Optical constants of HOYA - TaFD (Dense tantalum flint)
TAFD40

Wavelength: µm
 (0.36501 – 1.550)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.8106232-0.016351565λ^{2}+0.058801097λ^{-2}+0.0034919026λ^{-4}-0.0001694811λ^{-6}+3.2569333\text{×}10^{-05}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -1.53e-06 7.62e-09 -3.12e-11 1.08e-06 1.19e-09 0.287
nd: 2.00069
Vd: 25.46
glass_status: standard
density: 4.73 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 7.2e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 8.7e-06 K-1
dPgF: 0.0111
climatic_resistance: 1.0
stain_resistance: 1.0
acid_resistance: 1.0

Comments

Recommended glass type

References

HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

HOYA Corporation

Hoya Corporation is a Japanese company manufacturing optical products.

External links


Glass