Optical constants of HOYA - FC (Fluor crown)
FC5
Wavelength:
µm
(0.280 – 1.550)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.1894054-0.0099044908λ^{2}+0.008640337λ^{-2}+0.00022263067λ^{-4}-1.2291942\text{×}10^{-05}λ^{-6}+5.9386349\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_is_absolute: false λ_is_vacuum: false temperature: 20.0 °C coefficients_of_thermal_dispersion: -6.6046e-06 0.0 0.0 0.0 0.0 0.0 n_d: 1.48749 V_d: 70.45 glass_code: 487704 density: 2.45 g/cm3 coefficient_of_thermal_expansion_1: 9.3e-06 K-1 coefficient_of_thermal_expansion_2: 1.02e-05 K-1 ΔP_gF: 0.0092 climatic_resistance: 5.0 stain_resistance: 5.0 acid_resistance: 5.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia