$$n^2=3.164475-0.013801295λ^{2}+0.027926276λ^{-2}+0.00057403λ^{-4}+9.8223773\text{×}10^{-07}λ^{-6}+1.3284244\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.66812e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.80154 Vd: 45.46 glass_code: 802455 glass_status: standard density: 4.84 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.7e-06 K-1 dPgF: -0.0084 climatic_resistance: 1.0 stain_resistance: 3.0 acid_resistance: 3.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia