Optical constants of HOYA - LaC (Lanthanum crown)
MP-LAC130
Wavelength:
µm
(0.290 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.813412-0.01332448λ^{2}+0.01927865λ^{-2}+0.0004124452λ^{-4}-9.940432\text{×}10^{-06}λ^{-6}+9.622024\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.06e-06 7.53e-09 -3.42e-11 7.88e-07 1.05e-09 4.45e-10 nd: 1.69350 Vd: 53.20 glass_code: 694532 glass_status: standard density: 3.52 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.6e-06 K-1 dPgF: -0.0059 climatic_resistance: 1.0 stain_resistance: 4.0 acid_resistance: 4.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia