Optical constants of HOYA - PCD (Dense phosphate crown)
MP-PCD51-70
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5025436-0.010321437λ^{2}+0.012433636λ^{-2}+0.00021866535λ^{-4}-5.5793977\text{×}10^{-06}λ^{-6}+3.0188383\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -5.75e-06 4.33e-09 -1.7e-11 3.99e-07 4.04e-10 0.175 nd: 1.59271 Vd: 66.97 glass_code: 593670 glass_status: standard density: 3.14 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.16e-05 K-1 dPgF: 0.009 climatic_resistance: 1.0 acid_resistance: 4.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia