Optical constants of HOYA - TaFD (Dense tantalum flint)
MP-TAFD307
Wavelength:
µm
(0.350 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.4286062-0.013845333λ^{2}+0.037363009λ^{-2}+0.0011894554λ^{-4}-1.5979979\text{×}10^{-05}λ^{-6}+5.1827398\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.80622e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.88202 Vd: 37.22 glass_code: 882372 glass_status: standard density: 5.49 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.3e-06 K-1 dPgF: -0.0044 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 3.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia