Optical constants of HOYA - TaFD (Dense tantalum flint)
TAFD37A
Wavelength:
µm
(0.350 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.4958125-0.014342354λ^{2}+0.037807251λ^{-2}+0.0014184073λ^{-4}-4.6470269\text{×}10^{-05}λ^{-6}+6.919444\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.28e-07 8.14e-09 -5.08e-11 8.44e-07 7.6e-10 0.225 nd: 1.90043 Vd: 37.37 glass_code: 900374 glass_status: standard density: 4.9 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.5e-06 K-1 dPgF: -0.0043 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia