Optical constants of HOYA - FDS (Special dense flint)
E-FDS1-W
Wavelength:
µm
(0.36501 – 1.550)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.5044639-0.020333833λ^{2}+0.0538027λ^{-2}+0.0062874192λ^{-4}-0.00056922176λ^{-6}+7.3559387\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -4.37e-06 1.1e-08 -2.29e-11 1.06e-06 1.516e-09 0.311 nd: 1.92286 Vd: 20.88 glass_code: 923209 glass_status: standard density: 3.94 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.5e-06 K-1 dPgF: 0.0282 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 1.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia