Optical constants of HOYA - TaF (Tantalum flint)
MC-TAF1
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.070806-0.012276924λ^{2}+0.02456566λ^{-2}+0.00047436648λ^{-4}+5.432616\text{×}10^{-07}λ^{-6}+6.5976661\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.46184e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.77250 Vd: 49.47 glass_code: 773495 glass_status: special density: 4.83 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 9e-06 K-1 dPgF: -0.0052 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 3.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia