Optical constants of HOYA - FCD (Dense fluor crown)
FCD505
Wavelength:
µm
(0.320 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.502355-0.0072080042λ^{2}+0.012012743λ^{-2}+0.00034920842λ^{-4}-2.4729676\text{×}10^{-05}λ^{-6}+1.3801567\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.88e-05 4.93e-09 5.59e-11 5.35e-07 4.25e-10 1.81e-08 nd: 1.59282 Vd: 68.63 glass_code: 593686 glass_status: special density: 4.2 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.15e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.4e-05 K-1 dPgF: 0.0194 climatic_resistance: 1.0 stain_resistance: 1.0 acid_resistance: 3.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia