Optical constants of HOYA - LaF (Lanthanum flint)
M-LAF81
Wavelength:
µm
(0.330 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9167886-0.012398199λ^{2}+0.026675237λ^{-2}+0.00065190504λ^{-4}+4.6956175\text{×}10^{-06}λ^{-6}+2.691054\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.72608e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.73077 Vd: 40.50 glass_code: 731405 glass_status: special density: 3.22 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.13e-05 K-1 dPgF: -0.004 climatic_resistance: 1.0 stain_resistance: 5.0 acid_resistance: 3.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia