Optical constants of HOYA - LaC (Lanthanum crown)
LAC14
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8255229-0.013632902λ^{2}+0.019791402λ^{-2}+1.5032564\text{×}10^{-05}λ^{-4}+4.0761368\text{×}10^{-05}λ^{-6}-1.7527267\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.05e-06 1.07e-08 -2.21e-11 4.35e-07 4.49e-10 0.185 nd: 1.69680 Vd: 55.46 glass_code: 697555 glass_status: standard density: 3.67 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.2e-06 K-1 dPgF: -0.0059 climatic_resistance: 1.0 acid_resistance: 4.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia