Optical constants of HOYA - FCD (Dense fluor crown)
M-FCD500
Wavelength:
µm
(0.310 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3841554-0.0078084423λ^{2}+0.0097130883λ^{-2}+0.00049959889λ^{-4}-4.7303224\text{×}10^{-05}λ^{-6}+2.3205441\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.78e-05 -4.97e-09 7.88e-11 4.91e-07 3.43e-10 4.41e-08 nd: 1.55332 Vd: 71.68 glass_code: 553717 glass_status: standard density: 3.66 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.24e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.53e-05 K-1 dPgF: 0.0211 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 3.0
Comments
Glass for molded optics lens
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia