Optical constants of HOYA - LaF (Lanthanum flint)
LAF3

Wavelength: µm
 (0.320 – 1.550)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.8789799-0.008729237λ^{2}+0.024425656λ^{-2}+4.5491773\text{×}10^{-05}λ^{-4}+4.2802928\text{×}10^{-05}λ^{-6}-7.2834306\text{×}10^{-07}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -1.75538e-07 0.0 0.0 0.0 0.0 0.0
nd: 1.71700
Vd: 47.98
glass_code: 717480
density: 4.2 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 8e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 9.3e-06 K-1
dPgF: -0.0063
climatic_resistance: 1.0
stain_resistance: 2.0
acid_resistance: 4.0

Comments

General glass Type

References

HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

HOYA Corporation

Hoya Corporation is a Japanese company manufacturing optical products.

External links


Glass

External links