Optical constants of HOYA - PCD (Dense phosphate crown)
M-PCD4
Wavelength:
µm
(0.320 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.582335-0.009952039λ^{2}+0.01329184λ^{-2}+0.0004550621λ^{-4}-3.327132\text{×}10^{-05}λ^{-6}+1.730172\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.08e-05 2.42e-09 1.57e-11 7.21e-07 4.29e-10 1.46e-09 nd: 1.61881 Vd: 63.85 glass_code: 619639 glass_status: standard density: 3.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.3e-05 K-1 dPgF: 0.0084 climatic_resistance: 1.0 acid_resistance: 4.0
Comments
Glass for molded optics lens
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision