Optical constants of HOYA - FDS (Special dense flint)
MC-FDS910-50
Wavelength:
µm
(0.36501 – 1.550)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.1667902-0.013141416λ^{2}+0.047178656λ^{-2}+0.0022684284λ^{-4}-5.3672387\text{×}10^{-05}λ^{-6}+2.5328422\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.8056e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.82165 Vd: 24.04 glass_code: 822240 glass_status: standard density: 3.69 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.21e-05 K-1 dPgF: 0.0187 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia