Optical constants of HOYA - FCD (Dense fluor crown)
MP-FCD500-20
Wavelength:
µm
(0.310 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3850427-0.007914269λ^{2}+0.0094886852λ^{-2}+0.00057980093λ^{-4}-6.0011677\text{×}10^{-05}λ^{-6}+3.0355422\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.78e-05 -4.97e-09 7.88e-11 4.91e-07 3.43e-10 4.41e-08 nd: 1.55352 Vd: 71.72 glass_code: 554717 glass_status: standard density: 3.66 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.24e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.53e-05 K-1 dPgF: 0.0207 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 3.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia