Optical constants of HOYA - FD (Dense flint)
FD60
Wavelength:
µm
(0.360 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1171483-0.011616277λ^{2}+0.044864975λ^{-2}+0.0016588491λ^{-4}+2.5716854\text{×}10^{-05}λ^{-6}+1.4757657\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -5.29e-06 9.6e-09 -5.1e-11 1.06e-06 1.34e-09 0.282 nd: 1.80518 Vd: 25.46 glass_code: 805255 density: 3.36 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.09e-05 K-1 dPgF: 0.0132 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia