Optical constants of HOYA - FCD (Dense fluor crown)
FCD10
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.103249-0.0050247988λ^{2}+0.0065323077λ^{-2}+0.00013078405λ^{-4}-6.3652072\text{×}10^{-06}λ^{-6}+1.9254745\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.866e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.45650 Vd: 90.27 glass_code: 457903 glass_status: special density: 3.6 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.34e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.57e-05 K-1 dPgF: 0.049 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 2.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia