Optical constants of HOYA - FD (Dense flint)
FD225
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1189869-0.015820772λ^{2}+0.044425024λ^{-2}+0.0035834882λ^{-4}-0.00023943449λ^{-6}+3.8756542\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.09e-05 4.1e-09 -1.04e-11 1.01e-06 1.33e-09 0.307 nd: 1.80809 Vd: 22.76 glass_code: 808228 glass_status: standard density: 3.32 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1.18e-05 K-1 dPgF: 0.0213 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia