Optical constants of HOYA - TaF (Tantalum flint)
TAF1
Wavelength:
µm
(0.300 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0736378-0.015501284λ^{2}+0.023627699λ^{-2}+0.00066300852λ^{-4}-2.8353438\text{×}10^{-05}λ^{-6}+2.2090799\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.76e-06 9.56e-09 -3.12e-11 5.1e-07 3.46e-10 0.216 nd: 1.77250 Vd: 49.62 glass_code: 773496 glass_status: standard density: 4.28 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.3e-06 K-1 dPgF: -0.0086 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 3.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia