Optical constants of HOYA - FL (Light flint)
E-FL6
Wavelength:
µm
(0.350 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4079653-0.011135638λ^{2}+0.015704715λ^{-2}+0.00099186507λ^{-4}-7.9934653\text{×}10^{-05}λ^{-6}+7.0985473\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 3.42721e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.56732 Vd: 42.84 glass_code: 567428 density: 2.53 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.7e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.9e-06 K-1 dPgF: 0.0031 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)