Optical constants of HOYA - FD (Dense flint)
MP-FD80
Wavelength:
µm
(0.360 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.761638-0.01132633λ^{2}+0.02865346λ^{-2}+0.001529038λ^{-4}-8.743577\text{×}10^{-05}λ^{-6}+1.496579\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -8.15303e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.68893 Vd: 31.16 glass_code: 689312 glass_status: standard density: 3.26 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.15e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.43e-05 K-1 dPgF: 0.0115 climatic_resistance: 3.0 stain_resistance: 3.0 acid_resistance: 3.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia