Optical constants of HOYA - FD (Dense flint)
E-FD1
Wavelength:
µm
(0.360 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8508499-0.01323461λ^{2}+0.029415325λ^{-2}+0.0025542666λ^{-4}-0.00021232133λ^{-6}+2.2261936\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.50033e-07 0.0 0.0 0.0 0.0 0.0 nd: 1.71736 Vd: 29.50 glass_code: 717295 density: 3.08 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.09e-05 K-1 dPgF: 0.0082 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 1.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia