Optical constants of HOYA - TaFD (Dense tantalum flint)
TAFD32
Wavelength:
µm
(0.320 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.396108-0.013087065λ^{2}+0.034853516λ^{-2}+0.00079083177λ^{-4}+7.6995212\text{×}10^{-06}λ^{-6}+2.3516742\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.82e-07 8.11e-09 -2.84e-11 9.6e-07 9.61e-10 0.141 nd: 1.87070 Vd: 40.73 glass_code: 871407 glass_status: standard density: 4.84 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.4e-06 K-1 dPgF: -0.0067 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 2.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia