Optical constants of HOYA - FDS (Special dense flint)
MC-FDS2
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.771581-0.020445364λ^{2}+0.063942579λ^{-2}+0.008354547λ^{-4}-0.00082031984λ^{-6}+0.00010279507λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.17e-07 1.14e-08 -3.07e-11 1.84e-06 2.48e-09 0.308 nd: 2.00178 Vd: 19.32 glass_status: standard density: 5.09 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.01e-05 K-1 dPgF: 0.0312 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia