Optical constants of HOYA - FCD (Dense fluor crown)
FCD100
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.0482157-0.0043211222λ^{2}+0.0061826755λ^{-2}+3.141148\text{×}10^{-05}λ^{-4}+3.5370793\text{×}10^{-06}λ^{-6}-1.6694497\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.11e-05 -8.57e-09 2.98e-11 2.78e-07 2.18e-10 0.201 nd: 1.43700 Vd: 95.10 glass_code: 437951 glass_status: standard density: 3.53 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.39e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.75e-05 K-1 dPgF: 0.0564 climatic_resistance: 1.0 acid_resistance: 3.0
Comments
Recommended glass type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia