Optical constants of HOYA - TaFD (Dense tantalum flint)
M-TAFD305
Wavelength:
µm
(0.340 – 1.550)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.327184-0.01343242λ^{2}+0.033398λ^{-2}+0.001006047λ^{-4}-2.136908\text{×}10^{-05}λ^{-6}+3.972561\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.25e-06 1.17e-08 -4.51e-11 1.25e-06 1.27e-09 0.0455 nd: 1.85135 Vd: 40.10 glass_code: 851401 glass_status: standard density: 5.25 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.8e-06 K-1 dPgF: -0.0067 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 3.0
Comments
Glass for molded optics lens
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia