Optical constants of HOYA - FEL (Extra light flint)
E-FEL6
Wavelength:
µm
(0.340 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3068946-0.0096888755λ^{2}+0.01309702λ^{-2}+0.00065013927λ^{-4}-4.2328222\text{×}10^{-05}λ^{-6}+3.5888777\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.49277e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.53172 Vd: 48.84 glass_code: 532488 glass_status: special density: 2.51 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.5e-06 K-1 dPgF: 0.0051 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia