Optical constants of HOYA - NbFD (Dense niobium flint)
NBFD13
Wavelength:
µm
(0.340 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1729223-0.014248534λ^{2}+0.029168114λ^{-2}+0.001342876λ^{-4}-9.6178753\text{×}10^{-05}λ^{-6}+8.4042556\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.67424e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.80610 Vd: 40.73 glass_code: 806407 glass_status: standard density: 4.38 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.2e-06 K-1 dPgF: -0.0078 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 3.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia