1.00000E+001 IT 2.90000E-001 7.80000E-002 1.00000E+001 IT 3.00000E-001 1.50000E-001 1.00000E+001 IT 3.10000E-001 2.34000E-001 1.00000E+001 IT 3.20000E-001 4.06000E-001 1.00000E+001 IT 3.30000E-001 5.60000E-001 1.00000E+001 IT 3.40000E-001 6.99000E-001 1.00000E+001 IT 3.50000E-001 8.07000E-001 1.00000E+001 IT 3.60000E-001 8.86000E-001 1.00000E+001 IT 3.70000E-001 9.30000E-001 1.00000E+001 IT 3.80000E-001 9.56000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.78000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM MP-LAC14-80 1 698555 1.69760 55.51 0 1 1 GC Preforms for Precision molding ED 6.500000000E+000 8.000000000E+000 3.700000000E+000 -5.900000000E-003 0 0 CD 2.830673300E+000 -1.485586300E-002 1.810347200E-002 5.353997100E-004 -3.192977800E-005 2.034098300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.134560000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 5.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.90000E-002 1.00000E+001 IT 2.90000E-001 7.80000E-002 1.00000E+001 IT 3.00000E-001 1.50000E-001 1.00000E+001 IT 3.10000E-001 2.34000E-001 1.00000E+001 IT 3.20000E-001 4.06000E-001 1.00000E+001 IT 3.30000E-001 5.60000E-001 1.00000E+001 IT 3.40000E-001 6.99000E-001 1.00000E+001 IT 3.50000E-001 8.07000E-001 1.00000E+001 IT 3.60000E-001 8.86000E-001 1.00000E+001 IT 3.70000E-001 9.30000E-001 1.00000E+001 IT 3.80000E-001 9.56000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.78000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM M-TAC60 1 755512 1.75501 51.16 0 1 1 GC Glass for molded optics lens ED 6.200000000E+000 7.700000000E+000 4.410000000E+000 -7.700000000E-003 0 0 CD 3.017866000E+000 -1.579093400E-002 2.114470200E-002 9.313738900E-004 -6.937991400E-005 4.027620000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.378720000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.90000E-002 1.00000E+001 IT 2.90000E-001 6.20000E-002 1.00000E+001 IT 3.00000E-001 1.09000E-001 1.00000E+001 IT 3.10000E-001 1.67000E-001 1.00000E+001 IT 3.20000E-001 3.26000E-001 1.00000E+001 IT 3.30000E-001 4.93000E-001 1.00000E+001 IT 3.40000E-001 6.34000E-001 1.00000E+001 IT 3.50000E-001 7.54000E-001 1.00000E+001 IT 3.60000E-001 8.47000E-001 1.00000E+001 IT 3.70000E-001 9.08000E-001 1.00000E+001 IT 3.80000E-001 9.43000E-001 1.00000E+001 IT 3.90000E-001 9.63000E-001 1.00000E+001 IT 4.00000E-001 9.75000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.93000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-TAC60-90 1 756512 1.75591 51.18 0 1 1 GC Preforms for Precision molding ED 6.200000000E+000 7.700000000E+000 4.410000000E+000 -7.900000000E-003 0 0 CD 3.020921400E+000 -1.578010000E-002 2.114253000E-002 9.555655400E-004 -7.448981900E-005 4.360632000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.373350000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.90000E-002 1.00000E+001 IT 2.90000E-001 6.20000E-002 1.00000E+001 IT 3.00000E-001 1.09000E-001 1.00000E+001 IT 3.10000E-001 1.67000E-001 1.00000E+001 IT 3.20000E-001 3.26000E-001 1.00000E+001 IT 3.30000E-001 4.93000E-001 1.00000E+001 IT 3.40000E-001 6.34000E-001 1.00000E+001 IT 3.50000E-001 7.54000E-001 1.00000E+001 IT 3.60000E-001 8.47000E-001 1.00000E+001 IT 3.70000E-001 9.08000E-001 1.00000E+001 IT 3.80000E-001 9.43000E-001 1.00000E+001 IT 3.90000E-001 9.63000E-001 1.00000E+001 IT 4.00000E-001 9.75000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.98000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.93000E-001 1.00000E+001 IT 9.00000E-001 9.95000E-001 1.00000E+001 IT 9.50000E-001 9.96000E-001 1.00000E+001 IT 1.00000E+000 9.96000E-001 1.00000E+001 IT 1.05000E+000 9.96000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.96000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM M-TAC80 1 729540 1.72903 54.04 0 1 1 GC Glass for molded optics lens ED 6.100000000E+000 7.400000000E+000 4.280000000E+000 -6.300000000E-003 0 0 CD 2.935194800E+000 -1.619345800E-002 1.839228700E-002 1.008616700E-003 -8.756547400E-005 4.692133300E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.675460000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.50000E-002 1.00000E+001 IT 2.90000E-001 8.00000E-002 1.00000E+001 IT 3.00000E-001 1.36000E-001 1.00000E+001 IT 3.10000E-001 1.97000E-001 1.00000E+001 IT 3.20000E-001 3.67000E-001 1.00000E+001 IT 3.30000E-001 5.36000E-001 1.00000E+001 IT 3.40000E-001 6.71000E-001 1.00000E+001 IT 3.50000E-001 7.82000E-001 1.00000E+001 IT 3.60000E-001 8.65000E-001 1.00000E+001 IT 3.70000E-001 9.19000E-001 1.00000E+001 IT 3.80000E-001 9.50000E-001 1.00000E+001 IT 3.90000E-001 9.68000E-001 1.00000E+001 IT 4.00000E-001 9.79000E-001 1.00000E+001 IT 4.20000E-001 9.89000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM MP-TAC80-60 1 730541 1.72963 54.07 0 1 1 GC Preforms for Precision molding ED 6.100000000E+000 7.400000000E+000 4.280000000E+000 -6.400000000E-003 0 0 CD 2.937212800E+000 -1.618578900E-002 1.839514000E-002 1.026607100E-003 -9.237987200E-005 5.050923700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.672230000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.50000E-002 1.00000E+001 IT 2.90000E-001 8.00000E-002 1.00000E+001 IT 3.00000E-001 1.36000E-001 1.00000E+001 IT 3.10000E-001 1.97000E-001 1.00000E+001 IT 3.20000E-001 3.67000E-001 1.00000E+001 IT 3.30000E-001 5.36000E-001 1.00000E+001 IT 3.40000E-001 6.71000E-001 1.00000E+001 IT 3.50000E-001 7.82000E-001 1.00000E+001 IT 3.60000E-001 8.65000E-001 1.00000E+001 IT 3.70000E-001 9.19000E-001 1.00000E+001 IT 3.80000E-001 9.50000E-001 1.00000E+001 IT 3.90000E-001 9.68000E-001 1.00000E+001 IT 4.00000E-001 9.79000E-001 1.00000E+001 IT 4.20000E-001 9.89000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.95000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM M-FD80 1 689312 1.68893 31.16 0 1 1 GC Glass for molded optics lens ED 1.150000000E+001 1.430000000E+001 3.260000000E+000 1.150000000E-002 0 0 CD 2.761638000E+000 -1.132633000E-002 2.865346000E-002 1.529038000E-003 -8.743577000E-005 1.496579000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -8.153030000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 2.70000E-002 1.00000E+001 IT 3.70000E-001 2.13000E-001 1.00000E+001 IT 3.80000E-001 5.23000E-001 1.00000E+001 IT 3.90000E-001 7.36000E-001 1.00000E+001 IT 4.00000E-001 8.36000E-001 1.00000E+001 IT 4.20000E-001 9.11000E-001 1.00000E+001 IT 4.40000E-001 9.41000E-001 1.00000E+001 IT 4.60000E-001 9.57000E-001 1.00000E+001 IT 4.80000E-001 9.68000E-001 1.00000E+001 IT 5.00000E-001 9.76000E-001 1.00000E+001 IT 5.50000E-001 9.90000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM MP-FD80 1 689312 1.68893 31.16 0 1 1 GC Preforms for Precision molding ED 1.150000000E+001 1.430000000E+001 3.260000000E+000 1.150000000E-002 0 0 CD 2.761638000E+000 -1.132633000E-002 2.865346000E-002 1.529038000E-003 -8.743577000E-005 1.496579000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -8.153030000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 3.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 2.70000E-002 1.00000E+001 IT 3.70000E-001 2.13000E-001 1.00000E+001 IT 3.80000E-001 5.23000E-001 1.00000E+001 IT 3.90000E-001 7.36000E-001 1.00000E+001 IT 4.00000E-001 8.36000E-001 1.00000E+001 IT 4.20000E-001 9.11000E-001 1.00000E+001 IT 4.40000E-001 9.41000E-001 1.00000E+001 IT 4.60000E-001 9.57000E-001 1.00000E+001 IT 4.80000E-001 9.68000E-001 1.00000E+001 IT 5.00000E-001 9.76000E-001 1.00000E+001 IT 5.50000E-001 9.90000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.90000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM M-FDS2 1 002193 2.00178 19.32 0 1 1 GC Glass for molded optics lens ED 7.900000000E+000 1.010000000E+001 5.090000000E+000 3.120000000E-002 0 0 CD 3.771581000E+000 -2.044536400E-002 6.394257900E-002 8.354547000E-003 -8.203198400E-004 1.027950700E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.170000000E-007 1.140000000E-008 -3.070000000E-011 1.840000000E-006 2.480000000E-009 3.080000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.00000E-001 2.00000E-002 1.00000E+001 IT 4.20000E-001 3.34000E-001 1.00000E+001 IT 4.40000E-001 6.43000E-001 1.00000E+001 IT 4.60000E-001 7.92000E-001 1.00000E+001 IT 4.80000E-001 8.67000E-001 1.00000E+001 IT 5.00000E-001 9.11000E-001 1.00000E+001 IT 5.50000E-001 9.72000E-001 1.00000E+001 IT 6.00000E-001 9.91000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-FDS2 1 002193 2.00178 19.32 0 1 1 GC Preforms for Precision molding ED 7.900000000E+000 1.010000000E+001 5.090000000E+000 3.120000000E-002 0 0 CD 3.771581000E+000 -2.044536400E-002 6.394257900E-002 8.354547000E-003 -8.203198400E-004 1.027950700E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.170000000E-007 1.140000000E-008 -3.070000000E-011 1.840000000E-006 2.480000000E-009 3.080000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.00000E-001 2.00000E-002 1.00000E+001 IT 4.20000E-001 3.34000E-001 1.00000E+001 IT 4.40000E-001 6.43000E-001 1.00000E+001 IT 4.60000E-001 7.92000E-001 1.00000E+001 IT 4.80000E-001 8.67000E-001 1.00000E+001 IT 5.00000E-001 9.11000E-001 1.00000E+001 IT 5.50000E-001 9.72000E-001 1.00000E+001 IT 6.00000E-001 9.91000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-FDS2 1 002193 2.00178 19.32 0 1 1 GC Preforms for Precision molding ED 7.900000000E+000 1.010000000E+001 5.090000000E+000 3.120000000E-002 0 0 CD 3.771581000E+000 -2.044536400E-002 6.394257900E-002 8.354547000E-003 -8.203198400E-004 1.027950700E-004 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 2.170000000E-007 1.140000000E-008 -3.070000000E-011 1.840000000E-006 2.480000000E-009 3.080000000E-001 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 4.00000E-001 3.20000E-002 1.00000E+001 IT 4.20000E-001 4.57000E-001 1.00000E+001 IT 4.40000E-001 7.74000E-001 1.00000E+001 IT 4.60000E-001 8.84000E-001 1.00000E+001 IT 4.80000E-001 9.28000E-001 1.00000E+001 IT 5.00000E-001 9.54000E-001 1.00000E+001 IT 5.50000E-001 9.84000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.92000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.96000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM M-FDS910 1 821241 1.82115 24.06 0 1 1 GC Glass for molded optics lens ED 9.500000000E+000 1.210000000E+001 3.690000000E+000 1.870000000E-002 0 0 CD 3.165987000E+000 -1.349196000E-002 4.649918000E-002 2.471413000E-003 -8.659596000E-005 2.725927000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.807070000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.90000E-002 1.00000E+001 IT 3.80000E-001 1.50000E-001 1.00000E+001 IT 3.90000E-001 3.92000E-001 1.00000E+001 IT 4.00000E-001 5.96000E-001 1.00000E+001 IT 4.20000E-001 7.95000E-001 1.00000E+001 IT 4.40000E-001 8.77000E-001 1.00000E+001 IT 4.60000E-001 9.18000E-001 1.00000E+001 IT 4.80000E-001 9.44000E-001 1.00000E+001 IT 5.00000E-001 9.62000E-001 1.00000E+001 IT 5.50000E-001 9.88000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM MP-FDS910-50 1 822240 1.82165 24.04 0 1 1 GC Preforms for Precision molding ED 9.500000000E+000 1.210000000E+001 3.690000000E+000 1.870000000E-002 0 0 CD 3.166790200E+000 -1.314141600E-002 4.717865600E-002 2.268428400E-003 -5.367238700E-005 2.532842200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.805600000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.90000E-002 1.00000E+001 IT 3.80000E-001 1.50000E-001 1.00000E+001 IT 3.90000E-001 3.92000E-001 1.00000E+001 IT 4.00000E-001 5.96000E-001 1.00000E+001 IT 4.20000E-001 7.95000E-001 1.00000E+001 IT 4.40000E-001 8.77000E-001 1.00000E+001 IT 4.60000E-001 9.18000E-001 1.00000E+001 IT 4.80000E-001 9.44000E-001 1.00000E+001 IT 5.00000E-001 9.62000E-001 1.00000E+001 IT 5.50000E-001 9.88000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM MC-FDS910-50 1 822240 1.82165 24.04 0 1 1 GC Preforms for Precision molding ED 9.500000000E+000 1.210000000E+001 3.690000000E+000 1.870000000E-002 0 0 CD 3.166790200E+000 -1.314141600E-002 4.717865600E-002 2.268428400E-003 -5.367238700E-005 2.532842200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD -2.805600000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.70000E-001 1.50000E-002 1.00000E+001 IT 3.80000E-001 2.04000E-001 1.00000E+001 IT 3.90000E-001 5.31000E-001 1.00000E+001 IT 4.00000E-001 7.37000E-001 1.00000E+001 IT 4.20000E-001 8.85000E-001 1.00000E+001 IT 4.40000E-001 9.30000E-001 1.00000E+001 IT 4.60000E-001 9.52000E-001 1.00000E+001 IT 4.80000E-001 9.65000E-001 1.00000E+001 IT 5.00000E-001 9.75000E-001 1.00000E+001 IT 5.50000E-001 9.90000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.92000E-001 1.00000E+001 IT 7.00000E-001 9.94000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM M-NBFD10 1 834373 1.83441 37.28 0 1 1 GC Glass for molded optics lens ED 6.100000000E+000 7.700000000E+000 4.390000000E+000 -4.000000000E-003 0 0 CD 3.264623000E+000 -1.581977000E-002 3.225894000E-002 1.709312000E-003 -1.081957000E-004 1.058323000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.486610000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.09000E-001 1.00000E+001 IT 3.60000E-001 3.61000E-001 1.00000E+001 IT 3.70000E-001 6.03000E-001 1.00000E+001 IT 3.80000E-001 7.45000E-001 1.00000E+001 IT 3.90000E-001 8.27000E-001 1.00000E+001 IT 4.00000E-001 8.76000E-001 1.00000E+001 IT 4.20000E-001 9.29000E-001 1.00000E+001 IT 4.40000E-001 9.55000E-001 1.00000E+001 IT 4.60000E-001 9.70000E-001 1.00000E+001 IT 4.80000E-001 9.81000E-001 1.00000E+001 IT 5.00000E-001 9.89000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM MP-NBFD10-20 1 835373 1.83461 37.29 0 1 1 GC Preforms for Precision molding ED 6.100000000E+000 7.700000000E+000 4.390000000E+000 -4.700000000E-003 0 0 CD 3.272258600E+000 -1.881721100E-002 2.726450800E-002 3.278919300E-003 -3.282767200E-004 2.174336200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.484920000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 1.09000E-001 1.00000E+001 IT 3.60000E-001 3.61000E-001 1.00000E+001 IT 3.70000E-001 6.03000E-001 1.00000E+001 IT 3.80000E-001 7.45000E-001 1.00000E+001 IT 3.90000E-001 8.27000E-001 1.00000E+001 IT 4.00000E-001 8.76000E-001 1.00000E+001 IT 4.20000E-001 9.29000E-001 1.00000E+001 IT 4.40000E-001 9.55000E-001 1.00000E+001 IT 4.60000E-001 9.70000E-001 1.00000E+001 IT 4.80000E-001 9.81000E-001 1.00000E+001 IT 5.00000E-001 9.89000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.97000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM M-NBFD130 1 806407 1.80610 40.73 0 1 1 GC Glass for molded optics lens ED 5.800000000E+000 7.400000000E+000 4.560000000E+000 -5.600000000E-003 0 0 CD 3.173794000E+000 -1.498658000E-002 2.906741000E-002 1.204829000E-003 -5.355158000E-005 5.271350000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.032930000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 9.50000E-002 1.00000E+001 IT 3.50000E-001 3.34000E-001 1.00000E+001 IT 3.60000E-001 6.05000E-001 1.00000E+001 IT 3.70000E-001 7.79000E-001 1.00000E+001 IT 3.80000E-001 8.68000E-001 1.00000E+001 IT 3.90000E-001 9.16000E-001 1.00000E+001 IT 4.00000E-001 9.43000E-001 1.00000E+001 IT 4.20000E-001 9.68000E-001 1.00000E+001 IT 4.40000E-001 9.79000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.92000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.91000E-001 1.00000E+001 IT 8.50000E-001 9.91000E-001 1.00000E+001 IT 9.00000E-001 9.91000E-001 1.00000E+001 IT 9.50000E-001 9.92000E-001 1.00000E+001 IT 1.00000E+000 9.92000E-001 1.00000E+001 IT 1.05000E+000 9.93000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.94000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MP-NBFD130 1 806407 1.80610 40.73 0 1 1 GC Preforms for Precision molding ED 5.800000000E+000 7.400000000E+000 4.560000000E+000 -5.600000000E-003 0 0 CD 3.173794000E+000 -1.498658000E-002 2.906741000E-002 1.204829000E-003 -5.355158000E-005 5.271350000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.032930000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 9.50000E-002 1.00000E+001 IT 3.50000E-001 3.34000E-001 1.00000E+001 IT 3.60000E-001 6.05000E-001 1.00000E+001 IT 3.70000E-001 7.79000E-001 1.00000E+001 IT 3.80000E-001 8.68000E-001 1.00000E+001 IT 3.90000E-001 9.16000E-001 1.00000E+001 IT 4.00000E-001 9.43000E-001 1.00000E+001 IT 4.20000E-001 9.68000E-001 1.00000E+001 IT 4.40000E-001 9.79000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.92000E-001 1.00000E+001 IT 8.00000E-001 9.93000E-001 1.00000E+001 IT 8.30000E-001 9.91000E-001 1.00000E+001 IT 8.50000E-001 9.91000E-001 1.00000E+001 IT 9.00000E-001 9.91000E-001 1.00000E+001 IT 9.50000E-001 9.92000E-001 1.00000E+001 IT 1.00000E+000 9.92000E-001 1.00000E+001 IT 1.05000E+000 9.93000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.94000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.93000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MC-NBFD135 1 808409 1.80834 40.92 0 1 1 GC Preforms for Precision molding ED 6.200000000E+000 8.000000000E+000 4.670000000E+000 -6.100000000E-003 0 0 CD 3.181969800E+000 -1.492652200E-002 2.898764900E-002 1.222365400E-003 -5.291668800E-005 4.780722700E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 9.988370000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 1.42000E-001 1.00000E+001 IT 3.50000E-001 4.51000E-001 1.00000E+001 IT 3.60000E-001 7.13000E-001 1.00000E+001 IT 3.70000E-001 8.48000E-001 1.00000E+001 IT 3.80000E-001 9.14000E-001 1.00000E+001 IT 3.90000E-001 9.45000E-001 1.00000E+001 IT 4.00000E-001 9.63000E-001 1.00000E+001 IT 4.20000E-001 9.78000E-001 1.00000E+001 IT 4.40000E-001 9.85000E-001 1.00000E+001 IT 4.60000E-001 9.89000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM M-TAF31 1 801455 1.80139 45.45 0 1 1 GC Glass for molded optics lens ED 6.200000000E+000 7.700000000E+000 4.840000000E+000 -8.300000000E-003 0 0 CD 3.164358000E+000 -1.403321000E-002 2.767034000E-002 6.403025000E-004 -6.349234000E-006 1.615744000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.669320000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 3.20000E-002 1.00000E+001 IT 3.00000E-001 7.20000E-002 1.00000E+001 IT 3.10000E-001 1.28000E-001 1.00000E+001 IT 3.20000E-001 2.58000E-001 1.00000E+001 IT 3.30000E-001 4.09000E-001 1.00000E+001 IT 3.40000E-001 5.55000E-001 1.00000E+001 IT 3.50000E-001 6.90000E-001 1.00000E+001 IT 3.60000E-001 8.01000E-001 1.00000E+001 IT 3.70000E-001 8.76000E-001 1.00000E+001 IT 3.80000E-001 9.22000E-001 1.00000E+001 IT 3.90000E-001 9.48000E-001 1.00000E+001 IT 4.00000E-001 9.64000E-001 1.00000E+001 IT 4.20000E-001 9.79000E-001 1.00000E+001 IT 4.40000E-001 9.86000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM MP-TAF31-15 1 802455 1.80154 45.46 0 1 1 GC Preforms for Precision molding ED 6.200000000E+000 7.700000000E+000 4.840000000E+000 -8.400000000E-003 0 0 CD 3.164475000E+000 -1.380129500E-002 2.792627600E-002 5.740300000E-004 9.822377300E-007 1.328424400E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.668120000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 3.20000E-002 1.00000E+001 IT 3.00000E-001 7.20000E-002 1.00000E+001 IT 3.10000E-001 1.28000E-001 1.00000E+001 IT 3.20000E-001 2.58000E-001 1.00000E+001 IT 3.30000E-001 4.09000E-001 1.00000E+001 IT 3.40000E-001 5.55000E-001 1.00000E+001 IT 3.50000E-001 6.90000E-001 1.00000E+001 IT 3.60000E-001 8.01000E-001 1.00000E+001 IT 3.70000E-001 8.76000E-001 1.00000E+001 IT 3.80000E-001 9.22000E-001 1.00000E+001 IT 3.90000E-001 9.48000E-001 1.00000E+001 IT 4.00000E-001 9.64000E-001 1.00000E+001 IT 4.20000E-001 9.79000E-001 1.00000E+001 IT 4.40000E-001 9.86000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.99000E-001 1.00000E+001 IT 1.50000E+000 9.99000E-001 1.00000E+001 IT 1.55000E+000 9.99000E-001 1.00000E+001 NM MC-TAF31-15 1 802455 1.80154 45.46 0 1 1 GC Preforms for Precision molding ED 6.200000000E+000 7.700000000E+000 4.840000000E+000 -8.400000000E-003 0 0 CD 3.164475000E+000 -1.380129500E-002 2.792627600E-002 5.740300000E-004 9.822377300E-007 1.328424400E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.668120000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 3.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.80000E-002 1.00000E+001 IT 2.90000E-001 1.15000E-001 1.00000E+001 IT 3.00000E-001 2.19000E-001 1.00000E+001 IT 3.10000E-001 2.48000E-001 1.00000E+001 IT 3.20000E-001 4.68000E-001 1.00000E+001 IT 3.30000E-001 6.04000E-001 1.00000E+001 IT 3.40000E-001 7.20000E-001 1.00000E+001 IT 3.50000E-001 8.14000E-001 1.00000E+001 IT 3.60000E-001 8.86000E-001 1.00000E+001 IT 3.70000E-001 9.28000E-001 1.00000E+001 IT 3.80000E-001 9.55000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.78000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM M-TAF101 1 768492 1.76802 49.24 0 1 1 GC Glass for molded optics lens ED 5.900000000E+000 7.400000000E+000 4.560000000E+000 -8.100000000E-003 0 0 CD 3.056150000E+000 -1.384710000E-002 2.431126000E-002 4.980027000E-004 -7.318676000E-006 1.240410000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.692430000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.20000E-002 1.00000E+001 IT 2.90000E-001 1.14000E-001 1.00000E+001 IT 3.00000E-001 1.95000E-001 1.00000E+001 IT 3.10000E-001 2.57000E-001 1.00000E+001 IT 3.20000E-001 4.32000E-001 1.00000E+001 IT 3.30000E-001 6.01000E-001 1.00000E+001 IT 3.40000E-001 7.19000E-001 1.00000E+001 IT 3.50000E-001 8.14000E-001 1.00000E+001 IT 3.60000E-001 8.84000E-001 1.00000E+001 IT 3.70000E-001 9.30000E-001 1.00000E+001 IT 3.80000E-001 9.55000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.79000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-TAF101-100 1 769493 1.76902 49.29 0 1 1 GC Preforms for Precision molding ED 5.900000000E+000 7.400000000E+000 4.560000000E+000 -8.000000000E-003 0 0 CD 3.059156600E+000 -1.360471700E-002 2.462427200E-002 4.183424200E-004 2.536190800E-006 7.998082000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.692430000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.20000E-002 1.00000E+001 IT 2.90000E-001 1.14000E-001 1.00000E+001 IT 3.00000E-001 1.95000E-001 1.00000E+001 IT 3.10000E-001 2.57000E-001 1.00000E+001 IT 3.20000E-001 4.32000E-001 1.00000E+001 IT 3.30000E-001 6.01000E-001 1.00000E+001 IT 3.40000E-001 7.19000E-001 1.00000E+001 IT 3.50000E-001 8.14000E-001 1.00000E+001 IT 3.60000E-001 8.84000E-001 1.00000E+001 IT 3.70000E-001 9.30000E-001 1.00000E+001 IT 3.80000E-001 9.55000E-001 1.00000E+001 IT 3.90000E-001 9.70000E-001 1.00000E+001 IT 4.00000E-001 9.79000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.97000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-TAF101-100 1 769493 1.76902 49.29 0 1 1 GC Preforms for Precision molding ED 5.900000000E+000 7.400000000E+000 4.560000000E+000 -8.000000000E-003 0 0 CD 3.059156600E+000 -1.360471700E-002 2.462427200E-002 4.183424200E-004 2.536190800E-006 7.998082000E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.692430000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 7.10000E-002 1.00000E+001 IT 2.90000E-001 1.97000E-001 1.00000E+001 IT 3.00000E-001 2.95000E-001 1.00000E+001 IT 3.10000E-001 2.89000E-001 1.00000E+001 IT 3.20000E-001 5.43000E-001 1.00000E+001 IT 3.30000E-001 6.68000E-001 1.00000E+001 IT 3.40000E-001 7.70000E-001 1.00000E+001 IT 3.50000E-001 8.50000E-001 1.00000E+001 IT 3.60000E-001 9.05000E-001 1.00000E+001 IT 3.70000E-001 9.44000E-001 1.00000E+001 IT 3.80000E-001 9.64000E-001 1.00000E+001 IT 3.90000E-001 9.76000E-001 1.00000E+001 IT 4.00000E-001 9.83000E-001 1.00000E+001 IT 4.20000E-001 9.89000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.92000E-001 1.00000E+001 IT 1.50000E+000 9.92000E-001 1.00000E+001 IT 1.55000E+000 9.93000E-001 1.00000E+001 NM M-TAF105 1 773495 1.77250 49.50 0 1 1 GC Glass for molded optics lens ED 5.700000000E+000 7.000000000E+000 4.620000000E+000 -7.200000000E-003 0 0 CD 3.070563800E+000 -1.331023400E-002 2.528035500E-002 2.182923400E-004 3.255529300E-005 -8.130042100E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.740000000E-006 9.550000000E-009 -5.150000000E-011 6.480000000E-007 3.610000000E-010 1.660000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.00000E-002 1.00000E+001 IT 2.90000E-001 1.05000E-001 1.00000E+001 IT 3.00000E-001 1.95000E-001 1.00000E+001 IT 3.10000E-001 2.16000E-001 1.00000E+001 IT 3.20000E-001 4.52000E-001 1.00000E+001 IT 3.30000E-001 5.91000E-001 1.00000E+001 IT 3.40000E-001 7.10000E-001 1.00000E+001 IT 3.50000E-001 8.07000E-001 1.00000E+001 IT 3.60000E-001 8.81000E-001 1.00000E+001 IT 3.70000E-001 9.24000E-001 1.00000E+001 IT 3.80000E-001 9.51000E-001 1.00000E+001 IT 3.90000E-001 9.67000E-001 1.00000E+001 IT 4.00000E-001 9.76000E-001 1.00000E+001 IT 4.20000E-001 9.85000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MP-TAF105 1 773495 1.77250 49.50 0 1 1 GC Preforms for Precision molding ED 5.700000000E+000 7.000000000E+000 4.620000000E+000 -7.200000000E-003 0 0 CD 3.070563800E+000 -1.331023400E-002 2.528035500E-002 2.182923400E-004 3.255529300E-005 -8.130042100E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.740000000E-006 9.550000000E-009 -5.150000000E-011 6.480000000E-007 3.610000000E-010 1.660000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.00000E-002 1.00000E+001 IT 2.90000E-001 1.05000E-001 1.00000E+001 IT 3.00000E-001 1.95000E-001 1.00000E+001 IT 3.10000E-001 2.16000E-001 1.00000E+001 IT 3.20000E-001 4.52000E-001 1.00000E+001 IT 3.30000E-001 5.91000E-001 1.00000E+001 IT 3.40000E-001 7.10000E-001 1.00000E+001 IT 3.50000E-001 8.07000E-001 1.00000E+001 IT 3.60000E-001 8.81000E-001 1.00000E+001 IT 3.70000E-001 9.24000E-001 1.00000E+001 IT 3.80000E-001 9.51000E-001 1.00000E+001 IT 3.90000E-001 9.67000E-001 1.00000E+001 IT 4.00000E-001 9.76000E-001 1.00000E+001 IT 4.20000E-001 9.85000E-001 1.00000E+001 IT 4.40000E-001 9.89000E-001 1.00000E+001 IT 4.60000E-001 9.92000E-001 1.00000E+001 IT 4.80000E-001 9.94000E-001 1.00000E+001 IT 5.00000E-001 9.96000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.97000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-TAF105 1 773495 1.77250 49.50 0 1 1 GC Preforms for Precision molding ED 5.700000000E+000 7.000000000E+000 4.620000000E+000 -7.200000000E-003 0 0 CD 3.070563800E+000 -1.331023400E-002 2.528035500E-002 2.182923400E-004 3.255529300E-005 -8.130042100E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 4.740000000E-006 9.550000000E-009 -5.150000000E-011 6.480000000E-007 3.610000000E-010 1.660000000E-001 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 2.40000E-002 1.00000E+001 IT 2.90000E-001 9.80000E-002 1.00000E+001 IT 3.00000E-001 1.93000E-001 1.00000E+001 IT 3.10000E-001 2.15000E-001 1.00000E+001 IT 3.20000E-001 4.68000E-001 1.00000E+001 IT 3.30000E-001 6.07000E-001 1.00000E+001 IT 3.40000E-001 7.29000E-001 1.00000E+001 IT 3.50000E-001 8.26000E-001 1.00000E+001 IT 3.60000E-001 8.92000E-001 1.00000E+001 IT 3.70000E-001 9.39000E-001 1.00000E+001 IT 3.80000E-001 9.62000E-001 1.00000E+001 IT 3.90000E-001 9.77000E-001 1.00000E+001 IT 4.00000E-001 9.84000E-001 1.00000E+001 IT 4.20000E-001 9.91000E-001 1.00000E+001 IT 4.40000E-001 9.95000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.99000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.97000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.94000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM M-TAF401 1 774472 1.77377 47.17 0 1 1 GC Glass for molded optics lens ED 6.100000000E+000 7.700000000E+000 4.620000000E+000 -7.800000000E-003 0 0 CD 3.072790000E+000 -1.366385000E-002 2.527346000E-002 6.121820000E-004 -1.147045000E-005 1.543000000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.394120000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 1.20000E-002 1.00000E+001 IT 3.20000E-001 4.00000E-002 1.00000E+001 IT 3.30000E-001 2.00000E-001 1.00000E+001 IT 3.40000E-001 4.51000E-001 1.00000E+001 IT 3.50000E-001 6.63000E-001 1.00000E+001 IT 3.60000E-001 8.04000E-001 1.00000E+001 IT 3.70000E-001 8.86000E-001 1.00000E+001 IT 3.80000E-001 9.28000E-001 1.00000E+001 IT 3.90000E-001 9.52000E-001 1.00000E+001 IT 4.00000E-001 9.66000E-001 1.00000E+001 IT 4.20000E-001 9.78000E-001 1.00000E+001 IT 4.40000E-001 9.85000E-001 1.00000E+001 IT 4.60000E-001 9.89000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.93000E-001 1.00000E+001 IT 8.00000E-001 9.92000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.93000E-001 1.00000E+001 IT 9.00000E-001 9.94000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.94000E-001 1.00000E+001 IT 1.05000E+000 9.95000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM MP-TAF401 1 774472 1.77377 47.17 0 1 1 GC Preforms for Precision molding ED 6.100000000E+000 7.700000000E+000 4.620000000E+000 -7.800000000E-003 0 0 CD 3.072790000E+000 -1.366385000E-002 2.527346000E-002 6.121820000E-004 -1.147045000E-005 1.543000000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.394120000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.10000E-001 1.20000E-002 1.00000E+001 IT 3.20000E-001 4.00000E-002 1.00000E+001 IT 3.30000E-001 2.00000E-001 1.00000E+001 IT 3.40000E-001 4.51000E-001 1.00000E+001 IT 3.50000E-001 6.63000E-001 1.00000E+001 IT 3.60000E-001 8.04000E-001 1.00000E+001 IT 3.70000E-001 8.86000E-001 1.00000E+001 IT 3.80000E-001 9.28000E-001 1.00000E+001 IT 3.90000E-001 9.52000E-001 1.00000E+001 IT 4.00000E-001 9.66000E-001 1.00000E+001 IT 4.20000E-001 9.78000E-001 1.00000E+001 IT 4.40000E-001 9.85000E-001 1.00000E+001 IT 4.60000E-001 9.89000E-001 1.00000E+001 IT 4.80000E-001 9.92000E-001 1.00000E+001 IT 5.00000E-001 9.94000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.95000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.97000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.93000E-001 1.00000E+001 IT 8.00000E-001 9.92000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.93000E-001 1.00000E+001 IT 9.00000E-001 9.94000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.94000E-001 1.00000E+001 IT 1.05000E+000 9.95000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM MC-TAF401 1 774472 1.77377 47.17 0 1 1 GC Preforms for Precision molding ED 6.100000000E+000 7.700000000E+000 4.620000000E+000 -7.800000000E-003 0 0 CD 3.072790000E+000 -1.366385000E-002 2.527346000E-002 6.121820000E-004 -1.147045000E-005 1.543000000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.394120000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.20000E-001 1.11000E-001 1.00000E+001 IT 3.30000E-001 3.31000E-001 1.00000E+001 IT 3.40000E-001 5.60000E-001 1.00000E+001 IT 3.50000E-001 7.26000E-001 1.00000E+001 IT 3.60000E-001 8.40000E-001 1.00000E+001 IT 3.70000E-001 9.07000E-001 1.00000E+001 IT 3.80000E-001 9.43000E-001 1.00000E+001 IT 3.90000E-001 9.62000E-001 1.00000E+001 IT 4.00000E-001 9.75000E-001 1.00000E+001 IT 4.20000E-001 9.84000E-001 1.00000E+001 IT 4.40000E-001 9.88000E-001 1.00000E+001 IT 4.60000E-001 9.91000E-001 1.00000E+001 IT 4.80000E-001 9.91000E-001 1.00000E+001 IT 5.00000E-001 9.91000E-001 1.00000E+001 IT 5.50000E-001 9.91000E-001 1.00000E+001 IT 6.00000E-001 9.91000E-001 1.00000E+001 IT 6.50000E-001 9.91000E-001 1.00000E+001 IT 7.00000E-001 9.91000E-001 1.00000E+001 IT 7.50000E-001 9.93000E-001 1.00000E+001 IT 7.80000E-001 9.93000E-001 1.00000E+001 IT 8.00000E-001 9.92000E-001 1.00000E+001 IT 8.30000E-001 9.92000E-001 1.00000E+001 IT 8.50000E-001 9.93000E-001 1.00000E+001 IT 9.00000E-001 9.94000E-001 1.00000E+001 IT 9.50000E-001 9.95000E-001 1.00000E+001 IT 1.00000E+000 9.94000E-001 1.00000E+001 IT 1.05000E+000 9.95000E-001 1.00000E+001 IT 1.06000E+000 9.95000E-001 1.00000E+001 IT 1.10000E+000 9.95000E-001 1.00000E+001 IT 1.20000E+000 9.96000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.95000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.94000E-001 1.00000E+001 NM M-TAFD51 1 821427 1.82080 42.71 0 1 1 GC Glass for molded optics lens ED 6.400000000E+000 7.700000000E+000 5.010000000E+000 -7.200000000E-003 0 0 CD 3.227682000E+000 -1.453816000E-002 2.921210000E-002 1.057062000E-003 -4.787162000E-005 4.557239000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.044810000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 9.30000E-002 1.00000E+001 IT 3.50000E-001 3.23000E-001 1.00000E+001 IT 3.60000E-001 5.85000E-001 1.00000E+001 IT 3.70000E-001 7.59000E-001 1.00000E+001 IT 3.80000E-001 8.52000E-001 1.00000E+001 IT 3.90000E-001 9.03000E-001 1.00000E+001 IT 4.00000E-001 9.33000E-001 1.00000E+001 IT 4.20000E-001 9.61000E-001 1.00000E+001 IT 4.40000E-001 9.74000E-001 1.00000E+001 IT 4.60000E-001 9.82000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-TAFD51-50 1 821427 1.82130 42.72 0 1 1 GC Preforms for Precision molding ED 6.400000000E+000 7.700000000E+000 5.010000000E+000 -6.500000000E-003 0 0 CD 3.228805200E+000 -1.443304600E-002 2.986348800E-002 8.211928200E-004 -1.094349200E-005 2.580493900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.041230000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 9.30000E-002 1.00000E+001 IT 3.50000E-001 3.23000E-001 1.00000E+001 IT 3.60000E-001 5.85000E-001 1.00000E+001 IT 3.70000E-001 7.59000E-001 1.00000E+001 IT 3.80000E-001 8.52000E-001 1.00000E+001 IT 3.90000E-001 9.03000E-001 1.00000E+001 IT 4.00000E-001 9.33000E-001 1.00000E+001 IT 4.20000E-001 9.61000E-001 1.00000E+001 IT 4.40000E-001 9.74000E-001 1.00000E+001 IT 4.60000E-001 9.82000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.97000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MC-TAFD51-50 1 821427 1.82130 42.72 0 1 1 GC Preforms for Precision molding ED 6.400000000E+000 7.700000000E+000 5.010000000E+000 -6.500000000E-003 0 0 CD 3.228805200E+000 -1.443304600E-002 2.986348800E-002 8.211928200E-004 -1.094349200E-005 2.580493900E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.041230000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 8.80000E-002 1.00000E+001 IT 3.50000E-001 3.69000E-001 1.00000E+001 IT 3.60000E-001 6.66000E-001 1.00000E+001 IT 3.70000E-001 8.21000E-001 1.00000E+001 IT 3.80000E-001 9.00000E-001 1.00000E+001 IT 3.90000E-001 9.40000E-001 1.00000E+001 IT 4.00000E-001 9.60000E-001 1.00000E+001 IT 4.20000E-001 9.79000E-001 1.00000E+001 IT 4.40000E-001 9.85000E-001 1.00000E+001 IT 4.60000E-001 9.90000E-001 1.00000E+001 IT 4.80000E-001 9.93000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM M-TAFD305 1 851401 1.85135 40.10 0 1 1 GC Glass for molded optics lens ED 6.000000000E+000 7.800000000E+000 5.250000000E+000 -6.700000000E-003 0 0 CD 3.327184000E+000 -1.343242000E-002 3.339800000E-002 1.006047000E-003 -2.136908000E-005 3.972561000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.250000000E-006 1.170000000E-008 -4.510000000E-011 1.250000000E-006 1.270000000E-009 4.550000000E-002 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 3.90000E-002 1.00000E+001 IT 3.50000E-001 2.08000E-001 1.00000E+001 IT 3.60000E-001 4.81000E-001 1.00000E+001 IT 3.70000E-001 6.98000E-001 1.00000E+001 IT 3.80000E-001 8.20000E-001 1.00000E+001 IT 3.90000E-001 8.88000E-001 1.00000E+001 IT 4.00000E-001 9.27000E-001 1.00000E+001 IT 4.20000E-001 9.61000E-001 1.00000E+001 IT 4.40000E-001 9.76000E-001 1.00000E+001 IT 4.60000E-001 9.84000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.94000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.93000E-001 1.00000E+001 IT 9.50000E-001 9.94000E-001 1.00000E+001 IT 1.00000E+000 9.93000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.94000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MP-TAFD305 1 851401 1.85135 40.10 0 1 1 GC Preforms for Precision molding ED 6.000000000E+000 7.800000000E+000 5.250000000E+000 -6.700000000E-003 0 0 CD 3.327184000E+000 -1.343242000E-002 3.339800000E-002 1.006047000E-003 -2.136908000E-005 3.972561000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.250000000E-006 1.170000000E-008 -4.510000000E-011 1.250000000E-006 1.270000000E-009 4.550000000E-002 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 3.90000E-002 1.00000E+001 IT 3.50000E-001 2.08000E-001 1.00000E+001 IT 3.60000E-001 4.81000E-001 1.00000E+001 IT 3.70000E-001 6.98000E-001 1.00000E+001 IT 3.80000E-001 8.20000E-001 1.00000E+001 IT 3.90000E-001 8.88000E-001 1.00000E+001 IT 4.00000E-001 9.27000E-001 1.00000E+001 IT 4.20000E-001 9.61000E-001 1.00000E+001 IT 4.40000E-001 9.76000E-001 1.00000E+001 IT 4.60000E-001 9.84000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.99000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.94000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.93000E-001 1.00000E+001 IT 9.50000E-001 9.94000E-001 1.00000E+001 IT 1.00000E+000 9.93000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.94000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MC-TAFD305 1 851401 1.85135 40.10 0 1 1 GC Preforms for Precision molding ED 6.000000000E+000 7.800000000E+000 5.250000000E+000 -6.700000000E-003 0 0 CD 3.327184000E+000 -1.343242000E-002 3.339800000E-002 1.006047000E-003 -2.136908000E-005 3.972561000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.250000000E-006 1.170000000E-008 -4.510000000E-011 1.250000000E-006 1.270000000E-009 4.550000000E-002 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.40000E-001 2.40000E-002 1.00000E+001 IT 3.50000E-001 2.04000E-001 1.00000E+001 IT 3.60000E-001 5.09000E-001 1.00000E+001 IT 3.70000E-001 7.24000E-001 1.00000E+001 IT 3.80000E-001 8.45000E-001 1.00000E+001 IT 3.90000E-001 9.06000E-001 1.00000E+001 IT 4.00000E-001 9.39000E-001 1.00000E+001 IT 4.20000E-001 9.70000E-001 1.00000E+001 IT 4.40000E-001 9.79000E-001 1.00000E+001 IT 4.60000E-001 9.86000E-001 1.00000E+001 IT 4.80000E-001 9.90000E-001 1.00000E+001 IT 5.00000E-001 9.95000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.95000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.95000E-001 1.00000E+001 IT 7.80000E-001 9.95000E-001 1.00000E+001 IT 8.00000E-001 9.94000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.93000E-001 1.00000E+001 IT 9.50000E-001 9.94000E-001 1.00000E+001 IT 1.00000E+000 9.93000E-001 1.00000E+001 IT 1.05000E+000 9.94000E-001 1.00000E+001 IT 1.06000E+000 9.94000E-001 1.00000E+001 IT 1.10000E+000 9.94000E-001 1.00000E+001 IT 1.20000E+000 9.95000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM M-TAFD307 1 882372 1.88202 37.22 0 1 1 GC Glass for molded optics lens ED 6.700000000E+000 7.300000000E+000 5.490000000E+000 -4.400000000E-003 0 0 CD 3.428606200E+000 -1.384533300E-002 3.736300900E-002 1.189455400E-003 -1.597997900E-005 5.182739800E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.806220000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 5.40000E-002 1.00000E+001 IT 3.60000E-001 2.54000E-001 1.00000E+001 IT 3.70000E-001 5.17000E-001 1.00000E+001 IT 3.80000E-001 7.03000E-001 1.00000E+001 IT 3.90000E-001 8.13000E-001 1.00000E+001 IT 4.00000E-001 8.75000E-001 1.00000E+001 IT 4.20000E-001 9.34000E-001 1.00000E+001 IT 4.40000E-001 9.58000E-001 1.00000E+001 IT 4.60000E-001 9.71000E-001 1.00000E+001 IT 4.80000E-001 9.80000E-001 1.00000E+001 IT 5.00000E-001 9.87000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-TAFD307 1 882372 1.88202 37.22 0 1 1 GC Preforms for Precision molding ED 6.700000000E+000 7.300000000E+000 5.490000000E+000 -4.400000000E-003 0 0 CD 3.428606200E+000 -1.384533300E-002 3.736300900E-002 1.189455400E-003 -1.597997900E-005 5.182739800E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.806220000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 5.40000E-002 1.00000E+001 IT 3.60000E-001 2.54000E-001 1.00000E+001 IT 3.70000E-001 5.17000E-001 1.00000E+001 IT 3.80000E-001 7.03000E-001 1.00000E+001 IT 3.90000E-001 8.13000E-001 1.00000E+001 IT 4.00000E-001 8.75000E-001 1.00000E+001 IT 4.20000E-001 9.34000E-001 1.00000E+001 IT 4.40000E-001 9.58000E-001 1.00000E+001 IT 4.60000E-001 9.71000E-001 1.00000E+001 IT 4.80000E-001 9.80000E-001 1.00000E+001 IT 5.00000E-001 9.87000E-001 1.00000E+001 IT 5.50000E-001 9.96000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MC-TAFD307 1 882372 1.88202 37.22 0 1 1 GC Preforms for Precision molding ED 6.700000000E+000 7.300000000E+000 5.490000000E+000 -4.400000000E-003 0 0 CD 3.428606200E+000 -1.384533300E-002 3.736300900E-002 1.189455400E-003 -1.597997900E-005 5.182739800E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 7.806220000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.50000E-001 4.10000E-002 1.00000E+001 IT 3.60000E-001 2.57000E-001 1.00000E+001 IT 3.70000E-001 5.71000E-001 1.00000E+001 IT 3.80000E-001 7.49000E-001 1.00000E+001 IT 3.90000E-001 8.47000E-001 1.00000E+001 IT 4.00000E-001 8.98000E-001 1.00000E+001 IT 4.20000E-001 9.46000E-001 1.00000E+001 IT 4.40000E-001 9.65000E-001 1.00000E+001 IT 4.60000E-001 9.75000E-001 1.00000E+001 IT 4.80000E-001 9.81000E-001 1.00000E+001 IT 5.00000E-001 9.86000E-001 1.00000E+001 IT 5.50000E-001 9.93000E-001 1.00000E+001 IT 6.00000E-001 9.94000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.96000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.97000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM M-TAFD405 1 952298 1.95150 29.83 0 1 1 GC Glass for molded optics lens ED 6.000000000E+000 7.600000000E+000 5.450000000E+000 1.100000000E-003 0 0 CD 3.654235200E+000 -1.568832500E-002 4.809408900E-002 2.649806500E-003 -1.397185200E-004 1.958120100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.145880000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.50000E-002 1.00000E+001 IT 3.70000E-001 1.69000E-001 1.00000E+001 IT 3.80000E-001 4.02000E-001 1.00000E+001 IT 3.90000E-001 5.80000E-001 1.00000E+001 IT 4.00000E-001 6.94000E-001 1.00000E+001 IT 4.20000E-001 8.22000E-001 1.00000E+001 IT 4.40000E-001 8.87000E-001 1.00000E+001 IT 4.60000E-001 9.24000E-001 1.00000E+001 IT 4.80000E-001 9.47000E-001 1.00000E+001 IT 5.00000E-001 9.65000E-001 1.00000E+001 IT 5.50000E-001 9.89000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.95000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM MP-TAFD405 1 952298 1.95150 29.83 0 1 1 GC Preforms for Precision molding ED 6.000000000E+000 7.600000000E+000 5.450000000E+000 1.100000000E-003 0 0 CD 3.654235200E+000 -1.568832500E-002 4.809408900E-002 2.649806500E-003 -1.397185200E-004 1.958120100E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 8.145880000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 2.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.60000E-001 1.50000E-002 1.00000E+001 IT 3.70000E-001 1.69000E-001 1.00000E+001 IT 3.80000E-001 4.02000E-001 1.00000E+001 IT 3.90000E-001 5.80000E-001 1.00000E+001 IT 4.00000E-001 6.94000E-001 1.00000E+001 IT 4.20000E-001 8.22000E-001 1.00000E+001 IT 4.40000E-001 8.87000E-001 1.00000E+001 IT 4.60000E-001 9.24000E-001 1.00000E+001 IT 4.80000E-001 9.47000E-001 1.00000E+001 IT 5.00000E-001 9.65000E-001 1.00000E+001 IT 5.50000E-001 9.89000E-001 1.00000E+001 IT 6.00000E-001 9.96000E-001 1.00000E+001 IT 6.50000E-001 9.96000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.95000E-001 1.00000E+001 IT 8.50000E-001 9.94000E-001 1.00000E+001 IT 9.00000E-001 9.96000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.98000E-001 1.00000E+001 IT 1.55000E+000 9.98000E-001 1.00000E+001 NM M-LAC8 1 713539 1.71300 53.94 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.300000000E+000 7.900000000E+000 3.900000000E+000 -6.400000000E-003 0 0 CD 2.881748100E+000 -1.573080400E-002 1.769049300E-002 1.052669000E-003 -9.909308000E-005 5.524837800E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.470020000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 5.00000E-002 1.00000E+001 IT 3.00000E-001 1.10000E-001 1.00000E+001 IT 3.10000E-001 1.70000E-001 1.00000E+001 IT 3.20000E-001 3.50000E-001 1.00000E+001 IT 3.30000E-001 5.10000E-001 1.00000E+001 IT 3.40000E-001 6.60000E-001 1.00000E+001 IT 3.50000E-001 7.80000E-001 1.00000E+001 IT 3.60000E-001 8.60000E-001 1.00000E+001 IT 3.70000E-001 9.22000E-001 1.00000E+001 IT 3.80000E-001 9.52000E-001 1.00000E+001 IT 3.90000E-001 9.68000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-LAC8-30 1 713539 1.71330 53.95 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 6.300000000E+000 7.900000000E+000 3.900000000E+000 -6.400000000E-003 0 0 CD 2.882749800E+000 -1.574078900E-002 1.770797600E-002 1.048326500E-003 -9.833281100E-005 5.482868500E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 5.468080000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 2.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.90000E-001 5.00000E-002 1.00000E+001 IT 3.00000E-001 1.10000E-001 1.00000E+001 IT 3.10000E-001 1.70000E-001 1.00000E+001 IT 3.20000E-001 3.50000E-001 1.00000E+001 IT 3.30000E-001 5.10000E-001 1.00000E+001 IT 3.40000E-001 6.60000E-001 1.00000E+001 IT 3.50000E-001 7.80000E-001 1.00000E+001 IT 3.60000E-001 8.60000E-001 1.00000E+001 IT 3.70000E-001 9.22000E-001 1.00000E+001 IT 3.80000E-001 9.52000E-001 1.00000E+001 IT 3.90000E-001 9.68000E-001 1.00000E+001 IT 4.00000E-001 9.77000E-001 1.00000E+001 IT 4.20000E-001 9.86000E-001 1.00000E+001 IT 4.40000E-001 9.90000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.98000E-001 1.00000E+001 IT 8.50000E-001 9.98000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.96000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM M-FDS1 1 923209 1.92286 20.88 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 8.800000000E+000 1.110000000E+001 4.420000000E+000 2.630000000E-002 0 0 CD 3.498422400E+000 -1.689542000E-002 5.756707800E-002 5.169366800E-003 -3.996631000E-004 6.236858200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.836210000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.90000E-001 3.30000E-002 1.00000E+001 IT 4.00000E-001 2.09000E-001 1.00000E+001 IT 4.20000E-001 6.41000E-001 1.00000E+001 IT 4.40000E-001 8.23000E-001 1.00000E+001 IT 4.60000E-001 8.96000E-001 1.00000E+001 IT 4.80000E-001 9.32000E-001 1.00000E+001 IT 5.00000E-001 9.53000E-001 1.00000E+001 IT 5.50000E-001 9.83000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM MP-FDS1 1 923209 1.92286 20.88 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 8.800000000E+000 1.110000000E+001 4.420000000E+000 2.630000000E-002 0 0 CD 3.498422400E+000 -1.689542000E-002 5.756707800E-002 5.169366800E-003 -3.996631000E-004 6.236858200E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.836210000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 1.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.90000E-001 3.30000E-002 1.00000E+001 IT 4.00000E-001 2.09000E-001 1.00000E+001 IT 4.20000E-001 6.41000E-001 1.00000E+001 IT 4.40000E-001 8.23000E-001 1.00000E+001 IT 4.60000E-001 8.96000E-001 1.00000E+001 IT 4.80000E-001 9.32000E-001 1.00000E+001 IT 5.00000E-001 9.53000E-001 1.00000E+001 IT 5.50000E-001 9.83000E-001 1.00000E+001 IT 6.00000E-001 9.93000E-001 1.00000E+001 IT 6.50000E-001 9.94000E-001 1.00000E+001 IT 7.00000E-001 9.95000E-001 1.00000E+001 IT 7.50000E-001 9.96000E-001 1.00000E+001 IT 7.80000E-001 9.96000E-001 1.00000E+001 IT 8.00000E-001 9.97000E-001 1.00000E+001 IT 8.30000E-001 9.96000E-001 1.00000E+001 IT 8.50000E-001 9.96000E-001 1.00000E+001 IT 9.00000E-001 9.97000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.99000E-001 1.00000E+001 IT 1.40000E+000 9.98000E-001 1.00000E+001 IT 1.50000E+000 9.95000E-001 1.00000E+001 IT 1.55000E+000 9.96000E-001 1.00000E+001 NM M-LAF81 1 731405 1.73077 40.50 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 8.900000000E+000 1.130000000E+001 3.220000000E+000 -4.000000000E-003 0 0 CD 2.916788600E+000 -1.239819900E-002 2.667523700E-002 6.519050400E-004 4.695617500E-006 2.691054000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.726080000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 5.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.30000E-001 1.90000E-002 1.00000E+001 IT 3.40000E-001 1.67000E-001 1.00000E+001 IT 3.50000E-001 4.46000E-001 1.00000E+001 IT 3.60000E-001 6.58000E-001 1.00000E+001 IT 3.70000E-001 7.63000E-001 1.00000E+001 IT 3.80000E-001 8.26000E-001 1.00000E+001 IT 3.90000E-001 8.76000E-001 1.00000E+001 IT 4.00000E-001 9.14000E-001 1.00000E+001 IT 4.20000E-001 9.52000E-001 1.00000E+001 IT 4.40000E-001 9.68000E-001 1.00000E+001 IT 4.60000E-001 9.80000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.89000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MP-LAF81 1 731405 1.73077 40.50 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 8.900000000E+000 1.130000000E+001 3.220000000E+000 -4.000000000E-003 0 0 CD 2.916788600E+000 -1.239819900E-002 2.667523700E-002 6.519050400E-004 4.695617500E-006 2.691054000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.726080000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 5.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 3.30000E-001 1.90000E-002 1.00000E+001 IT 3.40000E-001 1.67000E-001 1.00000E+001 IT 3.50000E-001 4.46000E-001 1.00000E+001 IT 3.60000E-001 6.58000E-001 1.00000E+001 IT 3.70000E-001 7.63000E-001 1.00000E+001 IT 3.80000E-001 8.26000E-001 1.00000E+001 IT 3.90000E-001 8.76000E-001 1.00000E+001 IT 4.00000E-001 9.14000E-001 1.00000E+001 IT 4.20000E-001 9.52000E-001 1.00000E+001 IT 4.40000E-001 9.68000E-001 1.00000E+001 IT 4.60000E-001 9.80000E-001 1.00000E+001 IT 4.80000E-001 9.88000E-001 1.00000E+001 IT 5.00000E-001 9.93000E-001 1.00000E+001 IT 5.50000E-001 9.97000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.89000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM M-NBF1 1 743493 1.74330 49.33 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.700000000E+000 7.300000000E+000 4.250000000E+000 -6.800000000E-003 0 0 CD 2.975245000E+000 -1.425016000E-002 2.140074000E-002 9.755337000E-004 -6.979530000E-005 4.114924000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.123940000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.20000E-002 1.00000E+001 IT 2.90000E-001 1.32000E-001 1.00000E+001 IT 3.00000E-001 2.50000E-001 1.00000E+001 IT 3.10000E-001 3.27000E-001 1.00000E+001 IT 3.20000E-001 5.21000E-001 1.00000E+001 IT 3.30000E-001 6.48000E-001 1.00000E+001 IT 3.40000E-001 7.57000E-001 1.00000E+001 IT 3.50000E-001 8.38000E-001 1.00000E+001 IT 3.60000E-001 9.01000E-001 1.00000E+001 IT 3.70000E-001 9.38000E-001 1.00000E+001 IT 3.80000E-001 9.61000E-001 1.00000E+001 IT 3.90000E-001 9.72000E-001 1.00000E+001 IT 4.00000E-001 9.81000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.89000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MP-NBF1 1 743493 1.74330 49.33 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.700000000E+000 7.300000000E+000 4.250000000E+000 -6.800000000E-003 0 0 CD 2.975245000E+000 -1.425016000E-002 2.140074000E-002 9.755337000E-004 -6.979530000E-005 4.114924000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.123940000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 3.20000E-002 1.00000E+001 IT 2.90000E-001 1.32000E-001 1.00000E+001 IT 3.00000E-001 2.50000E-001 1.00000E+001 IT 3.10000E-001 3.27000E-001 1.00000E+001 IT 3.20000E-001 5.21000E-001 1.00000E+001 IT 3.30000E-001 6.48000E-001 1.00000E+001 IT 3.40000E-001 7.57000E-001 1.00000E+001 IT 3.50000E-001 8.38000E-001 1.00000E+001 IT 3.60000E-001 9.01000E-001 1.00000E+001 IT 3.70000E-001 9.38000E-001 1.00000E+001 IT 3.80000E-001 9.61000E-001 1.00000E+001 IT 3.90000E-001 9.72000E-001 1.00000E+001 IT 4.00000E-001 9.81000E-001 1.00000E+001 IT 4.20000E-001 9.87000E-001 1.00000E+001 IT 4.40000E-001 9.91000E-001 1.00000E+001 IT 4.60000E-001 9.93000E-001 1.00000E+001 IT 4.80000E-001 9.95000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.98000E-001 1.00000E+001 IT 6.50000E-001 9.98000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.99000E-001 1.00000E+001 IT 9.50000E-001 9.99000E-001 1.00000E+001 IT 1.00000E+000 9.99000E-001 1.00000E+001 IT 1.05000E+000 9.99000E-001 1.00000E+001 IT 1.06000E+000 9.99000E-001 1.00000E+001 IT 1.10000E+000 9.99000E-001 1.00000E+001 IT 1.20000E+000 9.99000E-001 1.00000E+001 IT 1.30000E+000 9.95000E-001 1.00000E+001 IT 1.40000E+000 9.89000E-001 1.00000E+001 IT 1.50000E+000 9.94000E-001 1.00000E+001 IT 1.55000E+000 9.95000E-001 1.00000E+001 NM MC-NBF1 1 743493 1.74330 49.33 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 5.700000000E+000 7.300000000E+000 4.250000000E+000 -6.800000000E-003 0 0 CD 2.975245000E+000 -1.425016000E-002 2.140074000E-002 9.755337000E-004 -6.979530000E-005 4.114924000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 1.123940000E-005 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 4.00000 4.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 1.70000E-001 1.00000E+001 IT 2.90000E-001 3.41000E-001 1.00000E+001 IT 3.00000E-001 4.51000E-001 1.00000E+001 IT 3.10000E-001 4.86000E-001 1.00000E+001 IT 3.20000E-001 6.77000E-001 1.00000E+001 IT 3.30000E-001 7.75000E-001 1.00000E+001 IT 3.40000E-001 8.52000E-001 1.00000E+001 IT 3.50000E-001 9.09000E-001 1.00000E+001 IT 3.60000E-001 9.46000E-001 1.00000E+001 IT 3.70000E-001 9.69000E-001 1.00000E+001 IT 3.80000E-001 9.81000E-001 1.00000E+001 IT 3.90000E-001 9.88000E-001 1.00000E+001 IT 4.00000E-001 9.92000E-001 1.00000E+001 IT 4.20000E-001 9.95000E-001 1.00000E+001 IT 4.40000E-001 9.96000E-001 1.00000E+001 IT 4.60000E-001 9.97000E-001 1.00000E+001 IT 4.80000E-001 9.97000E-001 1.00000E+001 IT 5.00000E-001 9.98000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.99000E-001 1.00000E+001 IT 6.50000E-001 9.99000E-001 1.00000E+001 IT 7.00000E-001 9.99000E-001 1.00000E+001 IT 7.50000E-001 9.99000E-001 1.00000E+001 IT 7.80000E-001 9.99000E-001 1.00000E+001 IT 8.00000E-001 9.99000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.97000E-001 1.00000E+001 IT 1.00000E+000 9.97000E-001 1.00000E+001 IT 1.05000E+000 9.97000E-001 1.00000E+001 IT 1.06000E+000 9.97000E-001 1.00000E+001 IT 1.10000E+000 9.97000E-001 1.00000E+001 IT 1.20000E+000 9.97000E-001 1.00000E+001 IT 1.30000E+000 9.96000E-001 1.00000E+001 IT 1.40000E+000 9.88000E-001 1.00000E+001 IT 1.50000E+000 9.88000E-001 1.00000E+001 IT 1.55000E+000 9.89000E-001 1.00000E+001 NM M-TAF1 1 773495 1.77250 49.47 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.600000000E+000 9.000000000E+000 4.830000000E+000 -5.200000000E-003 0 0 CD 3.070806000E+000 -1.227692400E-002 2.456566000E-002 4.743664800E-004 5.432616000E-007 6.597666100E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.461840000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 4.70000E-002 1.00000E+001 IT 2.90000E-001 1.16000E-001 1.00000E+001 IT 3.00000E-001 1.84000E-001 1.00000E+001 IT 3.10000E-001 2.02000E-001 1.00000E+001 IT 3.20000E-001 4.46000E-001 1.00000E+001 IT 3.30000E-001 5.98000E-001 1.00000E+001 IT 3.40000E-001 7.31000E-001 1.00000E+001 IT 3.50000E-001 8.31000E-001 1.00000E+001 IT 3.60000E-001 9.00000E-001 1.00000E+001 IT 3.70000E-001 9.42000E-001 1.00000E+001 IT 3.80000E-001 9.66000E-001 1.00000E+001 IT 3.90000E-001 9.78000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001 NM MC-TAF1 1 773495 1.77250 49.47 0 3 5 GC Not in a position to accept new order because of discontinuation. ED 7.600000000E+000 9.000000000E+000 4.830000000E+000 -5.200000000E-003 0 0 CD 3.070806000E+000 -1.227692400E-002 2.456566000E-002 4.743664800E-004 5.432616000E-007 6.597666100E-007 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 TD 3.461840000E-006 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 0.000000000E+000 2.000000000E+001 OD -1.00000 1.00000 1.00000 3.00000 -1.00000 -1.00000 LD 3.65010000E-001 1.01398000E+000 IT 2.80000E-001 4.70000E-002 1.00000E+001 IT 2.90000E-001 1.16000E-001 1.00000E+001 IT 3.00000E-001 1.84000E-001 1.00000E+001 IT 3.10000E-001 2.02000E-001 1.00000E+001 IT 3.20000E-001 4.46000E-001 1.00000E+001 IT 3.30000E-001 5.98000E-001 1.00000E+001 IT 3.40000E-001 7.31000E-001 1.00000E+001 IT 3.50000E-001 8.31000E-001 1.00000E+001 IT 3.60000E-001 9.00000E-001 1.00000E+001 IT 3.70000E-001 9.42000E-001 1.00000E+001 IT 3.80000E-001 9.66000E-001 1.00000E+001 IT 3.90000E-001 9.78000E-001 1.00000E+001 IT 4.00000E-001 9.85000E-001 1.00000E+001 IT 4.20000E-001 9.90000E-001 1.00000E+001 IT 4.40000E-001 9.92000E-001 1.00000E+001 IT 4.60000E-001 9.94000E-001 1.00000E+001 IT 4.80000E-001 9.96000E-001 1.00000E+001 IT 5.00000E-001 9.97000E-001 1.00000E+001 IT 5.50000E-001 9.98000E-001 1.00000E+001 IT 6.00000E-001 9.97000E-001 1.00000E+001 IT 6.50000E-001 9.97000E-001 1.00000E+001 IT 7.00000E-001 9.98000E-001 1.00000E+001 IT 7.50000E-001 9.98000E-001 1.00000E+001 IT 7.80000E-001 9.98000E-001 1.00000E+001 IT 8.00000E-001 9.98000E-001 1.00000E+001 IT 8.30000E-001 9.99000E-001 1.00000E+001 IT 8.50000E-001 9.99000E-001 1.00000E+001 IT 9.00000E-001 9.98000E-001 1.00000E+001 IT 9.50000E-001 9.98000E-001 1.00000E+001 IT 1.00000E+000 9.98000E-001 1.00000E+001 IT 1.05000E+000 9.98000E-001 1.00000E+001 IT 1.06000E+000 9.98000E-001 1.00000E+001 IT 1.10000E+000 9.98000E-001 1.00000E+001 IT 1.20000E+000 9.98000E-001 1.00000E+001 IT 1.30000E+000 9.98000E-001 1.00000E+001 IT 1.40000E+000 9.97000E-001 1.00000E+001 IT 1.50000E+000 9.96000E-001 1.00000E+001 IT 1.55000E+000 9.97000E-001 1.00000E+001