Optical constants of HOYA - LaC (Lanthanum crown)
LAC10
Wavelength:
µm
(0.300 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8951998-0.011701218λ^{2}+0.022126485λ^{-2}+0.00038494791λ^{-4}-7.9808302\text{×}10^{-06}λ^{-6}+1.5035116\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.44934e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.72000 Vd: 50.34 glass_code: 720503 glass_status: special density: 3.87 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.4e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.1e-06 K-1 dPgF: -0.0075 climatic_resistance: 1.0 stain_resistance: 4.0 acid_resistance: 4.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia