Optical constants of HOYA - PCD (Dense phosphate crown)
PCD40
Wavelength:
µm
(0.310 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5844463-0.0090521858λ^{2}+0.014301987λ^{-2}+0.0001705077λ^{-4}+4.964536\text{×}10^{-06}λ^{-6}-1.2927479\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.08e-05 2.42e-09 1.57e-11 7.21e-07 4.29e-10 1.46e-09 nd: 1.61997 Vd: 63.88 glass_code: 620639 glass_status: standard density: 3.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.03e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.3e-05 K-1 dPgF: 0.0093 climatic_resistance: 1.0 acid_resistance: 4.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia