Optical constants of HOYA - FDS (Special dense flint)
E-FDS3
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=4.1120387-0.01822767λ^{2}+0.089852105λ^{-2}+0.00787144λ^{-4}-0.00052228008λ^{-6}+0.00011773061λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.98e-06 1.44e-08 -3.95e-11 2.17e-06 2.05e-09 0.302 nd: 2.10420 Vd: 17.02 glass_code: 104170 density: 5.63 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.2e-06 K-1 dPgF: 0.0455 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia