LBC3N
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5388484-0.0066855865λ^{2}+0.015111456λ^{-2}-0.00015247241λ^{-4}+4.8340116\text{×}10^{-05}λ^{-6}-2.4061785\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.94562e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.60625 Vd: 63.71 glass_code: 606637 glass_status: special density: 3.84 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.24e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.4e-05 K-1 dPgF: 0.0108 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 3.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia