Optical constants of HOYA - FCD (Dense fluor crown)
FCD10A
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.1085888-0.0046553722λ^{2}+0.006954748λ^{-2}+3.2184141\text{×}10^{-05}λ^{-4}+5.2670946\text{×}10^{-06}λ^{-6}-2.7164844\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.04e-05 -8.81e-09 1.3e-11 3.44e-07 7.67e-11 0.154 nd: 1.45860 Vd: 90.20 glass_code: 459902 glass_status: standard density: 3.63 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.33e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.65e-05 K-1 dPgF: 0.0494 climatic_resistance: 1.0 stain_resistance: 5.0 acid_resistance: 2.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia