Optical constants of HOYA - FDS (Special dense flint)
FDS90

Wavelength: µm
 (0.36501 – 1.550)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.2606321-0.017780398λ^{2}+0.040902938λ^{-2}+0.0056076934λ^{-4}-0.00056434039λ^{-6}+5.4763391\text{×}10^{-05}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -4.62e-06 1.29e-08 -2.11e-11 1.04e-06 1.27e-09 0.296
nd: 1.84666
Vd: 23.78
glass_code: 847238
density: 3.5 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 8.7e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.07e-05 K-1
dPgF: 0.0137
climatic_resistance: 2.0
stain_resistance: 1.0
acid_resistance: 1.0

Comments

General glass Type

References

HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

HOYA Corporation

Hoya Corporation is a Japanese company manufacturing optical products.

External links


Glass

External links