Optical constants of HOYA - NbF (Niobium flint)
M-NBF1
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.975245-0.01425016λ^{2}+0.02140074λ^{-2}+0.0009755337λ^{-4}-6.97953\text{×}10^{-05}λ^{-6}+4.114924\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.12394e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.74330 Vd: 49.33 glass_code: 743493 glass_status: special density: 4.25 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.3e-06 K-1 dPgF: -0.0068 climatic_resistance: 1.0 stain_resistance: 4.0 acid_resistance: 4.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia