Optical constants of HOYA - LaCL (Light lanthanum crown)
LACL60
Wavelength:
µm
(0.280 – 1.550)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.6490884-0.014159869λ^{2}+0.014451135λ^{-2}+0.00052707873λ^{-4}-4.3447523\text{×}10^{-05}λ^{-6}+2.4612971\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.28907e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.64000 Vd: 60.20 glass_code: 640602 glass_status: special density: 3.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.8e-06 K-1 dPgF: -0.0039 climatic_resistance: 3.0 stain_resistance: 5.0 acid_resistance: 4.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia