Optical constants of HOYA - TaF (Tantalum flint)
M-TAF105
Wavelength:
µm
(0.280 – 1.550)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.0705638-0.013310234λ^{2}+0.025280355λ^{-2}+0.00021829234λ^{-4}+3.2555293\text{×}10^{-05}λ^{-6}-8.1300421\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.74e-06 9.55e-09 -5.15e-11 6.48e-07 3.61e-10 0.166 nd: 1.77250 Vd: 49.50 glass_code: 773495 glass_status: standard density: 4.62 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 7e-06 K-1 dPgF: -0.0072 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 4.0
Comments
Glass for molded optics lens
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia