Optical constants of HOYA - FD (Dense flint)
FD110
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0534415-0.01275181λ^{2}+0.040609369λ^{-2}+0.0022706109λ^{-4}-7.8086606\text{×}10^{-05}λ^{-6}+1.9874026\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.29676e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.78472 Vd: 25.72 glass_code: 785257 density: 3.22 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.1e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.08e-05 K-1 dPgF: 0.0138 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links