Optical constants of HOYA - TaFD (Dense tantalum flint)
TAFD45
Wavelength:
µm
(0.360 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.672962-0.0151805λ^{2}+0.0457187λ^{-2}+0.002186221λ^{-4}-9.93742\text{×}10^{-05}λ^{-6}+1.490466\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 8.36e-07 9.08e-09 -4.59e-11 9.61e-07 1.39e-09 0.246 nd: 1.95375 Vd: 32.32 glass_code: 954323 glass_status: standard density: 5.1 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.5e-06 K-1 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia