Optical constants of HOYA - FDS (Special dense flint)
FDS24
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.5126327-0.0153015λ^{2}+0.053936061λ^{-2}+0.0034949369λ^{-4}-0.00017950295λ^{-6}+3.4403181\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -3.37e-06 7.78e-09 -2.33e-11 1.13e-06 1.32e-09 0.275 nd: 1.92119 Vd: 23.96 glass_code: 921240 glass_status: standard density: 3.84 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.8e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.6e-06 K-1 dPgF: 0.0151 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia