Optical constants of HOYA - FD (Dense flint)
E-FD10
Wavelength:
µm
(0.36501 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.881518-0.013228312λ^{2}+0.03145559λ^{-2}+0.0026851666λ^{-4}-0.00022577544λ^{-6}+2.4693268\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.45505e-07 0.0 0.0 0.0 0.0 0.0 nd: 1.72825 Vd: 28.32 glass_code: 728283 density: 3.07 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.09e-05 K-1 dPgF: 0.0085 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
SF10 optical glass
SF10 is a popular optical glass. Most glass makers produce this or very similar glass under slightly different names.SF10 and similar glasses produced by different makers
Maker | Glass |
---|---|
Schott | N-SF10 |
Hikari | E-SF10 |
HOYA | E-FD10 |
Sumita | K-SFLD10 |
CDGM | ZF4 |
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia