Optical constants of HOYA - TaC (Tantalum crown)
MP-TAC80-60
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9372128-0.016185789λ^{2}+0.01839514λ^{-2}+0.0010266071λ^{-4}-9.2379872\text{×}10^{-05}λ^{-6}+5.0509237\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.67223e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.72963 Vd: 54.07 glass_code: 730541 glass_status: standard density: 4.28 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.4e-06 K-1 dPgF: -0.0064 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 4.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia