Optical constants of HOYA - BaFD (Dense barium flint)
BAFD7

Wavelength: µm
 (0.350 – 1.550)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.8217211-0.0097265483λ^{2}+0.024345979λ^{-2}+0.00078406305λ^{-4}-2.2431497\text{×}10^{-05}λ^{-6}+4.6726029\text{×}10^{-06}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 6.07532e-06 0.0 0.0 0.0 0.0 0.0
nd: 1.70154
Vd: 41.15
glass_code: 702412
density: 3.65 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 6.8e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 8.4e-06 K-1
dPgF: 0.0028
climatic_resistance: 1.0
stain_resistance: 1.0
acid_resistance: 1.0

Comments

General glass Type

References

HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

HOYA Corporation

Hoya Corporation is a Japanese company manufacturing optical products.

External links


Glass

External links