Optical constants of HOYA - FD (Dense flint)
FD140
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9851294-0.014237988λ^{2}+0.035496437λ^{-2}+0.0028457557λ^{-4}-0.00019006799λ^{-6}+2.4309252\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 8.31157e-07 0.0 0.0 0.0 0.0 0.0 nd: 1.76182 Vd: 26.61 glass_code: 762266 density: 3.14 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.4e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.02e-05 K-1 dPgF: 0.0118 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia