Optical constants of HOYA - FDS (Special dense flint)
FDS18
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.563784-0.025449644λ^{2}+0.058401659λ^{-2}+0.0092310983λ^{-4}-0.00095499727λ^{-6}+0.00011777456λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.60984e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.94595 Vd: 17.98 glass_code: 946180 density: 3.51 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.1e-06 K-1 dPgF: 0.0386 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision