Optical constants of HOYA - LaC (Lanthanum crown)
M-LAC8
Wavelength:
µm
(0.290 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8817481-0.015730804λ^{2}+0.017690493λ^{-2}+0.001052669λ^{-4}-9.909308\text{×}10^{-05}λ^{-6}+5.5248378\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 5.47002e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.71300 Vd: 53.94 glass_code: 713539 glass_status: special density: 3.9 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.9e-06 K-1 dPgF: -0.0064 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 4.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia